Grade Name Family Producer
CELANEX 1400A PBT Ticona
CELANEX 1462Z PBT-GF30 Ticona
CELANEX 1600A PBT Ticona
CELANEX 1602Z PBT Ticona
CELANEX 1632Z PBT-GF15 Ticona
CELANEX 1642Z PBT-GF20 Ticona
CELANEX 1662Z PBT-GF30 Ticona
CELANEX 1700A PBT Ticona
CELANEX 2000-2 PBT Ticona
CELANEX 2000-3 PBT Ticona
CELANEX 2001 PBT Ticona
CELANEX 2002-2 PBT Ticona
CELANEX 2002-3 PBT Ticona
CELANEX 2002UV PBT Ticona
CELANEX 2003-2 PBT Ticona
CELANEX 2003-3 PBT Ticona
CELANEX 2003HR PBT Ticona
CELANEX 2004-2 PBT Ticona
CELANEX 2008 PBT Ticona
CELANEX 2016 PBT Ticona
CELANEX 2300 GV1/10 PBT-GF10 Ticona
CELANEX 2300 GV1/20 PBT-GF20 Ticona
CELANEX 2300 GV1/30 PBT-GF30 Ticona
CELANEX 2300 GV1/50 PBT-GF50 Ticona
CELANEX 2300 GV3/20 PBT-GB20 Ticona
CELANEX 2300 GV3/30 PBT-GB30 Ticona
CELANEX 2302 GV1/15 PBT-GF15 Ticona
CELANEX 2302 GV1/20 PBT-GF20 Ticona
CELANEX 2302 GV1/30 PBT-GF30 Ticona
CELANEX 2401 MT PBT Ticona
CELANEX 2402 MT PBT Ticona
CELANEX 2404 MT PBT Ticona
CELANEX 2500 PBT Ticona
CELANEX 3100-2 PBT-GF7 Ticona
CELANEX 3105H PBT-GF15 Ticona
CELANEX 3109HR PBT-GF7 Ticona
CELANEX 3116 PBT-GF7 Ticona
CELANEX 3200 PBT-GF15 Ticona
CELANEX 3200-2 PBT-GF15 Ticona
CELANEX 3200HR PBT-GF15 Ticona
CELANEX 3201 PBT-GF15 Ticona
CELANEX 3202-2 PBT Ticona
CELANEX 3209HR PBT Ticona
CELANEX 3209HRT PBT-GF15 Ticona
CELANEX 3216 PBT-GF15 Ticona
CELANEX 3225HRT PBT-GF15 Ticona
CELANEX 3226 PBT Ticona
CELANEX 3300 PBT-GF30 Ticona
CELANEX 3300-2 PBT-GF30 Ticona
CELANEX 3300-2LM PBT Ticona
CELANEX 3300D PBT-GF30 Ticona
CELANEX 3300HR PBT-GF30 Ticona
CELANEX 3300LM PBT-GF30 Ticona
CELANEX 3309HR PBT-GF30 Ticona
CELANEX 3309HRHF PBT-GF30 Ticona
CELANEX 3309HRLM PBT-GF30 Ticona
CELANEX 3309HRT PBT-GF30 Ticona
CELANEX 3316 PBT-GF30 Ticona
CELANEX 3316CT PBT-(GF+MD)50 Ticona
CELANEX 3318 PBT-GF30 Ticona
CELANEX 3325HRT PBT-GF30 Ticona
CELANEX 3400-2 PBT-GF40 Ticona
CELANEX 3409HR PBT-GF40 Ticona
CELANEX 3425HRT PBT Ticona
CELANEX 4016 PBT Ticona
CELANEX 4022 PBT Ticona
CELANEX 4202 PBT-GF15 Ticona
CELANEX 4300 PBT-GF30 Ticona
CELANEX 4300LM PBT-GF30 Ticona
CELANEX 4302 PBT-GF30 Ticona
CELANEX 4302HS PBT-GF30 Ticona
CELANEX 4302LM PBT-GF30 Ticona
CELANEX 4305 PBT-GF33 Ticona
CELANEX 4306 PBT-GF30 Ticona
CELANEX 5200-2 PBT-GF15 Ticona
CELANEX 5202 PBT-GF15 Ticona
CELANEX 5202HF PBT-GF15 Ticona
CELANEX 5205HG PBT-GF15 Ticona
CELANEX 5214HF PBT-GF15 Ticona
CELANEX 5300-2 PBT-GF30 Ticona
