Grade Name Family Producer
POLYLUX® (MABS) Typ C1 MABS-I A. Schulman GmbH
POLYLUX® (MABS) Typ C12 MABS A. Schulman GmbH
POLYLUX® (MABS) Typ C2 MABS-I A. Schulman GmbH
POLYLUX® (MABS) Typ C4 MABS-I A. Schulman GmbH
POLYLUX® (MABS) Typ C5 MABS-I A. Schulman GmbH
Terlux® 2802 HD MABS BASF
Terlux® 2802 TR MABS BASF
Terlux® 2812 HD MABS BASF
Terlux® 2812 TR MABS BASF
Terlux® 2822 HD MABS BASF