View list of

CAMPUSplastics | All ALBIS Plastic GmbH grades

The international CAMPUS® database offers datasheets of the following materials from producer: ALBIS Plastic GmbH.

Please click on the grade of interest to generate a datasheet. You also may select a material by choosing an other producer or a specific polymer family. In addition you may select by any part of the grade name using the input box on the left.

Grade Name Family Producer
ALCOM PA12 920/30.4 TCD1 PA12-Z ALBIS Plastic GmbH
ALCOM® ABS 530/12 SI1 ABS ALBIS Plastic GmbH
ALCOM® ABS 530/22 SV 1287-04 MCS ABS ALBIS Plastic GmbH
ALCOM® ABS 530/22 UV GY1039-07MCS ABS ALBIS Plastic GmbH
ALCOM® ABS 530/23 HGB ABS-GB ALBIS Plastic GmbH
ALCOM® ABS 530/29 SV 1217-04 MCO ABS ALBIS Plastic GmbH
ALCOM® ABS 530/29 SV 1245-05 MCF ABS ALBIS Plastic GmbH
ALCOM® ABS 530/29 SV 31-753 MCF ABS ALBIS Plastic GmbH
ALCOM® ABS 530/29 SV1462-06MCO ABS ALBIS Plastic GmbH
ALCOM® ABS 530/3 GY 31-749 MCF ABS ALBIS Plastic GmbH
ALCOM® ABS 530/3 SV 31-745 MCF ABS ALBIS Plastic GmbH
ALCOM® ABS 530/3 SV 31-748 MCS ABS ALBIS Plastic GmbH
ALCOM® ABS 530/3.1 CF ABS-CF ALBIS Plastic GmbH
ALCOM® ABS 530/36 SV 1031-04 MCF ABS ALBIS Plastic GmbH
ALCOM® ASA 540/7 SV1104-03 MCO ASA ALBIS Plastic GmbH
ALCOM® ASA 540/7 UV GY1385-05 MCF ASA ALBIS Plastic GmbH
ALCOM® ASA 540/7 UV SV1490-05MCF ASA ALBIS Plastic GmbH
ALCOM® ASA 540/8 UV SV1034-04MCF ASA ALBIS Plastic GmbH
ALCOM® ASA 540/9 PTFE10 (ASA+PTFE) ALBIS Plastic GmbH
ALCOM® ASA+PC 540/5 UV MCF (ASA+PC) ALBIS Plastic GmbH
ALCOM® ASA/PC 540/5 UV SV1290-04MCF (ASA+PC) ALBIS Plastic GmbH
ALCOM® AWL 10 WT31-943LB ABS ALBIS Plastic GmbH
ALCOM® AWL 15/1 GY1084-05LB ABS-Z15 ALBIS Plastic GmbH
ALCOM® AWL 15/1 UV WT1471-04LB ABS-Z15 ALBIS Plastic GmbH
ALCOM® AWL 15/1 WT1384-04LB ABS-Z15 ALBIS Plastic GmbH
ALCOM® AWL 15/1 WT31-956LB ABS-Z15 ALBIS Plastic GmbH
ALCOM® MABS 560/1 SV 1214-04 MCF ABS ALBIS Plastic GmbH
ALCOM® PA46 920/1 PTFE15 (PA46+PTFE) ALBIS Plastic GmbH
ALCOM® PA6 900/1 CF10 GF25 IM PA6-I-(GF+CF)35 ALBIS Plastic GmbH
ALCOM® PA6 900/1 GF10 GB20 PA6-(GF+GB)30 ALBIS Plastic GmbH
ALCOM® PA6 900/1 GF10 MR20 PA6-(GF+MX)30 ALBIS Plastic GmbH
ALCOM® PA6 900/1 GF10 MR30 PA6-(GF+MX)40 ALBIS Plastic GmbH
ALCOM® PA6 900/1 GF15 GB15 PA6-(GF+GB)30 ALBIS Plastic GmbH
ALCOM® PA6 900/1 GF15 MR25 PA6-(GF+MX)40 ALBIS Plastic GmbH
ALCOM® PA6 900/1 GF15 MR25 UV PA6-(GF+MX)40 ALBIS Plastic GmbH
ALCOM® PA6 900/1 GF20 MR25 PA6-(GF+MX)45 ALBIS Plastic GmbH
ALCOM® PA6 900/1 GF30 MO2 PA6-GF... ALBIS Plastic GmbH
ALCOM® PA6 900/1 GF30 PTFE15 Si2 (PA6+PTFE)-GF... ALBIS Plastic GmbH
ALCOM® PA6 900/1 GF5 GB25 PA6-(GF+GB)30 ALBIS Plastic GmbH
ALCOM® PA6 900/1 MO1 PA6... ALBIS Plastic GmbH
ALCOM® PA6 900/1 PTFE10 IM (PA6+PTFE)-I ALBIS Plastic GmbH
ALCOM® PA6 900/1 Si3 PA6... ALBIS Plastic GmbH
ALCOM® PA6 900/11 GF10 MR20 PA6-I-(GF+MX)30 ALBIS Plastic GmbH
ALCOM® PA6 900/11 GF10 MR20 MCF PA6-(GF+MX)30 ALBIS Plastic GmbH
ALCOM® PA6 900/11 GF30 RD1303-06MCF PA6-GF30 ALBIS Plastic GmbH
ALCOM® PA6 900/11 GF30 SV 12-778MCF PA6-GF30 ALBIS Plastic GmbH
ALCOM® PA6 900/1GF30WT1165-10LB PA46-GF30... ALBIS Plastic GmbH
ALCOM® PA6 900/30.1 TCE10 PA6... ALBIS Plastic GmbH
ALCOM® PA6 900/7 GF15 PTFE10 (PA6+PTFE)-GF15 ALBIS Plastic GmbH
ALCOM® PA6 900/8 GF10 MR20 PA6-(GF+MX)30 ALBIS Plastic GmbH
ALCOM® PA6 900/8 GF10 MR20 IM PA6-I-(GF+MX)30 ALBIS Plastic GmbH
ALCOM® PA6 900/8 SV 1403-04 MCF PA6 ALBIS Plastic GmbH
ALCOM® PA6 99/0701 EC PA6-CD ALBIS Plastic GmbH
ALCOM® PA6/6T GF25 PTFE15 (PA6/6T+PTFE)-GF25 ALBIS Plastic GmbH
ALCOM® PA66 910/1 AR10 CF10 PA66-(CF+RF) ALBIS Plastic GmbH
ALCOM® PA66 910/1 AR15 PTFE10 (PA66+PTFE)-RF ALBIS Plastic GmbH
ALCOM® PA66 910/1 AR20 PA66-RF ALBIS Plastic GmbH
ALCOM® PA66 910/1 GB30 MO2 PA66-GB... ALBIS Plastic GmbH
ALCOM® PA66 910/1 GF15 GB25 PA66-(GF+GB)40 ALBIS Plastic GmbH
ALCOM® PA66 910/1 GF15 MR25 PA66-(GF+MX)40 ALBIS Plastic GmbH
