View list of

CAMPUSplastics | All PP grades

The international CAMPUS database offers datasheets of the following grades that are related to the polymer family: PP.

Please click on the grade of interest to generate a datasheet. You also may select a material by choosing an other polymer family or a specific producer. In addition you may select by any part of the grade name using the input box on the left.

Grade Name Family Producer
ALCOM® PP 620/1 WT 1034-05 LB PP-MX... ALBIS Plastic GmbH
ALCOM® PP 620/1 WT 1301-04 LB PP-MX... ALBIS Plastic GmbH
ALCOM® PP 620/1 WT1433-05LB PP-MX... ALBIS Plastic GmbH
ALCOM® PP 620/10 GY 1464-04 MCF PP ALBIS Plastic GmbH
ALCOM® PP 620/2 SV1246-04MCO Silver PP ALBIS Plastic GmbH
ALCOM® PP 620/30 TCD1 PP... ALBIS Plastic GmbH
ALCOM® PP 620/4010 PTFE15 (PP+PTFE) ALBIS Plastic GmbH
ALCOM® PP 620/6 HGB PP-GB ALBIS Plastic GmbH
ALCOM® PP 620/8 GF30 PTFE15 (PP+PTFE)-GF30 ALBIS Plastic GmbH
ALCOM® PP 69/0702 EC PP-CD ALBIS Plastic GmbH
ALCOM® PP 69/0703 EC PP-CD ALBIS Plastic GmbH
ALCOM® PP620/10 SV1435-05MCF PP ALBIS Plastic GmbH
ALTECH PP-B A 1000/120 UV PP ALBIS Plastic GmbH
ALTECH PP-B A 1000/310 IM PP-I ALBIS Plastic GmbH
ALTECH PP-B A 1000/540 FR PP FR ALBIS Plastic GmbH
ALTECH PP-B A 1000/546 FR PP FR ALBIS Plastic GmbH
ALTECH PP-B A 1000/587 IM PP-I ALBIS Plastic GmbH
ALTECH PP-B A 2015/550 GF15 CP PP-GF15 ALBIS Plastic GmbH
ALTECH PP-B A 2020/150 GF20 CP PP-GF20 ALBIS Plastic GmbH
ALTECH PP-B A 2030/150 GF30 CP PP-GF30 ALBIS Plastic GmbH
ALTECH PP-B A 2040/150 GF40 CP PP-GF40 ALBIS Plastic GmbH
ALTECH PP-B A 3030/500 GB30 PP-GB30 ALBIS Plastic GmbH
ALTECH PP-B A 4430/100 MR30 PP-(Z+T)30 ALBIS Plastic GmbH
ALTECH PP-B A 4430/120 MR30 UV PP-(Z+T)30 ALBIS Plastic GmbH
ALTECH PP-B A 4815/100 MR15 PP-MX15 ALBIS Plastic GmbH
ALTECH PP-B A 4920/100 MR20 PP-T20 ALBIS Plastic GmbH
ALTECH PP-B A 4925/500 MR25 PP-T25 ALBIS Plastic GmbH
ALTECH PP-B A 4930/507 MR30 PP-T30 ALBIS Plastic GmbH
ALTECH PP-B A 4930/520 MR30 UV PP-T30 ALBIS Plastic GmbH
ALTECH PP-B A 4940/600 MR40 PP-T40 ALBIS Plastic GmbH
ALTECH PP-B C 2015/550 GF15 CP PP-GF15 ALBIS Plastic GmbH
ALTECH PP-B C 2030/550 GF30 CP PP-GF30 ALBIS Plastic GmbH
ALTECH PP-B C 2040/550 GF40 CP PP-GF40 ALBIS Plastic GmbH
ALTECH PP-B C 4920/570 MR20 PP-T20 ALBIS Plastic GmbH