CELANEX 5300-2UV PBT-GF30 Ticona
CELANEX 531HS PBT Ticona
CELANEX 602AC PBT Ticona
CELANEX 6035GB20 PBT-GB20 Ticona
CELANEX 6400-2 PBT Ticona
CELANEX 6402R PBT-(GF+MX)40 Ticona
CELANEX 6406 PBT-(GF+P)40 Ticona
CELANEX 6407 PBT-(GF+P)30 Ticona
CELANEX 6407HR PBT-(GF+P)30 Ticona
CELANEX 6500 PBT-(GF+P)30 Ticona
CELANEX 6500HF PBT Ticona
CELANEX 6500HR PBT Ticona
CELANEX 6500LM PBT-(GF+P)30 Ticona
CELANEX 7316 PBT-(GF+P)35 Ticona
CELANEX 733LD PBT Ticona
CELANEX 7407 PBT-GF40 Ticona
CELANEX 7714 PBT Ticona
CELANEX 7716 PBT-(GF+P)35 Ticona
CELANEX D3200LC PBT Ticona
CELANEX J235 PBT Ticona
CELANEX J600 PBT-(GF+P)40 Ticona
CELANEX LW2333R PBT-(GB+GF)50 Ticona
CELANEX LW2547W PBT-(GF+MX)30 Ticona
CELANEX XFR 4840 PBT Ticona
CELANEX XFR 4840 10/0242 Black PBT Ticona
CELANEX XFR 6842 GF10 PBT-GF30 Ticona
CELANEX XFR 6842 GF15 PBT-GF30 Ticona
CELANEX XFR 6842 GF20 PBT-GF30 Ticona
CELANEX XFR 6842 GF30 PBT-GF30 Ticona
CELCON CF802 POM Ticona
CELCON GB10 POM-GB10 Ticona
CELCON GB25 POM-GB25 Ticona
CELCON GC10 POM-GF10 Ticona
CELCON GC15 POM-GF15 Ticona
CELCON GC20 POM-GF20 Ticona
CELCON GC25A POM-GF25 Ticona
CELCON GC25T POM-GF25 Ticona
CELCON GC25TF POM-GF25 Ticona
CELCON GC90UV POM-GF10 Ticona
CELCON LM90Z POM Ticona
CELCON LU-02 POM Ticona
CELCON LW25-S2 POM Ticona
CELCON LW90 POM Ticona
CELCON LW90-F2 POM Ticona
CELCON LW90-S2 POM Ticona
CELCON LW90-SC POM Ticona
CELCON LW90FS-K POM Ticona
CELCON M140 POM Ticona
CELCON M140-L1 POM Ticona
CELCON M15HP POM Ticona
CELCON M25 POM Ticona
CELCON M25UV POM Ticona
CELCON M270 POM Ticona
CELCON M270UV POM Ticona
CELCON M450 POM Ticona
CELCON M50 POM Ticona
CELCON M90 POM Ticona
CELCON M90-07 POM Ticona
CELCON M90-34 POM Ticona
CELCON M90-45H POM Ticona
CELCON M90-45XAP® POM Ticona
CELCON M90AW POM Ticona
CELCON M90SW POM Ticona
CELCON M90UV POM Ticona
CELCON MC270 POM-MD Ticona
CELCON MC270-HM POM-MD Ticona
CELCON MC90 POM-MD Ticona
CELCON MC90-HM POM-MD Ticona
CELCON MR25B POM Ticona
CELCON MR270B POM Ticona
CELCON MR50B POM Ticona
CELCON MR90B POM Ticona
CELCON UV140LG POM Ticona
CELCON UV25Z POM Ticona
CELCON UV270Z POM Ticona
CELCON UV90Z POM Ticona
CELCON WR25Z POM Ticona
CELCON WR90Z POM Ticona
Cellidor B 500-05 C ALBIS Plastic GmbH
Cellidor B 500-10 C ALBIS Plastic GmbH
Cellidor B 500-15 C ALBIS Plastic GmbH
Cellidor B 500-20 C ALBIS Plastic GmbH
Cellidor B 531-07 C ALBIS Plastic GmbH
Cellidor B 531-10 C ALBIS Plastic GmbH