ALCOM® PA66 910/1 GF15 PTFE10 (PA66+PTFE)-GF15 ALBIS Plastic GmbH
ALCOM® PA66 910/1 GF15 PTFE18 Si2 (PA66+PTFE)-GF... ALBIS Plastic GmbH
ALCOM® PA66 910/1 GF20 GB10 PA66-(GF+GB)30 ALBIS Plastic GmbH
ALCOM® PA66 910/1 GF20 GB10 PTFE10 (PA66+PTFE)-(GF+GB)30 ALBIS Plastic GmbH
ALCOM® PA66 910/1 GF30 MO2 PA66-GF... ALBIS Plastic GmbH
ALCOM® PA66 910/1 GF30 PTFE10 Si2 (PA66+PTFE)-GF... ALBIS Plastic GmbH
ALCOM® PA66 910/1 GF30 PTFE15 (PA66+PTFE)-GF30 ALBIS Plastic GmbH
ALCOM® PA66 910/1 GF30 PTFE15 Si2 (PA66+PTFE)-GF... ALBIS Plastic GmbH
ALCOM® PA66 910/1 GF30 PTFE20 (PA66+PTFE)-GF30 ALBIS Plastic GmbH
ALCOM® PA66 910/1 MO1 PA66... ALBIS Plastic GmbH
ALCOM® PA66 910/1 MO2 PA66... ALBIS Plastic GmbH
ALCOM® PA66 910/1 PTFE20 (PA66+PTFE) ALBIS Plastic GmbH
ALCOM® PA66 910/1 SV 1057-03 MCF PA66 ALBIS Plastic GmbH
ALCOM® PA66 910/1 UV GY1187-06MCF PA66 ALBIS Plastic GmbH
ALCOM® PA66 910/1.1 AR10 CF10 PA66-(CF+RF) ALBIS Plastic GmbH
ALCOM® PA66 910/1.1 CF10 PA66-CF ALBIS Plastic GmbH
ALCOM® PA66 910/1.1 CF10 GF10 IM PA66-I-(CF+GF)20 ALBIS Plastic GmbH
ALCOM® PA66 910/1.1 CF10 GF20 PA66-(CF+GF)30 ALBIS Plastic GmbH
ALCOM® PA66 910/1.1 CF10 PTFE10 (PA66+PTFE)-CF ALBIS Plastic GmbH
ALCOM® PA66 910/1.1 CF15 PA66-CF ALBIS Plastic GmbH
ALCOM® PA66 910/1.1 CF15 GF20 PA66-(CF+GF)35 ALBIS Plastic GmbH
ALCOM® PA66 910/1.1 CF15 TF15 Si2 (PA66+PTFE)-CF... ALBIS Plastic GmbH
ALCOM® PA66 910/1.1 CF20 PA66-CF ALBIS Plastic GmbH
ALCOM® PA66 910/1.1 CF30 PTFE15 (PA66+PTFE)-CF ALBIS Plastic GmbH
ALCOM® PA66 910/1.1 CF40 PA66-CF ALBIS Plastic GmbH
ALCOM® PA66 910/1.2 CF30 PA66-CF ALBIS Plastic GmbH
ALCOM® PA66 910/1.3 CF/GF30 PA66-(CF+GF) ALBIS Plastic GmbH
ALCOM® PA66 910/1.3 CF5 GF25 PA66-(CF+GF)30 ALBIS Plastic GmbH
ALCOM® PA66 910/1.9 GF30 MO2 PA66-GF... ALBIS Plastic GmbH
ALCOM® PA66 910/30.1 GF15 TCE5 PA66... ALBIS Plastic GmbH
ALCOM® PA66 910/30.1 TCE10 PA66... ALBIS Plastic GmbH
ALCOM® PA66 910/30.1 TCE2 PA66... ALBIS Plastic GmbH
ALCOM® PA66 910/30.2 TCD2 PA66... ALBIS Plastic GmbH
ALCOM® PA66 910/30.3 TCD1 PA66... ALBIS Plastic GmbH
ALCOM® PA66 910/32.1 TCE5 PA66-X ALBIS Plastic GmbH
ALCOM® PA66 910/7 GF25 MR15 PA66-(GF+MX)40 ALBIS Plastic GmbH
ALCOM® PA66 910/7GF25MR15-22-956 PA66-(GF+MX)40 ALBIS Plastic GmbH
ALCOM® PA66 910/8 GF30 PTFE15 (PA66+PTFE)-GF30 ALBIS Plastic GmbH
ALCOM® PA66 910/8 MR40 PTFE15 (PA66+PTFE)-MX ALBIS Plastic GmbH
ALCOM® PBT 700/1 GF20 PTFE15 (PBT+PTFE)-GF20 ALBIS Plastic GmbH
ALCOM® PBT 700/1 GF30 PTFE15 (PBT+PTFE)-GF30 ALBIS Plastic GmbH
ALCOM® PBT 700/1 GF30 PTFE15 Si2 (PBT+PTFE)-GF... ALBIS Plastic GmbH
ALCOM® PBT 700/1 PTFE20 (PBT+PTFE) ALBIS Plastic GmbH
ALCOM® PBT 700/1.1 CF20 PTFE15 (PBT+PTFE)-CF ALBIS Plastic GmbH
ALCOM® PBT 700/1.5 GF15 PTFE15 (PBT+PTFE)-GF15 ALBIS Plastic GmbH
ALCOM® PBT 700/1.5 GF15 PTFE15 HR (PBT+PTFE)-GF15 ALBIS Plastic GmbH
ALCOM® PBT 700/2 WT 31-956 LB PBT ALBIS Plastic GmbH
ALCOM® PBT 700/30.1 TCE10 PBT... ALBIS Plastic GmbH
ALCOM® PBT 700/30.2 TCD2 PBT... ALBIS Plastic GmbH
ALCOM® PBT 700/8 GF15 PTFE15 (PBT+PTFE)-GF15 ALBIS Plastic GmbH
ALCOM® PC 740/1 GF30 PTFE15 (PC+PTFE)-GF30 ALBIS Plastic GmbH
ALCOM® PC 740/1 PTFE10 (PC+PTFE) ALBIS Plastic GmbH
ALCOM® PC 740/1 PTFE15 (PC+PTFE) ALBIS Plastic GmbH
ALCOM® PC 740/1 PTFE20 (PC+PTFE) ALBIS Plastic GmbH
ALCOM® PC 740/1,2 GF30 PTFE13 Si2 (PC+PTFE)-GF... ALBIS Plastic GmbH
ALCOM® PC 740/1.1 CF10 PC-CF ALBIS Plastic GmbH
ALCOM® PC 740/1.1 CF10 GF20 PC-(CF+GF)30 ALBIS Plastic GmbH
ALCOM® PC 740/1.1 CF10 PTFE15 (PC+PTFE)-CF ALBIS Plastic GmbH
ALCOM® PC 740/1.1 CF20 PC-CF ALBIS Plastic GmbH
ALCOM® PC 740/1.1 CF30 PC-CF ALBIS Plastic GmbH
ALCOM® PC 740/171 GY1127-04LD PC ALBIS Plastic GmbH
ALCOM® PC 740/171 GY1127-05LD PC ALBIS Plastic GmbH
ALCOM® PC 740/25 UV WT1445-06LD PC-X ALBIS Plastic GmbH
ALCOM® PC 740/25 WT1302-05LB PC ALBIS Plastic GmbH
ALCOM® PC 740/2813P.1 CF PC-CF ALBIS Plastic GmbH
ALCOM® PC 740/30 UV FR BN1375-07LD PC FR ALBIS Plastic GmbH