ALTECH PP-B FC 2030/150 GF30 CP PP-GF30 ALBIS Plastic GmbH
ALTECH PP-H A 1000/100 DS PP ALBIS Plastic GmbH
ALTECH PP-H A 1000/149 FR PP FR ALBIS Plastic GmbH
ALTECH PP-H A 1000/249 FR PP FR ALBIS Plastic GmbH
ALTECH PP-H A 1000/576 PP ALBIS Plastic GmbH
ALTECH PP-H A 1000/620 UV PP ALBIS Plastic GmbH
ALTECH PP-H A 2020/100 GF20 PP-GF20 ALBIS Plastic GmbH
ALTECH PP-H A 2020/159 GF20 CP PP-GF20 ALBIS Plastic GmbH
ALTECH PP-H A 2020/750 GF20 CP PP-GF20 ALBIS Plastic GmbH
ALTECH PP-H A 2030/100 BK0002-00 PP-GF30 ALBIS Plastic GmbH
ALTECH PP-H A 2030/156 GF30 CP PP-GF30 ALBIS Plastic GmbH
ALTECH PP-H A 2030/157 GF30 CP PP-GF30 ALBIS Plastic GmbH
ALTECH PP-H A 2030/158 GF30 CP PP-GF30 ALBIS Plastic GmbH
ALTECH PP-H A 2030/159 GF30 CP PP-GF30 ALBIS Plastic GmbH
ALTECH PP-H A 2030/169 GF30 CP PP-GF30 ALBIS Plastic GmbH
ALTECH PP-H A 2030/250 GF30 CP PP-GF30 ALBIS Plastic GmbH
ALTECH PP-H A 2030/252 GF30 UV CP PP-GF30 ALBIS Plastic GmbH
ALTECH PP-H A 2030/652 GF30 UV PP-GF30 ALBIS Plastic GmbH
ALTECH PP-H A 2030/750 GF30 CP PP-GF30 ALBIS Plastic GmbH
ALTECH PP-H A 2035/500 GF35 PP-GF35 ALBIS Plastic GmbH
ALTECH PP-H A 2040/159 GF40 CP PP-GF40 ALBIS Plastic GmbH
ALTECH PP-H A 2040/652 GF 40 UV CP PP-GF40 ALBIS Plastic GmbH
ALTECH PP-H A 3020/100 GB20 PP-GB20 ALBIS Plastic GmbH
ALTECH PP-H A 3020/500 GB20 PP-GB20 ALBIS Plastic GmbH
ALTECH PP-H A 3030/100 GB30 PP-GB30 ALBIS Plastic GmbH
ALTECH PP-H A 3030/108 GB30 PP-GB30 ALBIS Plastic GmbH
ALTECH PP-H A 4818/100 MR18 DS PP-Z18 ALBIS Plastic GmbH
ALTECH PP-H A 4907/500 MR07 PP-T7 ALBIS Plastic GmbH
ALTECH PP-H A 4910/620 MR10 UV PP-T10 ALBIS Plastic GmbH
ALTECH PP-H A 4920/106 MR20 PP-T20 ALBIS Plastic GmbH
ALTECH PP-H A 4920/107 MR20 PP-T20 ALBIS Plastic GmbH
ALTECH PP-H A 4920/109 MR20 PP-T20 ALBIS Plastic GmbH
ALTECH PP-H A 4920/170 MR20 PP-T20 ALBIS Plastic GmbH
ALTECH PP-H A 4920/178 MR20 PP-T20 ALBIS Plastic GmbH
ALTECH PP-H A 4920/500 MR20 PP-T20 ALBIS Plastic GmbH
ALTECH PP-H A 4920/520 MR20 UV PP-T20 ALBIS Plastic GmbH
ALTECH PP-H A 4925/500 MR25 PP-MX25 ALBIS Plastic GmbH
ALTECH PP-H A 4930/100 MR30 PP-T30 ALBIS Plastic GmbH
ALTECH PP-H A 4930/106 MR30 PP-T30 ALBIS Plastic GmbH
ALTECH PP-H A 4930/506 MR30 PP-T30 ALBIS Plastic GmbH
ALTECH PP-H A 4940/100 MR40 PP-T40 ALBIS Plastic GmbH
ALTECH PP-H A 4940/106 MR40 PP-T40 ALBIS Plastic GmbH
