Grade Name Family Producer
CELSTRAN PPS-AF35-01-US PPS-RF35 Ticona
CELSTRAN PPS-GF30-01 PPS-GF30 Ticona
CELSTRAN PPS-GF40-01 PPS-GF40 Ticona
CELSTRAN PPS-GF50-01-US PPS-GF50 Ticona
CELSTRAN PPS-SF6-01 AF3005 Natural PPS... Ticona
FORTRON 0203 PPS Ticona
FORTRON 0203HS PPS Ticona
FORTRON 0205 PPS Ticona
FORTRON 0205B4/20µm PPS Ticona
FORTRON 0214 PPS Ticona
FORTRON 0300 PPS Ticona
FORTRON 0309 PPS Ticona
FORTRON 0317 PPS Ticona
FORTRON 0320 PPS Ticona
FORTRON 1115L0 PPS-GF15 Ticona
FORTRON 1120L4 PPS-GF20 Ticona
FORTRON 1130L0 PPS-GF30 Ticona
FORTRON 1130L4 PPS-GF30 Ticona
FORTRON 1131L4 ITT PPS-GF30 Ticona
FORTRON 1140E7 PPS-GF40 Ticona
FORTRON 1140L0 PPS-GF40 Ticona
FORTRON 1140L4 PPS-GF40 Ticona
FORTRON 1140L6 PPS-GF40 Ticona
FORTRON 1140L7 PPS-GF40 Ticona
FORTRON 1140LC6 PPS-GF40 Ticona
FORTRON 1141L4 PPS-GF40 Ticona
FORTRON 1200L1 PPS Ticona
FORTRON 1342L4 PPS-GF40 Ticona
FORTRON 4184L4 PPS-(GF+MD)53 Ticona
FORTRON 4184L6 PPS-(GF+MD)53 Ticona
FORTRON 4332L6 PPS Ticona
FORTRON 4665B6 PPS-(GF+MD)65 Ticona
FORTRON 6160B4 PPS-(GF+MD)60 Ticona
FORTRON 6162A7 PPS-(GF+MD) Ticona
FORTRON 6165A4 PPS-(GF+MD)65 Ticona
FORTRON 6165A6 PPS-(GF+MD)65 Ticona
FORTRON 6341L4 PPS-GF40 Ticona
FORTRON 6345L4 PPS-GF30 Ticona
FORTRON 6450A6 PPS-(GF+MD)51 Ticona
FORTRON 6850L6 PPS-(GF+MD)50 Ticona
FORTRON FX4330T7 PPS-GF30 Ticona
FORTRON FX4382T1 PPS Ticona
FORTRON MT9115L0 DW PPS-GF15 Ticona
FORTRON MT9120L4 PPS-GF20 Ticona
FORTRON MT9140L4 PPS-GF40 Ticona
FORTRON MT9140L6 PPS-GF40 Ticona
FORTRON MT9141L4 DW PPS-GF40 Ticona
FORTRON MT9203HS PPS Ticona
FORTRON MT9205C4 PPS Ticona
FORTRON MT9320C0 PPS Ticona
TEDUR L 9107-1 9902 Black PPS-GF40 ALBIS Plastic GmbH
TEDUR L 9107-1 Natural Color PPS-GF40 ALBIS Plastic GmbH
TEDUR L 9200-1 9901 Black PPS-(GF+MF(x))60 ALBIS Plastic GmbH
TEDUR L 9200-1 Natural Color PPS-(GF+MF(x))60 ALBIS Plastic GmbH
TEDUR L 9217-1 S BK9901 Black PPS-(GF+MF(x))65 ALBIS Plastic GmbH
TEDUR L 9300-1 9902 Black PPS-(GF+GB)40 ALBIS Plastic GmbH
TEDUR L 9310-4 9902 Black PPS-(MX+GB) ALBIS Plastic GmbH
TEDUR L 9400-1 9901 Black PPS-CF15 ALBIS Plastic GmbH
TEDUR L 9413-1 9901 Black (PPS+PTFE)-CF ALBIS Plastic GmbH
TEDUR L 9510-1 9901 Black PPS-GF40 ALBIS Plastic GmbH
TEDUR L 9510-1 Natural Color PPS-GF40 ALBIS Plastic GmbH
TEDUR L 9510-1 S BK9901 Black PPS-GF40 ALBIS Plastic GmbH
TEDUR L 9510-1 S NC0001-00 Natural PPS-GF40 ALBIS Plastic GmbH
TEDUR L 9510-5 BK0002-00 Black PPS-GF40 ALBIS Plastic GmbH
TEDUR L 9510-5 NC PPS-GF40 ALBIS Plastic GmbH
TEDUR L 9560 9901 Black PPS-MX50 ALBIS Plastic GmbH
TEDUR L 9560 S BK9901 Black PPS-MX50 ALBIS Plastic GmbH
TEDUR R 9519 9901 Black PPS ALBIS Plastic GmbH
TEDUR R 9529 9901 Black PPS ALBIS Plastic GmbH
VECTRA V143XL (LCP+PPS)... Ticona