ALCOM® PC 740/30 UV FR WT1030-08LD PC FR ALBIS Plastic GmbH
ALCOM® PC 740/34 UV FR WT1147-09LD2 PC FR ALBIS Plastic GmbH
ALCOM® PC 740/4 BL1355-06LD PC ALBIS Plastic GmbH
ALCOM® PC 740/4 BL1411-07LD PC ALBIS Plastic GmbH
ALCOM® PC 740/4 BL1435-07LD PC ALBIS Plastic GmbH
ALCOM® PC 740/4 CC1084-07LD PC ALBIS Plastic GmbH
ALCOM® PC 740/4 CC1119-05LD PC ALBIS Plastic GmbH
ALCOM® PC 740/4 CC1120-05LD PC ALBIS Plastic GmbH
ALCOM® PC 740/4 CC1121-05LD PC ALBIS Plastic GmbH
ALCOM® PC 740/4 CC1122-05LD PC ALBIS Plastic GmbH
ALCOM® PC 740/4 GN1354-06LD PC ALBIS Plastic GmbH
ALCOM® PC 740/4 GY1122-04LD PC ALBIS Plastic GmbH
ALCOM® PC 740/4 GY1146-03LD PC ALBIS Plastic GmbH
ALCOM® PC 740/4 GY1152-05LD PC ALBIS Plastic GmbH
ALCOM® PC 740/4 GY1156-04LD PC ALBIS Plastic GmbH
ALCOM® PC 740/4 GY1177-05LD PC ALBIS Plastic GmbH
ALCOM® PC 740/4 GY1262-05LD PC ALBIS Plastic GmbH
ALCOM® PC 740/4 GY1281-04LD PC ALBIS Plastic GmbH
ALCOM® PC 740/4 GY1320-04LD PC ALBIS Plastic GmbH
ALCOM® PC 740/4 GY1354-08LB PC ALBIS Plastic GmbH
ALCOM® PC 740/4 GY1503-04LD PC ALBIS Plastic GmbH
ALCOM® PC 740/4 LD PC ALBIS Plastic GmbH
ALCOM® PC 740/4 RD1123-05LD PC ALBIS Plastic GmbH
ALCOM® PC 740/4 RD1223-05LD PC ALBIS Plastic GmbH
ALCOM® PC 740/4 RD1451-06LD PC ALBIS Plastic GmbH
ALCOM® PC 740/4 UV CC1060-09LD PC ALBIS Plastic GmbH
ALCOM® PC 740/4 UV CC1320-08LG PC ALBIS Plastic GmbH
ALCOM® PC 740/4 UV CC1321-08LG PC ALBIS Plastic GmbH
ALCOM® PC 740/4 UV CC1322-08LG PC ALBIS Plastic GmbH
ALCOM® PC 740/4 UV CC1323-08LG PC ALBIS Plastic GmbH
ALCOM® PC 740/4 UV GY1156-04LD PC ALBIS Plastic GmbH
ALCOM® PC 740/4 UV GY1408-07LD PC ALBIS Plastic GmbH
ALCOM® PC 740/4 UV GY1416-04LD PC ALBIS Plastic GmbH
ALCOM® PC 740/4 UV LD PC ALBIS Plastic GmbH
ALCOM® PC 740/4 UV OR1075-05LD PC ALBIS Plastic GmbH
ALCOM® PC 740/4 UV RD1231-08LD PC ALBIS Plastic GmbH
ALCOM® PC 740/4 UV RD1472-05LD PC ALBIS Plastic GmbH
ALCOM® PC 740/4 UV WT1000-05LD PC ALBIS Plastic GmbH
ALCOM® PC 740/4 UV WT1048-08LD2 PC ALBIS Plastic GmbH
ALCOM® PC 740/4 UV WT1080-08LD2 PC ALBIS Plastic GmbH
ALCOM® PC 740/4 UV WT1081-08LD2 PC ALBIS Plastic GmbH
ALCOM® PC 740/4 UV WT1082-08LD2 PC ALBIS Plastic GmbH
ALCOM® PC 740/4 UV WT1083-08LD2 PC ALBIS Plastic GmbH
ALCOM® PC 740/4 UV WT1102-04LD PC ALBIS Plastic GmbH
ALCOM® PC 740/4 UV WT1119-04LD PC ALBIS Plastic GmbH
ALCOM® PC 740/4 UV WT1220-05LD PC ALBIS Plastic GmbH
ALCOM® PC 740/4 UV WT1257-04LD PC ALBIS Plastic GmbH
ALCOM® PC 740/4 UV WT1280-04LD PC ALBIS Plastic GmbH
ALCOM® PC 740/4 UV WT1296-07LD PC ALBIS Plastic GmbH
ALCOM® PC 740/4 UV WT1368-04LD PC ALBIS Plastic GmbH
ALCOM® PC 740/4 UV WT1370-07LD PC ALBIS Plastic GmbH
ALCOM® PC 740/4 UV WT1401-06LD PC ALBIS Plastic GmbH
ALCOM® PC 740/4 UV WT1414-04LD PC ALBIS Plastic GmbH
ALCOM® PC 740/4 UV WT1445-06LD PC ALBIS Plastic GmbH
ALCOM® PC 740/4 UV WT1516-04LD PC ALBIS Plastic GmbH
ALCOM® PC 740/4 WT1114-09LD PC ALBIS Plastic GmbH
ALCOM® PC 740/4 WT1140-03LD PC ALBIS Plastic GmbH
ALCOM® PC 740/4 WT1170-10LD3 WHITE PC ALBIS Plastic GmbH
ALCOM® PC 740/4 WT1171-10LD3 WHITE PC ALBIS Plastic GmbH
ALCOM® PC 740/4 WT1172-10LD3 WHITE PC ALBIS Plastic GmbH
ALCOM® PC 740/4 WT1245-04LD PC ALBIS Plastic GmbH
ALCOM® PC 740/4 YL1395-06LD PC ALBIS Plastic GmbH
ALCOM® PC 740/4.1 WT1056-09LD2 PC ALBIS Plastic GmbH
ALCOM® PC 740/4.2 UV WT1090/08LD2 PC ALBIS Plastic GmbH
ALCOM® PC 740/4.2 UV WT1100-08LD2 PC ALBIS Plastic GmbH
ALCOM® PC 740/42 GY1218-10LD GREY PC-X ALBIS Plastic GmbH
ALCOM® PC 740/6 UV WT1121-04LD PC ALBIS Plastic GmbH
ALCOM® PC 740/9 PTFE10 bl 41-511 (PC+PTFE) ALBIS Plastic GmbH
ALCOM® PC+ABS 750/1 PTFE5 (PC+ABS+PTFE) ALBIS Plastic GmbH
ALCOM® PC+ABS 750/8 PTFE5 UV (PC+ABS+PTFE) ALBIS Plastic GmbH
ALCOM® PC+ABS 750/8 PTFE8 (PC+ABS+PTFE) ALBIS Plastic GmbH
ALCOM® PC+AWL 750/15.1WT1378-04LB (PC+ABS) ALBIS Plastic GmbH
ALCOM® PC+AWL 750/20.1WT1407-04LB (PC+ABS)... ALBIS Plastic GmbH
ALCOM® PC+AWL 750/25 WT1110-04LB (PC+ABS)... ALBIS Plastic GmbH
