CAMPUSplastics | All PESU grades
The international CAMPUS® database offers datasheets of the following grades that are related to the polymer family: PESU.Please click on the grade of interest to generate a datasheet. You also may select a material by choosing an other polymer family or a specific producer. In addition you may select by any part of the grade name using the input box on the left.
| Grade Name | Family | Producer |
|---|---|---|
| Ultrason® E 1010 NAT | PESU | BASF |
| Ultrason® E 2010 C6 | PESU-CF30 | BASF |
| Ultrason® E 2010 G4 UN | PESU-GF20 | BASF |
| Ultrason® E 2010 G6 UN | PESU-GF30 | BASF |
| Ultrason® E 2010 NAT | PESU | BASF |
| Ultrason® E 2020 P | PESU | BASF |
| Ultrason® E 3010 NAT | PESU | BASF |
| Ultrason® E 6020 P | PESU | BASF |
| Ultrason® KR 4113 | (PESU+PTFE)-(CF+CD)30... | BASF |