CAMPUSplastics | All PA610 grades
The international CAMPUS database offers datasheets of the following grades that are related to the polymer family: PA610.Please click on the grade of interest to generate a datasheet. You also may select a material by choosing an other polymer family or a specific producer. In addition you may select by any part of the grade name using the input box on the left.
| Grade Name | Family | Producer |
|---|---|---|
| Grilamid XE 3959 black 9992 | PA610 | EMS-GRIVORY | a unit of EMS-CHEMIE AG |
| Grilamid XE 3959 nat | PA610 | EMS-GRIVORY | a unit of EMS-CHEMIE AG |
| Grilamid XE 3974 black 9992 | PA610 | EMS-GRIVORY | a unit of EMS-CHEMIE AG |
| Grilamid XE 3974 nat | PA610 | EMS-GRIVORY | a unit of EMS-CHEMIE AG |
| Grilamid XE 3975 black 9992 | PA610 | EMS-GRIVORY | a unit of EMS-CHEMIE AG |
| Grilamid XE 3975 nat | PA610 | EMS-GRIVORY | a unit of EMS-CHEMIE AG |
| Grilamid XE 3976 black 9992 | PA610-GF30 | EMS-GRIVORY | a unit of EMS-CHEMIE AG |
| Grilamid XE 3976 nat | PA610-GF30 | EMS-GRIVORY | a unit of EMS-CHEMIE AG |
| Grilamid XE 4073 nat | PA610-GF30 | EMS-GRIVORY | a unit of EMS-CHEMIE AG |
| Grilamid XE 4104 black 9992 | PA610-GF40 | EMS-GRIVORY | a unit of EMS-CHEMIE AG |
| Grilamid XE 4104 nat | PA610-GF40 | EMS-GRIVORY | a unit of EMS-CHEMIE AG |
| Grilamid XE 4105 black 9992 | PA610-GF50 | EMS-GRIVORY | a unit of EMS-CHEMIE AG |
| Grilamid XE 4105 nat | PA610-GF50 | EMS-GRIVORY | a unit of EMS-CHEMIE AG |
| Grilamid XE 4128 black 9221 | PA610 | EMS-GRIVORY | a unit of EMS-CHEMIE AG |
| Grilamid XE 4129 black 9020 | PA610 | EMS-GRIVORY | a unit of EMS-CHEMIE AG |
| Technyl® eXten D 218 V30 | PA610-GF30 | Rhodia Polyamide Engineering Plastics |
| Technyl® eXten D 238 V30 | PA610-I-GF30 | Rhodia Polyamide Engineering Plastics |
| Technyl® eXten D 437P | PA610 | Rhodia Polyamide Engineering Plastics |
| Technyl® eXten D 458P | PA610-I | Rhodia Polyamide Engineering Plastics |
| Ultramid® S3K Balance | PA610 | BASF |
| VESTAMID Terra HS16 nc (nf) | (PA610+PA*) | Evonik Industries AG |
| VESTAMID Terra HS18 nc (nf) | (PA610+PA*) | Evonik Industries AG |
| VESTAMID Terra HS18-GF30 nc (nf) | (PA610+PA*)-GF30 | Evonik Industries AG |
| VESTAMID Terra HS22 nc (nf) | (PA610+PA*) | Evonik Industries AG |
| Zytel® RS3061HSL BK039A | PA610 | DuPont Engineering Polymers |
| Zytel® RS30G30HSL BK038A | PA610-GF30 | DuPont Engineering Polymers |
| Zytel® RS30G30L NC010 | PA610-GF30 | DuPont Engineering Polymers |
| Zytel® RS3261THSL BK041A | PA610-I | DuPont Engineering Polymers |
| Zytel® RS3261TL NC010 | PA610-I | DuPont Engineering Polymers |
| Zytel® RSLC3030 NC010 | PA610 | DuPont Engineering Polymers |
| Zytel® RSLC3060 NC010 | PA610 | DuPont Engineering Polymers |
| Zytel® RSLC3090 NC010 | PA610 | DuPont Engineering Polymers |