ALCOM® PE 59/0703 EC (PE-LD+(EVAC))-CD ALBIS Plastic GmbH
ALCOM® POM 770/1 AR10 PTFE10 (POM+PTFE)-RF ALBIS Plastic GmbH
ALCOM® POM 770/1 MO2 POM... ALBIS Plastic GmbH
ALCOM® POM 770/1 PTFE1.5 (POM+PTFE) ALBIS Plastic GmbH
ALCOM® POM 770/1 PTFE10 (POM+PTFE) ALBIS Plastic GmbH
ALCOM® POM 770/1 PTFE15 (POM+PTFE) ALBIS Plastic GmbH
ALCOM® POM 770/1 PTFE18 Si2 (POM+PTFE) ALBIS Plastic GmbH
ALCOM® POM 770/1 PTFE20 (POM+PTFE) ALBIS Plastic GmbH
ALCOM® POM 770/1 Si2 POM... ALBIS Plastic GmbH
ALCOM® POM 770/1 WT1153-07LB POM ALBIS Plastic GmbH
ALCOM® POM 770/1.1 CF10 POM-CF ALBIS Plastic GmbH
ALCOM® POM 770/1.1 CF20 POM-CF ALBIS Plastic GmbH
ALCOM® POM 770/2732 AR15 POM-RF ALBIS Plastic GmbH
ALCOM® PP 620/1 WT 1034-05 LB PP-MX... ALBIS Plastic GmbH
ALCOM® PP 620/1 WT 1301-04 LB PP-MX... ALBIS Plastic GmbH
ALCOM® PP 620/1 WT1433-05LB PP-MX... ALBIS Plastic GmbH
ALCOM® PP 620/10 GY 1464-04 MCF PP ALBIS Plastic GmbH
ALCOM® PP 620/2 SV1246-04MCO Silver PP ALBIS Plastic GmbH
ALCOM® PP 620/30 TCD1 PP... ALBIS Plastic GmbH
ALCOM® PP 620/4010 PTFE15 (PP+PTFE) ALBIS Plastic GmbH
ALCOM® PP 620/6 HGB PP-GB ALBIS Plastic GmbH
ALCOM® PP 620/8 GF30 PTFE15 (PP+PTFE)-GF30 ALBIS Plastic GmbH
ALCOM® PP 69/0702 EC PP-CD ALBIS Plastic GmbH
ALCOM® PP 69/0703 EC PP-CD ALBIS Plastic GmbH
ALCOM® PP620/10 SV1435-05MCF PP ALBIS Plastic GmbH
ALCOM® PPA 930/1 GF30 PTFE15 (PA*+PTFE)-GF30 ALBIS Plastic GmbH
ALCOM® PS 59/0702 EC PS-CD ALBIS Plastic GmbH
ALCOM® PS 59/0707 EC PS-CD ALBIS Plastic GmbH
ALCOM® PWL 10/1 WT41-913LB PC ALBIS Plastic GmbH
ALCOM® PWL 10/1.1 WT1302-05LB WHITE PC-X10 ALBIS Plastic GmbH
ALCOM® TPU 810/1998.1 CF TPU-CF ALBIS Plastic GmbH
ALCOM® TPU 810/3070.1 CF15 TPU-CF ALBIS Plastic GmbH
ALCOM® TPU 810/4073 AR10 TPU ALBIS Plastic GmbH
ALFATER XL® A35I 2GP0050 TPV ALBIS Plastic GmbH
ALFATER XL® A40I 1GP0001 TPV ALBIS Plastic GmbH
ALFATER XL® A40I 2GP0050 TPV ALBIS Plastic GmbH
ALFATER XL® A40I 3EF0001 TPV ALBIS Plastic GmbH
ALFATER XL® A45E 1GP0000 TPV ALBIS Plastic GmbH
ALFATER XL® A45E 2GP0000 TPV ALBIS Plastic GmbH
ALFATER XL® A45I 1GP0000 TPV ALBIS Plastic GmbH
ALFATER XL® A45I 2GP0000 TPV ALBIS Plastic GmbH
ALFATER XL® A50E 1GP0000 TPV ALBIS Plastic GmbH
ALFATER XL® A50E 2GP0000 TPV ALBIS Plastic GmbH
ALFATER XL® A50E 2UV0000 TPV ALBIS Plastic GmbH
ALFATER XL® A50I 1GP0000 TPV ALBIS Plastic GmbH
ALFATER XL® A50I 2GP0000 TPV ALBIS Plastic GmbH
ALFATER XL® A50I 2GP0050 TPV ALBIS Plastic GmbH
ALFATER XL® A50I 3EF0001 TPV ALBIS Plastic GmbH
ALFATER XL® A55E 1GP0000 TPV ALBIS Plastic GmbH
ALFATER XL® A55E 2GP0000 TPV ALBIS Plastic GmbH
ALFATER XL® A55I 1GP0000 TPV ALBIS Plastic GmbH
ALFATER XL® A55I 2GP0000 TPV ALBIS Plastic GmbH
ALFATER XL® A60E 1GP0000 TPV ALBIS Plastic GmbH
ALFATER XL® A60E 2GP0000 TPV ALBIS Plastic GmbH
ALFATER XL® A60I 1GP0000 TPV ALBIS Plastic GmbH
ALFATER XL® A60I 2GP0000 TPV ALBIS Plastic GmbH
ALFATER XL® A60I 2GP0050 TPV ALBIS Plastic GmbH
ALFATER XL® A60I 2UV0000 TPV ALBIS Plastic GmbH
ALFATER XL® A60I 3EF0001 TPV ALBIS Plastic GmbH
ALFATER XL® A65E 1GP0000 TPV ALBIS Plastic GmbH
ALFATER XL® A65E 2GP0000 TPV ALBIS Plastic GmbH
ALFATER XL® A65E 2UV0000 TPV ALBIS Plastic GmbH
ALFATER XL® A65I 1GP0000 TPV ALBIS Plastic GmbH
ALFATER XL® A65I 2GP0000 TPV ALBIS Plastic GmbH
ALFATER XL® A65I 2UV0000 TPV ALBIS Plastic GmbH
ALFATER XL® A70E 1GP0000 TPV ALBIS Plastic GmbH
ALFATER XL® A70E 2GP0000 TPV ALBIS Plastic GmbH
ALFATER XL® A70I 1GP0000 TPV ALBIS Plastic GmbH
ALFATER XL® A70I 2GP0000 TPV ALBIS Plastic GmbH
ALFATER XL® A70I 2GP0050 TPV ALBIS Plastic GmbH
ALFATER XL® A70I 3EF0001 TPV ALBIS Plastic GmbH
ALFATER XL® A75E 1GP0000 TPV ALBIS Plastic GmbH
ALFATER XL® A75E 2GP0000 TPV ALBIS Plastic GmbH
ALFATER XL® A75I 1GP0000 TPV ALBIS Plastic GmbH
ALFATER XL® A75I 1UV0000 TPV ALBIS Plastic GmbH
ALFATER XL® A75I 2GP0000 TPV ALBIS Plastic GmbH
ALFATER XL® A80E 1GP0000 TPV ALBIS Plastic GmbH
ALFATER XL® A80E 2GP0000 TPV ALBIS Plastic GmbH
