The international CAMPUS database offers datasheets of the following grades that are related to the polymer family: PA6T/6I.Please click on the grade of interest to generate a datasheet. You also may select a material by choosing an other polymer family or a specific producer. In addition you may select by any part of the grade name using the input box on the left.
| Grade Name | Family | Producer |
|---|---|---|
| Grivory HT1V-3 FWA black 9225 | PA6T/6I-GF30 | EMS-GRIVORY | a unit of EMS-CHEMIE AG |
| Grivory HT1V-3 FWA nat | PA6T/6I-GF30 | EMS-GRIVORY | a unit of EMS-CHEMIE AG |
| Grivory HT1V-3 HY black 9205 | PA6T/6I-GF30 | EMS-GRIVORY | a unit of EMS-CHEMIE AG |
| Grivory HT1V-4 FWA black 9225 | PA6T/6I-GF40 | EMS-GRIVORY | a unit of EMS-CHEMIE AG |
| Grivory HT1V-4 FWA nat | PA6T/6I-GF40 | EMS-GRIVORY | a unit of EMS-CHEMIE AG |
| Grivory HT1V-4 HY black 9205 | PA6T/6I-GF40 | EMS-GRIVORY | a unit of EMS-CHEMIE AG |
| Grivory HT1V-5 FWA black 9225 | PA6T/6I-GF50 | EMS-GRIVORY | a unit of EMS-CHEMIE AG |
| Grivory HT1V-5 FWA nat | PA6T/6I-GF50 | EMS-GRIVORY | a unit of EMS-CHEMIE AG |
| Grivory HT1V-5 HY black 9205 | PA6T/6I-GF50 | EMS-GRIVORY | a unit of EMS-CHEMIE AG |
| Grivory HT1V-6 FWA black 9225 | PA6T/6I-GF60 | EMS-GRIVORY | a unit of EMS-CHEMIE AG |
| Grivory HT1V-65H black 9205 | PA6T/6I-GF65 | EMS-GRIVORY | a unit of EMS-CHEMIE AG |
| Grivory HTM-4H1 | PA6T/6I-MD40 | EMS-GRIVORY | a unit of EMS-CHEMIE AG |
| Grivory HTV-3H1 black 9205 | PA6T/6I-GF30 | EMS-GRIVORY | a unit of EMS-CHEMIE AG |
| Grivory HTV-3H1 nat | PA6T/6I-GF30 | EMS-GRIVORY | a unit of EMS-CHEMIE AG |
| Grivory HTV-45H1 black 9205 | PA6T/6I-GF45 | EMS-GRIVORY | a unit of EMS-CHEMIE AG |
| Grivory HTV-4H1 black 9205 | PA6T/6I-GF40 | EMS-GRIVORY | a unit of EMS-CHEMIE AG |
| Grivory HTV-4H1 nat | PA6T/6I-GF40 | EMS-GRIVORY | a unit of EMS-CHEMIE AG |
| Grivory HTV-5H1 black 9205 | PA6T/6I-GF50 | EMS-GRIVORY | a unit of EMS-CHEMIE AG |
| Grivory HTV-5H1 nat | PA6T/6I-GF50 | EMS-GRIVORY | a unit of EMS-CHEMIE AG |
| Grivory HTV-6H1 black 9205 | PA6T/6I-GF60 | EMS-GRIVORY | a unit of EMS-CHEMIE AG |
| Grivory HTV-6H1 nat | PA6T/6I-GF60 | EMS-GRIVORY | a unit of EMS-CHEMIE AG |