The international CAMPUS database offers datasheets of the following grades that are related to the polymer family: PE-HD.Please click on the grade of interest to generate a datasheet. You also may select a material by choosing an other polymer family or a specific producer. In addition you may select by any part of the grade name using the input box on the left.
| Grade Name | Family | Producer |
|---|---|---|
| ALTECH PE-HD A 2020/506 GF20 | (PE-HD)-GF20 | ALBIS Plastic GmbH |
| CELSTRAN PEHD-GF40-01 | (PE-HD)-GF40 | Ticona |
| CELSTRAN PEHD-GF60-01-US | (PE-HD)-GF60 | Ticona |
| GUR GHR 8020 | (PE-HD) | Ticona |
| GUR GHR 8110 | (PE-HD) | Ticona |
| POLYFLAM® RHD 5000 E | (PE-HD) FR | A. Schulman GmbH |
| RADILENE® R 70 IE 0 2060 C | (PE-HD) | RadiciPlastics |
| RADILENE® R 70 IE 0 5058 B | (PE-HD) | RadiciPlastics |