ALFATER XL® A80E 2UV0000 TPV ALBIS Plastic GmbH
ALFATER XL® A80I 1GP0000 TPV ALBIS Plastic GmbH
ALFATER XL® A80I 2GP0000 TPV ALBIS Plastic GmbH
ALFATER XL® A80I 2GP0050 TPV ALBIS Plastic GmbH
ALFATER XL® A80I 2OR0000 TPV ALBIS Plastic GmbH
ALFATER XL® A80I 3EF0001 TPV ALBIS Plastic GmbH
ALFATER XL® A85E 1GP0000 TPV ALBIS Plastic GmbH
ALFATER XL® A85E 2GP0000 TPV ALBIS Plastic GmbH
ALFATER XL® A85I 1GP0000 TPV ALBIS Plastic GmbH
ALFATER XL® A85I 2GP0000 TPV ALBIS Plastic GmbH
ALFATER XL® A90E 1GP0000 TPV ALBIS Plastic GmbH
ALFATER XL® A90E 1MD0000 TPV ALBIS Plastic GmbH
ALFATER XL® A90E 2GP0000 TPV ALBIS Plastic GmbH
ALFATER XL® A90I 1GP0002 TPV ALBIS Plastic GmbH
ALFATER XL® A90I 1GP0004 TPV ALBIS Plastic GmbH
ALFATER XL® A90I 1MR0000 TPV ALBIS Plastic GmbH
ALFATER XL® A90I 1UV0000 TPV ALBIS Plastic GmbH
ALFATER XL® A90I 2GP0000 TPV ALBIS Plastic GmbH
ALFATER XL® A90I 2GP0050 TPV ALBIS Plastic GmbH
ALFATER XL® A90I 2OR0000 TPV ALBIS Plastic GmbH
ALFATER XL® A90I 3EF0001 TPV ALBIS Plastic GmbH
ALFATER XL® D35I 2UV0000 TPV ALBIS Plastic GmbH
ALFATER XL® D40E 1GP0000 TPV ALBIS Plastic GmbH
ALFATER XL® D40E 2GP0000 TPV ALBIS Plastic GmbH
ALFATER XL® D40I 1GP0000 TPV ALBIS Plastic GmbH
ALFATER XL® D40I 2GP0000 TPV ALBIS Plastic GmbH
ALFATER XL® D40I 2GP0050 TPV ALBIS Plastic GmbH
ALFATER XL® D40I 2UV0000 TPV ALBIS Plastic GmbH
ALFATER XL® D40I 3EF0001 TPV ALBIS Plastic GmbH
ALFATER XL® D45E 1GP0000 TPV ALBIS Plastic GmbH
ALFATER XL® D50E 1GP0001 TPV ALBIS Plastic GmbH
ALFATER XL® D50E 2GP0000 TPV ALBIS Plastic GmbH
ALFATER XL® D50I 1GP0000 TPV ALBIS Plastic GmbH
ALFATER XL® D50I 2GP0000 TPV ALBIS Plastic GmbH
ALFATER XL® D50I 2GP0050 TPV ALBIS Plastic GmbH
ALTECH 6 PA 1461 Z 2 PA6-GF30 ALBIS Plastic GmbH
ALTECH ABS A 1000/100 ABS ALBIS Plastic GmbH
ALTECH ABS A 1000/106 ABS ALBIS Plastic GmbH
ALTECH ABS A 1000/139 AS ABS ALBIS Plastic GmbH
ALTECH ABS A 1000/177 ABS ALBIS Plastic GmbH
ALTECH ABS A 1000/578 ABS ALBIS Plastic GmbH
ALTECH ABS A 1000/587 ABS ALBIS Plastic GmbH
ALTECH ABS A 2017/500 GF17 ABS-GF17 ALBIS Plastic GmbH
ALTECH ABS A 2020/100 GF20 ABS-GF20 ALBIS Plastic GmbH
ALTECH ABS A 3030/576 GB30 AS ABS-GB30 ALBIS Plastic GmbH
ALTECH ABS A 3230/516 GB20 GF10 ABS-(GB+GF)30 ALBIS Plastic GmbH
ALTECH PA6 A 1000/107 PA6 ALBIS Plastic GmbH
ALTECH PA6 A 1000/108 PA6 ALBIS Plastic GmbH
ALTECH PA6 A 1000/109 PA6 ALBIS Plastic GmbH
ALTECH PA6 A 1000/110 IM PA6-I ALBIS Plastic GmbH
ALTECH PA6 A 1000/120 UV PA6 ALBIS Plastic GmbH
ALTECH PA6 A 1000/126 UV PA6 ALBIS Plastic GmbH
ALTECH PA6 A 1000/149 FR PA6 FR ALBIS Plastic GmbH
ALTECH PA6 A 1000/310 IM PA6-I ALBIS Plastic GmbH
ALTECH PA6 A 1000/316 IM PA6-I ALBIS Plastic GmbH
ALTECH PA6 A 1000/506 HV PA6 ALBIS Plastic GmbH
ALTECH PA6 A 1000/510 IM PA6-I ALBIS Plastic GmbH
ALTECH PA6 A 1000/518 IM PA6-I ALBIS Plastic GmbH
ALTECH PA6 A 1000/520 UV HV PA6 ALBIS Plastic GmbH
ALTECH PA6 A 1000/586 PA6 ALBIS Plastic GmbH
ALTECH PA6 A 1000/700 PA6 ALBIS Plastic GmbH
ALTECH PA6 A 1000/716 IM PA6-I ALBIS Plastic GmbH
ALTECH PA6 A 2003/710 GF3 IM PA6-I-GF3 ALBIS Plastic GmbH
ALTECH PA6 A 2010/100 GF10 PA6-GF10 ALBIS Plastic GmbH
ALTECH PA6 A 2015/109 GF15 PA6-GF15 ALBIS Plastic GmbH
ALTECH PA6 A 2015/210 GF15 IM PA6-I-GF15 ALBIS Plastic GmbH
ALTECH PA6 A 2015/220 GF15 UV PA6-GF15 ALBIS Plastic GmbH
ALTECH PA6 A 2015/310 GF15 IM PA6-I-GF15 ALBIS Plastic GmbH
ALTECH PA6 A 2015/321 GF15 UV IM PA6-I-GF15 ALBIS Plastic GmbH
ALTECH PA6 A 2015/610 GF15 IM PA6-I-GF15 ALBIS Plastic GmbH
ALTECH PA6 A 2015/710 GF15 IM PA6-I-GF15 ALBIS Plastic GmbH
ALTECH PA6 A 2020/109 GF20 PA6-GF20 ALBIS Plastic GmbH
ALTECH PA6 A 2025/109 GF25 PA6-GF25 ALBIS Plastic GmbH
ALTECH PA6 A 2030/109 GF30 PA6-GF30 ALBIS Plastic GmbH
ALTECH PA6 A 2030/209 GF30 PA6-GF30 ALBIS Plastic GmbH
ALTECH PA6 A 2030/212 GF30 IM UV PA6-I-GF30 ALBIS Plastic GmbH
ALTECH PA6 A 2030/319 GF30 IM PA6-I-GF30 ALBIS Plastic GmbH
