The international CAMPUS database offers datasheets of the following grades that are related to the polymer family: PEEK.Please click on the grade of interest to generate a datasheet. You also may select a material by choosing an other polymer family or a specific producer. In addition you may select by any part of the grade name using the input box on the left.
| Grade Name | Family | Producer |
|---|---|---|
| VESTAKEEP 2000 CF30 | PEEK-CF30 | Evonik Industries AG |
| VESTAKEEP 2000 FC30 | (PEEK+PTFE)-(CF+CD)20 | Evonik Industries AG |
| VESTAKEEP 2000 G | PEEK | Evonik Industries AG |
| VESTAKEEP 2000 GF30 | PEEK-GF30 | Evonik Industries AG |
| VESTAKEEP 3300 G | PEEK | Evonik Industries AG |
| VESTAKEEP 4000 CC20 | PEEK-MX | Evonik Industries AG |
| VESTAKEEP 4000 CF30 | PEEK-CF30 | Evonik Industries AG |
| VESTAKEEP 4000 FC30 | (PEEK+PTFE)-(CF+CD)20 | Evonik Industries AG |
| VESTAKEEP 4000 GF30 | PEEK-GF30 | Evonik Industries AG |
| VESTAKEEP L 4000 G | PEEK | Evonik Industries AG |