Cellidor B 631-10 C ALBIS Plastic GmbH
Cellidor CP 2810-11 C ALBIS Plastic GmbH
Cellidor CP 300-10 C ALBIS Plastic GmbH
Cellidor CP 300-13 C ALBIS Plastic GmbH
Cellidor CP 300-15 C ALBIS Plastic GmbH
Cellidor CP 300-17 C ALBIS Plastic GmbH
Cellidor CP 300-20 C ALBIS Plastic GmbH
Cellidor CP 310-10 C ALBIS Plastic GmbH
Cellidor CP 3406-08 C ALBIS Plastic GmbH
Cellidor CP 3406-11 C ALBIS Plastic GmbH
Cellidor CP 400-08 C ALBIS Plastic GmbH
Cellidor CP 400-08 GF25 C-GF25 ALBIS Plastic GmbH
Cellidor CP 400-10 C ALBIS Plastic GmbH
Cellidor CP 400-12 C ALBIS Plastic GmbH
Cellidor CP 400-15 C ALBIS Plastic GmbH
Cellidor CP 400-17 C ALBIS Plastic GmbH
Cellidor CP 410-10 C ALBIS Plastic GmbH
Cellidor CP 430-13 AG C ALBIS Plastic GmbH
CELSTRAN +PP-GF30-04CN02/10 PP-GF30 Ticona
CELSTRAN +PP-GF30-05CN01/10 PP-GF30 Ticona
CELSTRAN +PP-GF40-04CN03 PP-GF40 Ticona
CELSTRAN +PP-GF40-04CN03/10 PP-GF40 Ticona
CELSTRAN +PP-GF40-04CN15/10 PP-GF40 Ticona
CELSTRAN +PP-GF45-05X551/1X PP-GF45 Ticona
CELSTRAN +PP-GF60-04CN15/10 PP-GF60 Ticona
CELSTRAN PA6-GF30-01 PA6-GF30 Ticona
CELSTRAN PA6-GF40-01 PA6-GF40 Ticona
CELSTRAN PA6-GF40-03 PA6-GF40 Ticona
CELSTRAN PA6-GF50-01 PA6-GF50 Ticona
CELSTRAN PA6-GF50-03 PA6-GF50 Ticona
CELSTRAN PA6-GF60-01 PA6-GF60 Ticona
CELSTRAN PA6-GF60-03 PA6-GF60 Ticona
CELSTRAN PA66-AF35-02-US PA66-RF35 Ticona
CELSTRAN PA66-CF40-01-US PA66-CF40 Ticona
CELSTRAN PA66-GF20-02P11/12 PA66-GF20 Ticona
CELSTRAN PA66-GF30-02 PA66-GF30 Ticona
CELSTRAN PA66-GF30-07 PA66-GF30 Ticona
CELSTRAN PA66-GF40-01 PA66-GF40 Ticona
CELSTRAN PA66-GF40-0101P10/11 PA666-GF40 Ticona
CELSTRAN PA66-GF40-02-US PA66-GF40 Ticona
CELSTRAN PA66-GF40-02P11 PA66-GF40 Ticona
CELSTRAN PA66-GF40-02P11/15 PA66-GF40 Ticona
CELSTRAN PA66-GF40-07 PA66-GF40 Ticona
CELSTRAN PA66-GF40-BV340C P11/3x PA66-GF40 Ticona
CELSTRAN PA66-GF50-0111P10 PA666-GF50 Ticona
CELSTRAN PA66-GF50-0111P10/11 PA666-GF50 Ticona
CELSTRAN PA66-GF50-0111P10/30478 PA666-GF50 Ticona
CELSTRAN PA66-GF50-0111P7.5/11 PA666-GF50 Ticona
CELSTRAN PA66-GF50-0112P7,5/10 PA666-GF50 Ticona
CELSTRAN PA66-GF50-02 AD3007 PA66-GF50 Ticona
CELSTRAN PA66-GF50-02 P11 PA66-GF50 Ticona
CELSTRAN PA66-GF50-02 P11/14 PA66-GF50 Ticona
CELSTRAN PA66-GF50-02 P7 PA66-GF50 Ticona
CELSTRAN PA66-GF50-02 P7/12 PA66-GF50 Ticona
CELSTRAN PA66-GF50-02-US PA66-GF50 Ticona
CELSTRAN PA66-GF50-07 PA66-GF50 Ticona
CELSTRAN PA66-GF50-20 PA66-GF50 Ticona