ALTECH PA6 A 2030/320 GF30 UV PA6-GF30 ALBIS Plastic GmbH
ALTECH PA6 A 2030/577 GF30 PA6-GF30 ALBIS Plastic GmbH
ALTECH PA6 A 2030/586 GF30 PA6-GF30 ALBIS Plastic GmbH
ALTECH PA6 A 2030/587 GF30 PA6-GF30 ALBIS Plastic GmbH
ALTECH PA6 A 2030/610 GF30 IM PA6-I-GF30 ALBIS Plastic GmbH
ALTECH PA6 A 2035/109 GF35 PA6-GF35 ALBIS Plastic GmbH
ALTECH PA6 A 4030/109 MR30 PA6-MX30 ALBIS Plastic GmbH
ALTECH PA6 A 4030/210 MR30 PA6-MX30 ALBIS Plastic GmbH
ALTECH PA6 A 4040/100 MR40 PA6-MX40 ALBIS Plastic GmbH
ALTECH PA6 B 1000/109 PA6 ALBIS Plastic GmbH
ALTECH PA6 B 1000/209 PA6 ALBIS Plastic GmbH
ALTECH PA6 B 1000/509 PA6 ALBIS Plastic GmbH
ALTECH PA6 B 2015/100 GF15 PA6-GF15 ALBIS Plastic GmbH
ALTECH PA6 B 2015/106 GF15 PA6-GF15 ALBIS Plastic GmbH
ALTECH PA6 B 2025/309 GF25 PA6-GF25 ALBIS Plastic GmbH
ALTECH PA6 B 2030/209 GF30 PA6-GF30 ALBIS Plastic GmbH
ALTECH PA6 C 2030/100 GF30 PA6-GF30 ALBIS Plastic GmbH
ALTECH PA6 C 2030/119 GF30 IM PA6-I-GF30 ALBIS Plastic GmbH
ALTECH PA6 C 2030/219 GF30 IM PA6-I-GF30 ALBIS Plastic GmbH
ALTECH PA6 C 3030/100 GB30 PA6-GB30 ALBIS Plastic GmbH
ALTECH PA6 C 3030/320 GB30 UV PA6-GB30 ALBIS Plastic GmbH
ALTECH PA6 C 3230/100 GB20 GF10 PA6-(GB+GF)30 ALBIS Plastic GmbH
ALTECH PA6 C 4230/100 GF10 MR20 PA6-(GF+MX)30 ALBIS Plastic GmbH
ALTECH PA6+ASA A 1000/220 UV (PA6+ASA) ALBIS Plastic GmbH
ALTECH PA6+ASA A 1000/312 UV IM (PA6+ASA)-I ALBIS Plastic GmbH
ALTECH PA6+ASA A 4010/220 MR10 (PA6+ASA)-MX10 ALBIS Plastic GmbH
ALTECH PA6+ASA A4010221MR10UV IM (PA6+ASA)-I-MX10 ALBIS Plastic GmbH
ALTECH PA6+PA666 A2030/100GF30IM (PA6+PA666)-I-GF30 ALBIS Plastic GmbH
ALTECH PA6/6T A 2050/510 GF50 IM PA6/6T-I ALBIS Plastic GmbH
ALTECH PA66 A 1000/109 PA66 ALBIS Plastic GmbH
ALTECH PA66 A 1000/276 PA66 ALBIS Plastic GmbH
ALTECH PA66 A 1000/310 IM PA66-I ALBIS Plastic GmbH
ALTECH PA66 A 1000/510 IM PA66-I ALBIS Plastic GmbH
ALTECH PA66 A 1000/512 IM PA66-I ALBIS Plastic GmbH
ALTECH PA66 A 2015/109 GF15 PA66-GF15 ALBIS Plastic GmbH
ALTECH PA66 A 2015/310 GF15 IM PA66-I-GF15 ALBIS Plastic GmbH
ALTECH PA66 A 2015/510 GF15 IM PA66-I-GF15 ALBIS Plastic GmbH
ALTECH PA66 A 2015/710 GF15 IM PA66-I-GF15 ALBIS Plastic GmbH
ALTECH PA66 A 2020/100 GF20 PA66-GF20 ALBIS Plastic GmbH
ALTECH PA66 A 2020/109 GF20 PA66-GF20 ALBIS Plastic GmbH
ALTECH PA66 A 2025/109 GF25 PA66-GF25 ALBIS Plastic GmbH
ALTECH PA66 A 2025/567 GF25 PA66-GF25 ALBIS Plastic GmbH
ALTECH PA66 A 2025/568 GF25 PA66-GF25 ALBIS Plastic GmbH
ALTECH PA66 A 2025/576 GF25 PA66-GF25 ALBIS Plastic GmbH
ALTECH PA66 A 2030/100 GF30 PA66-GF30 ALBIS Plastic GmbH
ALTECH PA66 A 2030/106 GF30 PA66-GF30 ALBIS Plastic GmbH
ALTECH PA66 A 2030/109 GF30 PA66-GF30 ALBIS Plastic GmbH
ALTECH PA66 A 2030/310 GF30 IM PA66-I-GF30 ALBIS Plastic GmbH
ALTECH PA66 A 2030/500 GF30 PA66-GF30 ALBIS Plastic GmbH
ALTECH PA66 A 2030/507 GF30 PA66-GF30 ALBIS Plastic GmbH
ALTECH PA66 A 2030/516 GF30 IM PA66-I-GF30 ALBIS Plastic GmbH
ALTECH PA66 A 2030/588 GF30 PA66-GF30 ALBIS Plastic GmbH
ALTECH PA66 A 2035/109 GF35 PA66-GF35 ALBIS Plastic GmbH
ALTECH PA66 A 2035/310 PA66-I-GF35 ALBIS Plastic GmbH
ALTECH PA66 A 2035/506 GF35 PA66-I-GF35 ALBIS Plastic GmbH
ALTECH PA66 A 2035/507 GF35 EF PA66-I-GF35 ALBIS Plastic GmbH
ALTECH PA66 A 2040/100 GF40 PA66-GF40 ALBIS Plastic GmbH
ALTECH PA66 A 2040/310 GF40 IM PA66-I-GF40 ALBIS Plastic GmbH
ALTECH PA66 A 2045/220 GF45 UV PA66-GF45 ALBIS Plastic GmbH
ALTECH PA66 A 2050/100 GF50 PA66-GF50 ALBIS Plastic GmbH
ALTECH PA66 A 2050/106 GF50 PA66-GF50 ALBIS Plastic GmbH
ALTECH PA66 A 2050/576 GF50 PA66-GF50 ALBIS Plastic GmbH
ALTECH PA66 A 3015/100 GB15 PA66-GB15 ALBIS Plastic GmbH
ALTECH PA66 A 3020/100 GB20 PA66-GB20 ALBIS Plastic GmbH
ALTECH PA66 A 3030/109 GB30 PA66-GB30 ALBIS Plastic GmbH
ALTECH PA66 A 3040/100 GB40 PA66-GB40 ALBIS Plastic GmbH
ALTECH PA66 A 4030/100 MR30 PA66-MX30 ALBIS Plastic GmbH
ALTECH PA66 A 4040/100 MR40 PA66-MX40 ALBIS Plastic GmbH