ALTECH PP-H C 2030/550 GF30 CP PP-GF30 ALBIS Plastic GmbH
ALTECH PP-H C 2030/567 GF30 PP-GF30 ALBIS Plastic GmbH
ALTECH PP-H C 4920/570 MR20 PP-T20 ALBIS Plastic GmbH
ALTECH PP-H C 4940/570 MR40 PP-T40 ALBIS Plastic GmbH
ALTECH PP-H FC 4920/100 MR20 PP-T20 ALBIS Plastic GmbH
CELSTRAN +PP-GF30-04CN02/10 PP-GF30 Ticona
CELSTRAN +PP-GF30-05CN01/10 PP-GF30 Ticona
CELSTRAN +PP-GF40-04CN03 PP-GF40 Ticona
CELSTRAN +PP-GF40-04CN03/10 PP-GF40 Ticona
CELSTRAN +PP-GF40-04CN15/10 PP-GF40 Ticona
CELSTRAN +PP-GF45-05X551/1X PP-GF45 Ticona
CELSTRAN +PP-GF60-04CN15/10 PP-GF60 Ticona
CELSTRAN PP-GF25-0403 P10/10 PP-GF25 Ticona
CELSTRAN PP-GF30-02 PP-GF30 Ticona
CELSTRAN PP-GF30-03 PP-GF30 Ticona
CELSTRAN PP-GF30-04 PP-GF30 Ticona
CELSTRAN PP-GF30-0403 P10 PP-GF30 Ticona
CELSTRAN PP-GF30-0403 P10/10 PP-GF30 Ticona
CELSTRAN PP-GF30-0405 P10/10 PP-GF30 Ticona
CELSTRAN PP-GF30-0453 P10/10 PP-GF30 Ticona
CELSTRAN PP-GF30-05 PP-GF30 Ticona
CELSTRAN PP-GF30-0501 P8/13 PP-GF30 Ticona
CELSTRAN PP-GF30-0501P10 PP-GF30 Ticona
CELSTRAN PP-GF30-0501P10/13 PP-GF30 Ticona
CELSTRAN PP-GF30-10 PP-GF30 Ticona
CELSTRAN PP-GF40-02 PP-GF40 Ticona
CELSTRAN PP-GF40-03 PP-GF40 Ticona
CELSTRAN PP-GF40-04 PP-GF40 Ticona
CELSTRAN PP-GF40-0405 P10/10 PP-GF40 Ticona
CELSTRAN PP-GF40-0414 P10 PP-GF40 Ticona
CELSTRAN PP-GF40-0414 P7/10 PP-GF40 Ticona
CELSTRAN PP-GF40-0414P10/10 PP-GF40 Ticona
CELSTRAN PP-GF40-05 PP-GF40 Ticona
CELSTRAN PP-GF40-0501 P10/13 PP-GF40 Ticona
CELSTRAN PP-GF40-10 PP-GF40 Ticona
CELSTRAN PP-GF45M15-04CN15/10 PP-(GF+MF)60 Ticona
CELSTRAN PP-GF50-02 PP-GF50 Ticona
CELSTRAN PP-GF50-03 PP-GF50 Ticona
CELSTRAN PP-GF50-0403 P10 PP-GF50 Ticona
CELSTRAN PP-GF50-0403P10/10 PP-GF50 Ticona
CELSTRAN PP-GF50-0405P10/10 PP-GF50 Ticona
CELSTRAN PP-GF50-0453P10/10 PP-GF50 Ticona
CELSTRAN PP-GF50-0455P10/10 PP-GF50 Ticona
CELSTRAN PP-GF50-0458 P10/10 PP-GF50 Ticona
CELSTRAN PP-GF50-10 PP-GF50 Ticona
COMPEL PP-GF30-04 PP Ticona
POLYFLAM® RIPP 3125 PP-T25 FR A. Schulman GmbH
POLYFLAM® RIPP 3125 CS1 PP-T25 FR A. Schulman GmbH
POLYFLAM® RIPP 3625 CS1 PP-GF25 FR A. Schulman GmbH
POLYFLAM® RIPP 374 ND CS1 PP-T20 FR A. Schulman GmbH
POLYFLAM® RIPP 490 PP FR A. Schulman GmbH
POLYFLAM® RIPP 490 E CS1 PP FR A. Schulman GmbH
POLYFLAM® RIPP 510 D PP FR A. Schulman GmbH
POLYFLAM® RIPP 510 DF PP FR A. Schulman GmbH