CELSTRAN PA66-GF50-20 AD3007 PA66-GF50 Ticona
CELSTRAN PA66-GF60-0101P10 PA666-GF60 Ticona
CELSTRAN PA66-GF60-0104P10/11 PA666-GF60 Ticona
CELSTRAN PA66-GF60-02 P11/12 PA66-GF60 Ticona
CELSTRAN PA66-GF60-02 P11/14 PA66-GF60 Ticona
CELSTRAN PA66-GF60-02-US PA66-GF60 Ticona
CELSTRAN PA66-SF10-02 PA66-MF(x)10 Ticona
CELSTRAN PA66-SF50-02 AF3001 PA66-MF(x)50 Ticona
CELSTRAN PA66-SF6-02 PA66-MF(x)6 Ticona
CELSTRAN PBT-CF40-08 PBT-CF40 Ticona
CELSTRAN PBT-GF30-08 PBT-GF30 Ticona
CELSTRAN PBT-GF40-08 PBT-GF40 Ticona
CELSTRAN PBT-GF50-08 PBT-GF50 Ticona
CELSTRAN PEHD-GF40-01 (PE-HD)-GF40 Ticona
CELSTRAN PEHD-GF60-01-US (PE-HD)-GF60 Ticona
CELSTRAN PP-GF25-0403 P10/10 PP-GF25 Ticona
CELSTRAN PP-GF30-02 PP-GF30 Ticona
CELSTRAN PP-GF30-03 PP-GF30 Ticona
CELSTRAN PP-GF30-04 PP-GF30 Ticona
CELSTRAN PP-GF30-0403 P10 PP-GF30 Ticona
CELSTRAN PP-GF30-0403 P10/10 PP-GF30 Ticona
CELSTRAN PP-GF30-0405 P10/10 PP-GF30 Ticona
CELSTRAN PP-GF30-0453 P10/10 PP-GF30 Ticona
CELSTRAN PP-GF30-05 PP-GF30 Ticona
CELSTRAN PP-GF30-0501 P8/13 PP-GF30 Ticona
CELSTRAN PP-GF30-0501P10 PP-GF30 Ticona
CELSTRAN PP-GF30-0501P10/13 PP-GF30 Ticona
CELSTRAN PP-GF30-10 PP-GF30 Ticona
CELSTRAN PP-GF40-02 PP-GF40 Ticona
CELSTRAN PP-GF40-03 PP-GF40 Ticona
CELSTRAN PP-GF40-04 PP-GF40 Ticona
CELSTRAN PP-GF40-0405 P10/10 PP-GF40 Ticona
CELSTRAN PP-GF40-0414 P10 PP-GF40 Ticona
CELSTRAN PP-GF40-0414 P7/10 PP-GF40 Ticona
CELSTRAN PP-GF40-0414P10/10 PP-GF40 Ticona
CELSTRAN PP-GF40-05 PP-GF40 Ticona
CELSTRAN PP-GF40-0501 P10/13 PP-GF40 Ticona
CELSTRAN PP-GF40-10 PP-GF40 Ticona
CELSTRAN PP-GF45M15-04CN15/10 PP-(GF+MF)60 Ticona
CELSTRAN PP-GF50-02 PP-GF50 Ticona
CELSTRAN PP-GF50-03 PP-GF50 Ticona
CELSTRAN PP-GF50-0403 P10 PP-GF50 Ticona
CELSTRAN PP-GF50-0403P10/10 PP-GF50 Ticona
CELSTRAN PP-GF50-0405P10/10 PP-GF50 Ticona
CELSTRAN PP-GF50-0453P10/10 PP-GF50 Ticona
CELSTRAN PP-GF50-0455P10/10 PP-GF50 Ticona
CELSTRAN PP-GF50-0458 P10/10 PP-GF50 Ticona
CELSTRAN PP-GF50-10 PP-GF50 Ticona
CELSTRAN PPS-AF35-01-US PPS-RF35 Ticona
CELSTRAN PPS-GF30-01 PPS-GF30 Ticona
CELSTRAN PPS-GF40-01 PPS-GF40 Ticona
CELSTRAN PPS-GF50-01-US PPS-GF50 Ticona
CELSTRAN PPS-SF6-01 AF3005 Natural PPS... Ticona
CELSTRAN TPU-CF40-01 TPU-CF40 Ticona
CELSTRAN TPU-GF30-01-US TPU-GF30 Ticona
CELSTRAN TPU-GF40-01-US TPU-GF40 Ticona
CELSTRAN TPU-GF50-01-US TPU-GF50 Ticona
CELSTRAN TPU-GF60-01-US TPU-GF60 Ticona
COMPEL PP-GF30-04 PP Ticona
