Grade Name Family Producer
ALCOM® ABS 530/12 SI1 ABS ALBIS Plastic GmbH
ALCOM® ABS 530/22 SV 1287-04 MCS ABS ALBIS Plastic GmbH
ALCOM® ABS 530/22 UV GY1039-07MCS ABS ALBIS Plastic GmbH
ALCOM® ABS 530/23 HGB ABS-GB ALBIS Plastic GmbH
ALCOM® ABS 530/29 SV 1217-04 MCO ABS ALBIS Plastic GmbH
ALCOM® ABS 530/29 SV 1245-05 MCF ABS ALBIS Plastic GmbH
ALCOM® ABS 530/29 SV 31-753 MCF ABS ALBIS Plastic GmbH
ALCOM® ABS 530/29 SV1462-06MCO ABS ALBIS Plastic GmbH
ALCOM® ABS 530/3 GY 31-749 MCF ABS ALBIS Plastic GmbH
ALCOM® ABS 530/3 SV 31-745 MCF ABS ALBIS Plastic GmbH
ALCOM® ABS 530/3 SV 31-748 MCS ABS ALBIS Plastic GmbH
ALCOM® ABS 530/3.1 CF ABS-CF ALBIS Plastic GmbH
ALCOM® ABS 530/36 SV 1031-04 MCF ABS ALBIS Plastic GmbH
ALCOM® AWL 10 WT31-943LB ABS ALBIS Plastic GmbH
ALCOM® AWL 15/1 GY1084-05LB ABS-Z15 ALBIS Plastic GmbH
ALCOM® AWL 15/1 UV WT1471-04LB ABS-Z15 ALBIS Plastic GmbH
ALCOM® AWL 15/1 WT1384-04LB ABS-Z15 ALBIS Plastic GmbH
ALCOM® AWL 15/1 WT31-956LB ABS-Z15 ALBIS Plastic GmbH
ALCOM® MABS 560/1 SV 1214-04 MCF ABS ALBIS Plastic GmbH
ALTECH ABS A 1000/100 ABS ALBIS Plastic GmbH
ALTECH ABS A 1000/106 ABS ALBIS Plastic GmbH
ALTECH ABS A 1000/139 AS ABS ALBIS Plastic GmbH
ALTECH ABS A 1000/177 ABS ALBIS Plastic GmbH
ALTECH ABS A 1000/578 ABS ALBIS Plastic GmbH
ALTECH ABS A 1000/587 ABS ALBIS Plastic GmbH
ALTECH ABS A 2017/500 GF17 ABS-GF17 ALBIS Plastic GmbH
ALTECH ABS A 2020/100 GF20 ABS-GF20 ALBIS Plastic GmbH
ALTECH ABS A 3030/576 GB30 AS ABS-GB30 ALBIS Plastic GmbH
ALTECH ABS A 3230/516 GB20 GF10 ABS-(GB+GF)30 ALBIS Plastic GmbH
Bayblend® T45 PG (ABS+PC) Bayer MaterialScience
POLYFLAM® RABS 90000 UV5 ABS FR A. Schulman GmbH
POLYFLAM® RABS 90000 UV5 natur LS ABS FR A. Schulman GmbH
POLYFLAM® RABS 90350 UV5 ABS-GF15 FR A. Schulman GmbH
POLYFLAM® RABS 90350 UV5-5V ABS-MD15 FR A. Schulman GmbH
POLYFLAM® RABS 90950 UV5 ABS-GF20 FR A. Schulman GmbH
POLYFLAM® RMMB 40300 (ABS+PC) FR... A. Schulman GmbH
POLYFLAM® RMMB 40400 (ABS+PC) FR... A. Schulman GmbH
POLYFLAM® RMMB 4070 (ABS+PC) FR... A. Schulman GmbH
POLYFLAM® RMMB 4070 HF (ABS+PC) FR... A. Schulman GmbH
POLYFLAM® RMMB 60600 (ABS+PC) FR... A. Schulman GmbH
POLYFLAM® RMMB 60700 (ABS+PC) FR... A. Schulman GmbH
POLYFLAM® RMMK 125 (ABS+PA6) FR... A. Schulman GmbH
POLYMAN® (ABS) CR K3000 ABS A. Schulman GmbH
POLYMAN® (ABS) CR K4000 ABS A. Schulman GmbH
POLYMAN® (ABS) E/HI ABS-I A. Schulman GmbH
POLYMAN® (ABS) E/HI CA ABS-I A. Schulman GmbH
POLYMAN® (ABS) FABS 10 GB ABS-GB10 A. Schulman GmbH
POLYMAN® (ABS) FABS 15 GB ABS-GB15 A. Schulman GmbH
POLYMAN® (ABS) FABS 20 GB ABS-GB20 A. Schulman GmbH
POLYMAN® (ABS) FABS 20 GB HH ABS-GB20 A. Schulman GmbH
POLYMAN® (ABS) FABS 20 MW UV ABS-MD20 A. Schulman GmbH
POLYMAN® (ABS) FABS 30 GB ABS-GB30 A. Schulman GmbH
POLYMAN® (ABS) HH ABS A. Schulman GmbH
POLYMAN® (ABS) HH 2 ABS A. Schulman GmbH
POLYMAN® (ABS) HH 3 ABS A. Schulman GmbH
POLYMAN® (ABS) HH 3 D ABS A. Schulman GmbH
POLYMAN® (ABS) LC 145 ABS A. Schulman GmbH