ALTECH PA66 B 1000/109 PA66 ALBIS Plastic GmbH
ALTECH PA66 B 1000/209 PA66 ALBIS Plastic GmbH
ALTECH PA66 B 1000/500 PA66 ALBIS Plastic GmbH
ALTECH PA66 B 2015/506 GF15 PA66-GF15 ALBIS Plastic GmbH
ALTECH PA66 B 2025/106 GF25 PA66-GF25 ALBIS Plastic GmbH
ALTECH PA66 B 2030/109 GF30 PA66-GF30 ALBIS Plastic GmbH
ALTECH PA66 B 2030/209 GF30 PA66-GF30 ALBIS Plastic GmbH
ALTECH PA66 B 2030/507 GF30 PA66-GF30 ALBIS Plastic GmbH
ALTECH PA66 B 3020/100 GB20 PA66-GB20 ALBIS Plastic GmbH
ALTECH PA66 B 3050/100 GB50 PA66-GB50 ALBIS Plastic GmbH
ALTECH PA66+PA6 A 1000/567 (PA66+PA6) ALBIS Plastic GmbH
ALTECH PA66+PP A 2030/577 GF30 (PA66+PP)-GF30 ALBIS Plastic GmbH
ALTECH PA66+PP A 2030/578 (PA66+PP)-GF30 ALBIS Plastic GmbH
ALTECH PA66/6 A 4030/510 MR30 IM (PA666+ASA)-I-MX30 ALBIS Plastic GmbH
ALTECH PBT A 1000/506 PBT ALBIS Plastic GmbH
ALTECH PBT A 1000/507 PBT ALBIS Plastic GmbH
ALTECH PBT A 2020/340 GF20 FR PBT-GF20 FR ALBIS Plastic GmbH
ALTECH PBT A 2020/510 GF20 IM PBT-I-GF20 ALBIS Plastic GmbH
ALTECH PBT A 2030/340 GF30 FR PBT-GF30 FR ALBIS Plastic GmbH
ALTECH PBT A 3030/100 GB30 PBT-GB30 ALBIS Plastic GmbH
ALTECH PBT+ASA A 2020/510 GF20 (PBT+ASA)-GF20 ALBIS Plastic GmbH
ALTECH PBT+ASA A 2030/500 GF30 (PBT+ASA)-GF30 ALBIS Plastic GmbH
ALTECH PC A 1000/170 PC ALBIS Plastic GmbH
ALTECH PC A 1000/226 UV PC ALBIS Plastic GmbH
ALTECH PC A 1000/227 PC ALBIS Plastic GmbH
ALTECH PC A 1000/326 UV PC ALBIS Plastic GmbH
ALTECH PC A 1000/346 PC ALBIS Plastic GmbH
ALTECH PC A 1000/526 UV BK1307-06 PC ALBIS Plastic GmbH
ALTECH PC A 1000/578 UV PC ALBIS Plastic GmbH
ALTECH PC A 1000/619 PC ALBIS Plastic GmbH
ALTECH PC A 1000/620 UV PC ALBIS Plastic GmbH
ALTECH PC B 1000/520 UV PC ALBIS Plastic GmbH
ALTECH PC B 1000/576 PC ALBIS Plastic GmbH
ALTECH PC B 1000/588 UV AS PC ALBIS Plastic GmbH
ALTECH PC B 1000/620 UV PC ALBIS Plastic GmbH
ALTECH PC B 2010/100 GF10 PC-GF10 ALBIS Plastic GmbH
ALTECH PC C 1000/100 PC ALBIS Plastic GmbH
ALTECH PC+ABS A 1000/107 (PC+ABS) ALBIS Plastic GmbH
ALTECH PC+ABS A 1000/520 UV (PC+ABS) ALBIS Plastic GmbH
ALTECH PC+ABS A 1000/540 (PC+ABS) ALBIS Plastic GmbH
ALTECH PC+ABS A 1000/620 UV (PC+ABS) ALBIS Plastic GmbH
ALTECH PC+ASA A 1000/320 (PC+ASA) ALBIS Plastic GmbH
ALTECH PC+ASA A 1000/527 UV (PC+ASA) ALBIS Plastic GmbH
ALTECH PC+ASA A 4010/520 UV (PC+ASA)-MX10 ALBIS Plastic GmbH
ALTECH PC-HT A 1000/500 PC ALBIS Plastic GmbH
ALTECH PE-HD A 2020/506 GF20 (PE-HD)-GF20 ALBIS Plastic GmbH
ALTECH POM A 1000/106 POM ALBIS Plastic GmbH
ALTECH POM A 1000/120 UV POM ALBIS Plastic GmbH
ALTECH POM A 1000/320 UV POM ALBIS Plastic GmbH
ALTECH POM A 1000/620 UV POM ALBIS Plastic GmbH
ALTECH POM A 2010/500 GF10 POM-GF10 ALBIS Plastic GmbH
ALTECH POM A 2010/720 GF10 UV POM-GF10 ALBIS Plastic GmbH
ALTECH POM A 2020/100 POM-GF20 ALBIS Plastic GmbH
ALTECH PP-B A 1000/120 UV PP ALBIS Plastic GmbH
ALTECH PP-B A 1000/310 IM PP-I ALBIS Plastic GmbH
ALTECH PP-B A 1000/540 FR PP FR ALBIS Plastic GmbH
ALTECH PP-B A 1000/546 FR PP FR ALBIS Plastic GmbH
ALTECH PP-B A 1000/587 IM PP-I ALBIS Plastic GmbH
ALTECH PP-B A 2015/550 GF15 CP PP-GF15 ALBIS Plastic GmbH
ALTECH PP-B A 2020/150 GF20 CP PP-GF20 ALBIS Plastic GmbH
ALTECH PP-B A 2030/150 GF30 CP PP-GF30 ALBIS Plastic GmbH
ALTECH PP-B A 2040/150 GF40 CP PP-GF40 ALBIS Plastic GmbH
ALTECH PP-B A 3030/500 GB30 PP-GB30 ALBIS Plastic GmbH
ALTECH PP-B A 4430/100 MR30 PP-(Z+T)30 ALBIS Plastic GmbH
ALTECH PP-B A 4430/120 MR30 UV PP-(Z+T)30 ALBIS Plastic GmbH
ALTECH PP-B A 4815/100 MR15 PP-MX15 ALBIS Plastic GmbH
ALTECH PP-B A 4920/100 MR20 PP-T20 ALBIS Plastic GmbH
ALTECH PP-B A 4925/500 MR25 PP-T25 ALBIS Plastic GmbH
ALTECH PP-B A 4930/507 MR30 PP-T30 ALBIS Plastic GmbH
ALTECH PP-B A 4930/520 MR30 UV PP-T30 ALBIS Plastic GmbH
ALTECH PP-B A 4940/600 MR40 PP-T40 ALBIS Plastic GmbH
ALTECH PP-B C 2015/550 GF15 CP PP-GF15 ALBIS Plastic GmbH
ALTECH PP-B C 2030/550 GF30 CP PP-GF30 ALBIS Plastic GmbH
ALTECH PP-B C 2040/550 GF40 CP PP-GF40 ALBIS Plastic GmbH