POLYFLAM® RIPP 5440 PP FR A. Schulman GmbH
POLYFLAM® RPP 2000 PP-GF25 FR A. Schulman GmbH
POLYFLAM® RPP 2000 E PP-GF25 FR A. Schulman GmbH
POLYFLAM® RPP 2000 S PP-GF25 FR A. Schulman GmbH
POLYFLAM® RPP 2120 PP-T20 FR A. Schulman GmbH
POLYFLAM® RPP 3130 CS1 PP-T30 FR A. Schulman GmbH
POLYFLAM® RPP 3225 CS1 PP-GF25 FR A. Schulman GmbH
POLYFLAM® RPP 3230 CS1 PP-GF30 FR A. Schulman GmbH
POLYFLAM® RPP 374 ND CS1 PP-T20 FR A. Schulman GmbH
POLYFLAM® RPP 374 ND CS1 5V PP-T20 FR A. Schulman GmbH
POLYFLAM® RPP 4225 CS1 PP-GF25 FR A. Schulman GmbH
POLYFLAM® RPP 490 CS1 PP FR A. Schulman GmbH
POLYFLAM® RPP 500 D PP FR A. Schulman GmbH
POLYFLAM® RPP 500 DE PP FR A. Schulman GmbH
POLYFLAM® RPP 500 DF PP FR A. Schulman GmbH
POLYFLAM® RPP 60335 CS1 5V PP-GF25 FR A. Schulman GmbH
POLYFORT® AFP 2934 PP-I A. Schulman GmbH
POLYFORT® AFP 2936 schwarz PP A. Schulman GmbH
POLYFORT® AFP 3300 PP-I A. Schulman GmbH
POLYFORT® AFP 3306 Rezyklat PP-I A. Schulman GmbH
POLYFORT® AFP 3318 PP-I-T20 A. Schulman GmbH
POLYFORT® FIP 20 M K1033 PP-MD20 A. Schulman GmbH
POLYFORT® FIP 20 MA K1469 PP-MD20 A. Schulman GmbH
POLYFORT® FIP 40 MA K1544 PP-MD40 A. Schulman GmbH
POLYFORT® FIPP 10 T PP-T10 A. Schulman GmbH
POLYFORT® FIPP 15 M HSR 3329 PP-MD15 A. Schulman GmbH
POLYFORT® FIPP 15 M HSR K1757 PP-MD15 A. Schulman GmbH
POLYFORT® FIPP 20 M HSR 3329 PP-MD20 A. Schulman GmbH
POLYFORT® FIPP 20 T PP-T20 A. Schulman GmbH
POLYFORT® FIPP 20 T LE K1731 PP-T20 A. Schulman GmbH
POLYFORT® FIPP 20 T LE K1756 PP-T20 A. Schulman GmbH
POLYFORT® FIPP 20 T LE K1832 PP-T20 A. Schulman GmbH
POLYFORT® FIPP 20 TSP UVA/2 PP-T20 A. Schulman GmbH
POLYFORT® FIPP 30 GFC PP-GF30 A. Schulman GmbH
POLYFORT® FIPP 30 T K1005 PP-T30 A. Schulman GmbH
POLYFORT® FIPP 30 TF PP-T30 A. Schulman GmbH
POLYFORT® FIPP 65/10 BSGF PP-(Z+GF)75 A. Schulman GmbH
POLYFORT® FIPP 70/10 MGF PP-(MD+GF)80 A. Schulman GmbH
POLYFORT® FIPP 75 M PP-MD75 A. Schulman GmbH
POLYFORT® FIPP 80/5 MGF PP-(MD+GF)80 A. Schulman GmbH
POLYFORT® FIPP MKF 4025 PP-I-GF10 A. Schulman GmbH
POLYFORT® FIPP XSR 1020 PP-MD20 A. Schulman GmbH
POLYFORT® FIPP XSR 5000 PP A. Schulman GmbH
POLYFORT® FPP 10 T WLB PP-T10 A. Schulman GmbH
POLYFORT® FPP 20 GB PP-GB20 A. Schulman GmbH
POLYFORT® FPP 20 GF PP-GF20 A. Schulman GmbH
POLYFORT® FPP 20 GFC PP-GF20 A. Schulman GmbH
