The international CAMPUS database offers datasheets of the following grades that are related to the polymer family: PAIND/INDT.Please click on the grade of interest to generate a datasheet. You also may select a material by choosing an other polymer family or a specific producer. In addition you may select by any part of the grade name using the input box on the left.
| Grade Name | Family | Producer |
|---|---|---|
| TROGAMID BX7304 nc (nf) | (PAIND/INDT+PA612) | Evonik Industries AG |
| TROGAMID BX9724 blk (sw) | (PAIND/INDT+PA66)-GF40 | Evonik Industries AG |
| TROGAMID CX7323 nc (nf) | PAIND/INDT | Evonik Industries AG |
| TROGAMID CX9701 nc (nf) | PAIND/INDT | Evonik Industries AG |
| TROGAMID CX9704 | PAIND/INDT | Evonik Industries AG |
| TROGAMID CX9710 nc (nf) | PAIND/INDT | Evonik Industries AG |
| TROGAMID myCX | PAIND/INDT | Evonik Industries AG |
| TROGAMID T-GF35 nc (nf) | PAIND/INDT-GF35 | Evonik Industries AG |
| TROGAMID T5000 nc (nf) | PAIND/INDT | Evonik Industries AG |
| TROGAMID T5002 nc (nf) | PAIND/INDT | Evonik Industries AG |
| TROGAMID T5004 nc (nf) | PAIND/INDT | Evonik Industries AG |
| TROGAMID TX7389 nc (nf) | PAIND/INDT | Evonik Industries AG |