The international CAMPUS database offers datasheets of the following grades that are related to the polymer family: PET.Please click on the grade of interest to generate a datasheet. You also may select a material by choosing an other polymer family or a specific producer. In addition you may select by any part of the grade name using the input box on the left.
| Grade Name | Family | Producer |
|---|---|---|
| Arnite® A-X07248 | PET-GF50 | DSM Engineering Plastics |
| Arnite® A-X07302 (AV2 390 XT-P) | PET-GF50 | DSM Engineering Plastics |
| Arnite® A02 306 | PET | DSM Engineering Plastics |
| Arnite® A04 900 | PET | DSM Engineering Plastics |
| Arnite® A06 101 | PET | DSM Engineering Plastics |
| Arnite® A06 300 | PET | DSM Engineering Plastics |
| Arnite® A06 700 | PET | DSM Engineering Plastics |
| Arnite® AV2 360 S | PET-GF33 FR(17) | DSM Engineering Plastics |
| Arnite® AV2 365 SN | PET-GF33 FR(17) | DSM Engineering Plastics |
| Arnite® AV2 370 /B | PET-GF35 | DSM Engineering Plastics |
| Arnite® AV2 370 HF | PET-GF35 | DSM Engineering Plastics |
| Arnite® AV2 370 XL | PET-GF35 | DSM Engineering Plastics |
| Arnite® AV2 370 XT (A-X05320) | PET-GF35 | DSM Engineering Plastics |
| Arnite® AV2 372 | PET-GF35 | DSM Engineering Plastics |
| Arnite® AV2 390 | PET-GF50 | DSM Engineering Plastics |
| Arnite® AV2 390 XL | PET-GF50 | DSM Engineering Plastics |
| Arnite® AV2 390 XT (A-X04961) | PET-GF50 | DSM Engineering Plastics |
| IMPET 2700 GV1/45 (Europe) | PET-GF45 | Ticona |
| IMPET 330R | PET-GF30 | Ticona |
| IMPET 340R | PET-GF45 | Ticona |
| IMPET 830R | PET-GF35 | Ticona |
| Pocan® DP T7140 LDS | (PET+PBT)-(MD+GF)44 | LANXESS Deutschland GmbH |
| Rynite® 408 NC010 | PET-I-GF30 | DuPont Engineering Polymers |
| Rynite® 415HP NC010 | PET-I-GF15 | DuPont Engineering Polymers |
| Rynite® 515CS BK575M | PET-GF15 | DuPont Engineering Polymers |
| Rynite® 530 NC010 | PET-GF30 | DuPont Engineering Polymers |
| Rynite® 530HTE BK503 | PET-GF30 | DuPont Engineering Polymers |
| Rynite® 540SUV BK544 | PET-GF40 | DuPont Engineering Polymers |
| Rynite® 545 NC010 | PET-GF45 | DuPont Engineering Polymers |
| Rynite® 555 NC010A | PET-GF55 | DuPont Engineering Polymers |
| Rynite® 625FD BK505 | PET-I-(MD+GF)25 | DuPont Engineering Polymers |
| Rynite® 815ER NC010 | PET-I-GF15 | DuPont Engineering Polymers |
| Rynite® 935 NC010 | PET-(MD+GF)35 | DuPont Engineering Polymers |
| Rynite® 935SUV BK593 | PET-(MD+GF)35 | DuPont Engineering Polymers |
| Rynite® 936CS NC011 | PET-(GX+GF)36 | DuPont Engineering Polymers |
| Rynite® 940 NC010 | PET-(GF+MD)40 | DuPont Engineering Polymers |
| Rynite® FR515 NC010 | PET-GF15 FR(17) | DuPont Engineering Polymers |
| Rynite® FR515CS GY906 | PET-GF15 FR(17) | DuPont Engineering Polymers |
| Rynite® FR530 NC010 | PET-GF30 FR(17) | DuPont Engineering Polymers |
| Rynite® FR530L NC010 | PET-GF30 FR(17) | DuPont Engineering Polymers |
| Rynite® FR531 NC010 | PET-(GF+X)38 FR(17) | DuPont Engineering Polymers |
| Rynite® FR543 NC010 | PET-GF43 FR(17) | DuPont Engineering Polymers |
| Rynite® FR815ER BK507 | PET-GF15 FR(17) | DuPont Engineering Polymers |
| Rynite® FR945 NC010 | PET-(MD+GF)45 FR(17) | DuPont Engineering Polymers |
| Rynite® GW520CS NC010 | PET-GF20 FR(16) | DuPont Engineering Polymers |
| Rynite® PCR108 BK515 | PET-I-(GF+MD)35 | DuPont Engineering Polymers |
| Rynite® RE15022 NC010 | PET-GF36 | DuPont Engineering Polymers |
| Rynite® RE15030 BK503 | PET-GF30 | DuPont Engineering Polymers |
| Rynite® RE15245 BK504 | PET-GF | DuPont Engineering Polymers |
| Rynite® RE19020 BK507 | PET-GF | DuPont Engineering Polymers |
| Rynite® RE19045 BK507 | PET-(GF+MD)46 FR(17) | DuPont Engineering Polymers |
| Rynite® RE19051 BK507 | PET-(GF+MD)40 FR(16) | DuPont Engineering Polymers |
| Rynite® RE19099 BK507 | PET-(GF+MD)35 FR(17) | DuPont Engineering Polymers |
| Rynite® RE5060 BK505 | PET-(GF+MD)35 | DuPont Engineering Polymers |
| Rynite® RE5231 BK533 | PET-(GF+MD)35 | DuPont Engineering Polymers |
| Rynite® RE5264 NC010 | PET-GF36 | DuPont Engineering Polymers |
| Rynite® RE5329 NC010 | PET-(GX+GF)36 | DuPont Engineering Polymers |
| Rynite® RE5333 NC010 | PET-GX | DuPont Engineering Polymers |
| Rynite® RE8000 BK575 | PET-I-MD | DuPont Engineering Polymers |
| Rynite® RE9078 NC010 | PET-(GF+MD)40 FR(16) | DuPont Engineering Polymers |
| Rynite® SST35 NC010 | PET-I-GF35 | DuPont Engineering Polymers |
| SCHULADUR® E FLF 3624 | PET-GF36 | A. Schulman GmbH |
| SCHULADUR® E GF 35 | PET-GF35 | A. Schulman GmbH |