ALTECH PP-B C 4920/570 MR20 PP-T20 ALBIS Plastic GmbH
ALTECH PP-B FC 2030/150 GF30 CP PP-GF30 ALBIS Plastic GmbH
ALTECH PP-H A 1000/100 DS PP ALBIS Plastic GmbH
ALTECH PP-H A 1000/149 FR PP FR ALBIS Plastic GmbH
ALTECH PP-H A 1000/249 FR PP FR ALBIS Plastic GmbH
ALTECH PP-H A 1000/576 PP ALBIS Plastic GmbH
ALTECH PP-H A 1000/620 UV PP ALBIS Plastic GmbH
ALTECH PP-H A 2020/100 GF20 PP-GF20 ALBIS Plastic GmbH
ALTECH PP-H A 2020/159 GF20 CP PP-GF20 ALBIS Plastic GmbH
ALTECH PP-H A 2020/750 GF20 CP PP-GF20 ALBIS Plastic GmbH
ALTECH PP-H A 2030/100 BK0002-00 PP-GF30 ALBIS Plastic GmbH
ALTECH PP-H A 2030/156 GF30 CP PP-GF30 ALBIS Plastic GmbH
ALTECH PP-H A 2030/157 GF30 CP PP-GF30 ALBIS Plastic GmbH
ALTECH PP-H A 2030/158 GF30 CP PP-GF30 ALBIS Plastic GmbH
ALTECH PP-H A 2030/159 GF30 CP PP-GF30 ALBIS Plastic GmbH
ALTECH PP-H A 2030/169 GF30 CP PP-GF30 ALBIS Plastic GmbH
ALTECH PP-H A 2030/250 GF30 CP PP-GF30 ALBIS Plastic GmbH
ALTECH PP-H A 2030/252 GF30 UV CP PP-GF30 ALBIS Plastic GmbH
ALTECH PP-H A 2030/652 GF30 UV PP-GF30 ALBIS Plastic GmbH
ALTECH PP-H A 2030/750 GF30 CP PP-GF30 ALBIS Plastic GmbH
ALTECH PP-H A 2035/500 GF35 PP-GF35 ALBIS Plastic GmbH
ALTECH PP-H A 2040/159 GF40 CP PP-GF40 ALBIS Plastic GmbH
ALTECH PP-H A 2040/652 GF 40 UV CP PP-GF40 ALBIS Plastic GmbH
ALTECH PP-H A 3020/100 GB20 PP-GB20 ALBIS Plastic GmbH
ALTECH PP-H A 3020/500 GB20 PP-GB20 ALBIS Plastic GmbH
ALTECH PP-H A 3030/100 GB30 PP-GB30 ALBIS Plastic GmbH
ALTECH PP-H A 3030/108 GB30 PP-GB30 ALBIS Plastic GmbH
ALTECH PP-H A 4818/100 MR18 DS PP-Z18 ALBIS Plastic GmbH
ALTECH PP-H A 4907/500 MR07 PP-T7 ALBIS Plastic GmbH
ALTECH PP-H A 4910/620 MR10 UV PP-T10 ALBIS Plastic GmbH
ALTECH PP-H A 4920/106 MR20 PP-T20 ALBIS Plastic GmbH
ALTECH PP-H A 4920/107 MR20 PP-T20 ALBIS Plastic GmbH
ALTECH PP-H A 4920/109 MR20 PP-T20 ALBIS Plastic GmbH
ALTECH PP-H A 4920/170 MR20 PP-T20 ALBIS Plastic GmbH
ALTECH PP-H A 4920/178 MR20 PP-T20 ALBIS Plastic GmbH
ALTECH PP-H A 4920/500 MR20 PP-T20 ALBIS Plastic GmbH
ALTECH PP-H A 4920/520 MR20 UV PP-T20 ALBIS Plastic GmbH
ALTECH PP-H A 4925/500 MR25 PP-MX25 ALBIS Plastic GmbH
ALTECH PP-H A 4930/100 MR30 PP-T30 ALBIS Plastic GmbH
ALTECH PP-H A 4930/106 MR30 PP-T30 ALBIS Plastic GmbH
ALTECH PP-H A 4930/506 MR30 PP-T30 ALBIS Plastic GmbH
ALTECH PP-H A 4940/100 MR40 PP-T40 ALBIS Plastic GmbH
ALTECH PP-H A 4940/106 MR40 PP-T40 ALBIS Plastic GmbH
ALTECH PP-H C 2030/550 GF30 CP PP-GF30 ALBIS Plastic GmbH
ALTECH PP-H C 2030/567 GF30 PP-GF30 ALBIS Plastic GmbH
ALTECH PP-H C 4920/570 MR20 PP-T20 ALBIS Plastic GmbH
ALTECH PP-H C 4940/570 MR40 PP-T40 ALBIS Plastic GmbH
ALTECH PP-H FC 4920/100 MR20 PP-T20 ALBIS Plastic GmbH
ALTECH PS-HI A 1000/240 FR PS ALBIS Plastic GmbH
ALTECH PSU A 1000/100 PSU ALBIS Plastic GmbH
Cellidor B 500-05 C ALBIS Plastic GmbH
Cellidor B 500-10 C ALBIS Plastic GmbH
Cellidor B 500-15 C ALBIS Plastic GmbH
Cellidor B 500-20 C ALBIS Plastic GmbH
Cellidor B 531-07 C ALBIS Plastic GmbH
Cellidor B 531-10 C ALBIS Plastic GmbH
Cellidor B 631-10 C ALBIS Plastic GmbH
Cellidor CP 2810-11 C ALBIS Plastic GmbH
Cellidor CP 300-10 C ALBIS Plastic GmbH
Cellidor CP 300-13 C ALBIS Plastic GmbH
Cellidor CP 300-15 C ALBIS Plastic GmbH
Cellidor CP 300-17 C ALBIS Plastic GmbH
Cellidor CP 300-20 C ALBIS Plastic GmbH
Cellidor CP 310-10 C ALBIS Plastic GmbH
Cellidor CP 3406-08 C ALBIS Plastic GmbH
Cellidor CP 3406-11 C ALBIS Plastic GmbH
Cellidor CP 400-08 C ALBIS Plastic GmbH
Cellidor CP 400-08 GF25 C-GF25 ALBIS Plastic GmbH
Cellidor CP 400-10 C ALBIS Plastic GmbH
Cellidor CP 400-12 C ALBIS Plastic GmbH
Cellidor CP 400-15 C ALBIS Plastic GmbH
Cellidor CP 400-17 C ALBIS Plastic GmbH
Cellidor CP 410-10 C ALBIS Plastic GmbH
Cellidor CP 430-13 AG C ALBIS Plastic GmbH
Procom 1111 H PP ALBIS Plastic GmbH
Procom 1111 L TA 8 PP-T40 ALBIS Plastic GmbH
PS 158 K KG2 UV Q 262 PS ALBIS Plastic GmbH
PS 495F PC PS ALBIS Plastic GmbH