View list of

CAMPUSplastics | All RadiciPlastics grades

The international CAMPUS® database offers datasheets of the following materials from producer: RadiciPlastics.

Please click on the grade of interest to generate a datasheet. You also may select a material by choosing an other producer or a specific polymer family. In addition you may select by any part of the grade name using the input box on the left.

Grade Name Family Producer
HERAFLEX® A 35-13-40 TPS RadiciPlastics
HERAFLEX® A 40-11-91 TPS RadiciPlastics
HERAFLEX® A 55 11 I HW TPS RadiciPlastics
HERAFLEX® A 55 11 I RKT TPS RadiciPlastics
HERAFLEX® A 55 42 I HW2E TPS RadiciPlastics
HERAFLEX® A 57-41-90 TPS RadiciPlastics
HERAFLEX® A 60 31 I HS1 TPS RadiciPlastics
HERAFLEX® A 65 31 I HW TPS RadiciPlastics
HERAFLEX® A 65-21-20 UV TPS RadiciPlastics
HERAFLEX® A 70-21-22 TPS RadiciPlastics
HERAFLEX® A 70-21-22 UV TPS RadiciPlastics
HERAFLEX® A 70-22-90 HG TPS RadiciPlastics
HERAFLEX® A 75-21-60 TPS RadiciPlastics
HERAFLEX® A 80-21-94 TPS RadiciPlastics
HERAFLEX® A 80-42-90 G TPS RadiciPlastics
HERAFLEX® A 90-11-44 UV TPS RadiciPlastics
HERAFLEX® A 90-21-90 TPS RadiciPlastics
HERAFLEX® B 35D 11 I SL 250 TPS RadiciPlastics
HERAFLEX® B 60 11 I HP TPS RadiciPlastics
HERAFLEX® B 80 31 I HP TPS RadiciPlastics
HERAFLEX® E 3918 TPC RadiciPlastics
HERAFLEX® E 4718 TPC RadiciPlastics
HERAFLEX® E 5620 TPC RadiciPlastics
HERAFLEX® E 6521 TPC RadiciPlastics
HERAFLEX® E 7722 TPC RadiciPlastics
HERAFLEX® HA 60-22-60 TPS RadiciPlastics
HERAFLEX® HP 40-21-60 TPS RadiciPlastics
HERAFLEX® P 40D 11 I HF 1530 TPO RadiciPlastics
HERAFLEX® P 40D 21 I HF TPO RadiciPlastics
HERAFLEX® P 46D 11 I RB T 200 TPO RadiciPlastics
HERAFLEX® P 51D 11 I RB T 270 TPO RadiciPlastics
HERAFLEX® P 55D 11 I HF 330 TPO RadiciPlastics
RADIFLAM® A AE PA66 FR RadiciPlastics
RADIFLAM® A FR PA66 FR RadiciPlastics
RADIFLAM® A RV250AF PA66-GF25 FR RadiciPlastics
RADIFLAM® A RV250FR PA66-GF25 FR RadiciPlastics
RADIFLAM® A RV300AE PA66-GF30 FR RadiciPlastics
RADIFLAM® A RV300AF PA66-GF30 FR RadiciPlastics
RADIFLAM® A RV350AF PA66-GF35 FR RadiciPlastics
RADIFLAM® B N100AE PBT FR RadiciPlastics
RADIFLAM® B RV250AE PBT-GF25 FR RadiciPlastics
RADIFLAM® S AE PA6 FR RadiciPlastics
RADIFLAM® S FR PA6 FR RadiciPlastics
RADIFLAM® S RV250FR PA6-GF25 FR RadiciPlastics
RADIFLAM® S RV300AE PA6-GF30 FR RadiciPlastics
RADILENE® R 30 IE 0 3036 B (PE-LD) RadiciPlastics
RADILENE® R 70 IE 0 2060 C (PE-HD) RadiciPlastics
RADILENE® R 70 IE 0 5058 B (PE-HD) RadiciPlastics
RADILENE® R 70 IF 0 4058 A (PE-HD) RadiciPlastics
RADILON® A 35E 990 PA66 RadiciPlastics
RADILON® A 38 PA66 RadiciPlastics
RADILON® A 42 PA66 RadiciPlastics
RADILON® A CF350 PA66-CF35 RadiciPlastics
RADILON® A CP300K PA66-MX30 RadiciPlastics
RADILON® A CP400 PA66-MX40 RadiciPlastics