POLYFORT® FPP 20 GFC K1400 PP-GF20 A. Schulman GmbH
POLYFORT® FPP 20 GFC SHH PP-GF20 A. Schulman GmbH
POLYFORT® FPP 20 GFC SHH LW PP-GF20 A. Schulman GmbH
POLYFORT® FPP 20 GFM HI PP-I-GF20 A. Schulman GmbH
POLYFORT® FPP 20 GFM HI HH PP-I-GF20 A. Schulman GmbH
POLYFORT® FPP 20 T PP-T20 A. Schulman GmbH
POLYFORT® FPP 20 T K1534 natur PP-T20 A. Schulman GmbH
POLYFORT® FPP 20 T K1639 PP-T20 A. Schulman GmbH
POLYFORT® FPP 20 T K1751 PP-T20 A. Schulman GmbH
POLYFORT® FPP 20 T K1751 Mischung PP-T20 A. Schulman GmbH
POLYFORT® FPP 20 T SHH LW PP-T20 A. Schulman GmbH
POLYFORT® FPP 20 T WLB PP-T20 A. Schulman GmbH
POLYFORT® FPP 20 TF WLB PP-T20 A. Schulman GmbH
POLYFORT® FPP 20/10 GFM PP-GF30 A. Schulman GmbH
POLYFORT® FPP 22 T K1093 PP-T22 A. Schulman GmbH
POLYFORT® FPP 22 T LE K1684 PP-T22 A. Schulman GmbH
POLYFORT® FPP 30 GF PP-GF30 A. Schulman GmbH
POLYFORT® FPP 30 GFC PP-GF30 A. Schulman GmbH
POLYFORT® FPP 30 GFC HI PP-I-GF30 A. Schulman GmbH
POLYFORT® FPP 30 GFC K1079 PP-GF30 A. Schulman GmbH
POLYFORT® FPP 30 GFC-F WLB PP-GF30 A. Schulman GmbH
POLYFORT® FPP 30 T SHH REC PP-T30 A. Schulman GmbH
POLYFORT® FPP 30 T UV LE PP-T30 A. Schulman GmbH
POLYFORT® FPP 30/10 GBGF PP-(GF+GB)40 A. Schulman GmbH
POLYFORT® FPP 38 T K1419 V PP-T38 A. Schulman GmbH
POLYFORT® FPP 38 T K1785 PP-T38 A. Schulman GmbH
POLYFORT® FPP 40 GFC PP-GF40 A. Schulman GmbH
POLYFORT® FPP 40 GFC HI PP-I-GF40 A. Schulman GmbH
POLYFORT® FPP 40 GFC HI CS1 K1875 PP-I-GF40 A. Schulman GmbH
POLYFORT® FPP 40 GFC LE PP-GF40 A. Schulman GmbH
POLYFORT® FPP 40 GM PP-K40 A. Schulman GmbH
POLYFORT® FPP 40 K PP-K40 A. Schulman GmbH
POLYFORT® FPP 40 T PP-T40 A. Schulman GmbH
POLYFORT® FPP 40 T K1442 PP-T40 A. Schulman GmbH
POLYFORT® FPP 40 T LE K1858 PP-T40 A. Schulman GmbH
POLYFORT® FPP 40 T REC PP-T40 A. Schulman GmbH
POLYFORT® FPP 40 T WLB PP-T40 A. Schulman GmbH
POLYFORT® FPP 70 BS PP-Z70 A. Schulman GmbH
POLYFORT® FPP 75 M schwarz PP-MD75 A. Schulman GmbH
POLYFORT® FPP FX 2020 E PP-K40 A. Schulman GmbH
Procom 1111 H PP ALBIS Plastic GmbH
Procom 1111 L TA 8 PP-T40 ALBIS Plastic GmbH
SCHULATEC® PP LGF 30 H PP-GF30 A. Schulman GmbH
SCHULATEC® PP LGF 40 H PP-GF40 A. Schulman GmbH
SCHULATEC® PP LGF 50 H PP-GF50 A. Schulman GmbH
SCHULATEC® PP LGF 50 HP PP-GF50 A. Schulman GmbH
SCHULATEC® PP LGF 60 H PP-GF60 A. Schulman GmbH