POLYMAN® (ABS) LC 165 ABS A. Schulman GmbH
POLYMAN® (ABS) LC 185 A ABS A. Schulman GmbH
POLYMAN® (ABS) LP 126/2 GL ABS A. Schulman GmbH
POLYMAN® (ABS) LP 128/2 GL ABS A. Schulman GmbH
POLYMAN® (ABS) LP 137 A ABS A. Schulman GmbH
POLYMAN® (ABS) LP 299/2 GLA ABS A. Schulman GmbH
POLYMAN® (ABS) LP 330 ABS A. Schulman GmbH
POLYMAN® (ABS) LP 500 RCP ABS A. Schulman GmbH
POLYMAN® (ABS) LP 520 NT ABS A. Schulman GmbH
POLYMAN® (ABS) M/AQ ABS A. Schulman GmbH
POLYMAN® (ABS) M/AQ schwarz LE ABS A. Schulman GmbH
POLYMAN® (ABS) M/AQ WS 1,5 ABS A. Schulman GmbH
POLYMAN® (ABS) M/HI ABS A. Schulman GmbH
POLYMAN® (ABS) M/HI-A ABS A. Schulman GmbH
POLYMAN® (ABS) M/HI-G ABS A. Schulman GmbH
POLYMAN® (ABS) M/HI-W ABS A. Schulman GmbH
POLYMAN® (ABS) M/HI-W K1808 ABS A. Schulman GmbH
POLYMAN® (ABS) M/MI-A ABS A. Schulman GmbH
POLYMAN® (ABS) M/MI-A 40 ABS A. Schulman GmbH
POLYMAN® (ABS) M/MI-A 40 CA ABS A. Schulman GmbH
POLYMAN® (ABS) M/MI-A K1777 ABS A. Schulman GmbH
POLYMAN® (ABS) M/SHI ABS A. Schulman GmbH
POLYMAN® (ABS) M/TK ABS A. Schulman GmbH
POLYMAN® (ABS) M/TK-A ABS A. Schulman GmbH
POLYMAN® (ABS) M/TK-HH ABS A. Schulman GmbH
POLYMAN® (ABS) M/TK-HI ABS A. Schulman GmbH
POLYMAN® (PS) LP 600 NT ABS A. Schulman GmbH
POLYMAN® FABS 17 GF ABS-GF17 A. Schulman GmbH
POLYMAN® FABS 20 GF ABS-GF20 A. Schulman GmbH
SCHULABLEND® (ABS/PA) M/MK (ABS+PA6)... A. Schulman GmbH
SCHULABLEND® (ABS/PA) M/MK 20 GF (ABS+PA6)-GF20... A. Schulman GmbH
SCHULABLEND® (ABS/PA) M/MK 8 GF (ABS+PA6)-GF8 A. Schulman GmbH
SCHULABLEND® (ABS/PA) M/MK K2004 (ABS+PA6) A. Schulman GmbH
SCHULABLEND® (ABS/PA) M/MK NC 400 (ABS+PA6)-MD20 A. Schulman GmbH
SCHULABLEND® (ABS/PA) M/MK NC 800 (ABS+PA6)-MD20 A. Schulman GmbH
SCHULABLEND® (PC/ABS) M/MB 3 (ABS+PC)... A. Schulman GmbH
SCHULABLEND® (PC/ABS) M/MB 5 (ABS+PC)... A. Schulman GmbH
SCHULABLEND® (PC/ABS) M/MB 5 GF 20 (ABS+PC)-GF20... A. Schulman GmbH
SCHULABLEND® (PC/ABS) M/MB 5 GF 5 (ABS+PC)-GF5... A. Schulman GmbH
SCHULABLEND® (PC/ABS) M/MB 6 (ABS+PC)... A. Schulman GmbH
SCHULABLEND® (PC/ABS) M/MB 705 (ABS+PC) A. Schulman GmbH
SINKRAL® B 432/E ABS Polimeri Europa
SINKRAL® B 532/E ABS Polimeri Europa
SINKRAL® C 333/M2 ABS Polimeri Europa
SINKRAL® C 442 ABS Polimeri Europa
SINKRAL® D 232/M3 ABS Polimeri Europa
SINKRAL® E 332 ABS Polimeri Europa
SINKRAL® F 332 ABS Polimeri Europa
Terblend® N NG-02 (ABS+PA6)-GF8 BASF
Terblend® N NG-02 EF (ABS+PA6)-GF8 BASF
Terblend® N NG-02 UV (ABS+PA6)-GF8 BASF
Terblend® N NG-04 (ABS+PA6)-GF20 BASF
Terblend® N NG-06 (ABS+PA6)-GF30 BASF
Terblend® N NM-11 (ABS+PA6) BASF
Terblend® N NM-12 (ABS+PA6) BASF
Terblend® N NM-12 UV (ABS+PA6) BASF
Terblend® N NM-13 (ABS+PA6) BASF
Terblend® N NM-19 (ABS+PA6) BASF
Terblend® N NM-19 XP (ABS+PA6) BASF
Terblend® N NM-21 EF (ABS+PA6) BASF
Terblend® N NMX04 (ABS+PA6) BASF
Terluran® GP-22 ABS BASF
Terluran® GP-35 ABS BASF
Terluran® HD-15 ABS BASF
Terluran® HH-112 ABS BASF
Terluran® HH-112 Q 457 ABS BASF
Terluran® HI-10 ABS BASF
Terluran® SP-6 ABS BASF