RADILON® A CV300LK PA66-GB30 RadiciPlastics
RADILON® A ECP3808 PA66-I-MX30 RadiciPlastics
RADILON® A ERV1906LK PA66-I-GF13 RadiciPlastics
RADILON® A ERV3012 PA66-I-GF18 RadiciPlastics
RADILON® A ESL128 PA66-I RadiciPlastics
RADILON® A HS PA66 RadiciPlastics
RADILON® A HSK PA66 RadiciPlastics
RADILON® A HSX PA66-I RadiciPlastics
RADILON® A HSX88 PA66-I RadiciPlastics
RADILON® A LX14080 PA66 RadiciPlastics
RADILON® A RCF3505 PA66-(CF+GF)35 RadiciPlastics
RADILON® A RV150 PA66-GF15 RadiciPlastics
RADILON® A RV200 PA66-GF20 RadiciPlastics
RADILON® A RV250 PA66-GF25 RadiciPlastics
RADILON® A RV300 PA66-GF30 RadiciPlastics
RADILON® A RV300 990 PA66-GF30 RadiciPlastics
RADILON® A RV300R PA66-GF30 RadiciPlastics
RADILON® A RV300RKC PA66-GF30 RadiciPlastics
RADILON® A RV330 PA66-GF33 RadiciPlastics
RADILON® A RV350 PA66-GF35 RadiciPlastics
RADILON® A RV400 PA66-GF40 RadiciPlastics
RADILON® A RV500 PA66-GF50 RadiciPlastics
RADILON® A USX200 PA66-I RadiciPlastics
RADILON® A USZ200 PA66-I RadiciPlastics
RADILON® CA HS PA666 RadiciPlastics
RADILON® CA RV300L PA666-GF30 RadiciPlastics
RADILON® CS 35FL PA6 RadiciPlastics
RADILON® CS 38FL PA6 RadiciPlastics
RADILON® CS T PA6 RadiciPlastics
RADILON® CS T 38FL PA6 RadiciPlastics
RADILON® S 32HS PA6 RadiciPlastics
RADILON® S 35FL PA6 RadiciPlastics
RADILON® S 35HR PA6 RadiciPlastics
RADILON® S 38F PA6 RadiciPlastics
RADILON® S 38M PA6-I RadiciPlastics
RADILON® S 40 EP3215 PA6-I RadiciPlastics
RADILON® S 40E PA6 RadiciPlastics
RADILON® S 40FL PA6 RadiciPlastics
RADILON® S CP300 PA6-MX30 RadiciPlastics
RADILON® S CP400 PA6-MX40 RadiciPlastics
RADILON® S CV300 PA6-GB30 RadiciPlastics
RADILON® S ERV3808K PA6-I-MX30 RadiciPlastics
RADILON® S ESL128 PA6-I RadiciPlastics
RADILON® S HS PA6 RadiciPlastics
RADILON® S HSX PA6-I RadiciPlastics
RADILON® S HSX88 PA6-I RadiciPlastics
RADILON® S LHS PA6 RadiciPlastics
RADILON® S LVHPL128 PA6-I RadiciPlastics
RADILON® S RCP3010LK PA6-(GF+MX)30 RadiciPlastics
RADILON® S RCV3015 PA6-(GF+GB)30 RadiciPlastics
RADILON® S RCV3515 PA6-(GF+GB)35 RadiciPlastics
RADILON® S RV150 PA6-GF15 RadiciPlastics
RADILON® S RV200 PA6-GF20 RadiciPlastics
RADILON® S RV250 PA6-GF25 RadiciPlastics
RADILON® S RV300 PA6-GF30 RadiciPlastics
RADILON® S RV300LK PA6-GF30 RadiciPlastics
RADILON® S RV300R PA6-GF30 RadiciPlastics
RADILON® S RV330 PA6-GF33 RadiciPlastics
RADILON® S RV350 PA6-GF35 RadiciPlastics
RADILON® S RV500 PA6-GF50 RadiciPlastics
RADILON® S USX200 PA6-I RadiciPlastics
RADILON® S USZ200 PA6-I RadiciPlastics
RADITER® B N100 PBT RadiciPlastics
RADITER® B RV150 PBT-GF15 RadiciPlastics
RADITER® B RV200 PBT-GF20 RadiciPlastics
RADITER® B RV300 PBT-GF30 RadiciPlastics
RADITER® B RVA100 (PBT+ASA)-GF10 RadiciPlastics
RADITER® B RVA200 (PBT+ASA)-GF20 RadiciPlastics
RADITER® B RVA300 (PBT+ASA)-GF30 RadiciPlastics