Crastin® 6129 NC010 PBT DuPont Engineering Polymers
Crastin® 6129C NC010 PBT DuPont Engineering Polymers
Crastin® 6130 NC010 PBT DuPont Engineering Polymers
Crastin® 6130C NC010 PBT DuPont Engineering Polymers
Crastin® 6131 NC010 PBT DuPont Engineering Polymers
Crastin® 6131C NC010 PBT DuPont Engineering Polymers
Crastin® 6134 NC010 PBT DuPont Engineering Polymers
Crastin® BM6450XD BK560 PBT DuPont Engineering Polymers
Crastin® CE15315 NC010 PBT-GF15 FR(17) DuPont Engineering Polymers
Crastin® CE15330 NC010 PBT-GF30 FR(17) DuPont Engineering Polymers
Crastin® CE2055 NC010 PBT DuPont Engineering Polymers
Crastin® CE2061 BK560 PBT-GF20 DuPont Engineering Polymers
Crastin® CE2548 GY740 PBT-I-MD20 DuPont Engineering Polymers
Crastin® FG6129 NC010 PBT DuPont Engineering Polymers
Crastin® FG6130 NC010 PBT DuPont Engineering Polymers
Crastin® FGS600F40 NC010 PBT DuPont Engineering Polymers
Crastin® HR5315HF NC010 PBT-I-GF15 DuPont Engineering Polymers
Crastin® HR5330HF NC010 PBT-I-GF30 DuPont Engineering Polymers
Crastin® HTI668FR NC010 PBT-(MD+GF)45 FR(17) DuPont Engineering Polymers
Crastin® LW9020 NC010 (PBT+ASA)-GF20 DuPont Engineering Polymers
Crastin® LW9020FR NC010 (PBT+ASA)-GF20 FR(17) DuPont Engineering Polymers
Crastin® LW9030 NC010 (PBT+ASA)-GF30 DuPont Engineering Polymers
Crastin® LW9030FR NC010 (PBT+ASA)-GF30 FR(17) DuPont Engineering Polymers
Crastin® LW9320 NC010 (PBT+SAN)-I-GF20 DuPont Engineering Polymers
Crastin® LW9320LM BK591 (PBT+SAN)-I-GF20 DuPont Engineering Polymers
Crastin® LW9330 NC010 (PBT+SAN)-I-GF30 DuPont Engineering Polymers
Crastin® S600F10 NC010 PBT DuPont Engineering Polymers
Crastin® S600F20 NC010 PBT DuPont Engineering Polymers
Crastin® S600F40 NC010 PBT DuPont Engineering Polymers
Crastin® S600LF NC010 PBT DuPont Engineering Polymers
Crastin® S610SF BK851 PBT DuPont Engineering Polymers
Crastin® S620F20 NC010 PBT DuPont Engineering Polymers
Crastin® SK601 NC010 PBT-GF10 DuPont Engineering Polymers
Crastin® SK602 NC010 PBT-GF15 DuPont Engineering Polymers
Crastin® SK603 NC010 PBT-GF20 DuPont Engineering Polymers
Crastin® SK605 NC010 PBT-GF30 DuPont Engineering Polymers
Crastin® SK608 BK509 PBT-GF45 DuPont Engineering Polymers
Crastin® SK609 NC010 PBT-GF50 DuPont Engineering Polymers
Crastin® SK612SF NC010 PBT-GF15 DuPont Engineering Polymers
Crastin® SK615SF NC010 PBT-GF30 DuPont Engineering Polymers
Crastin® SK641FR NC010 PBT-GF10 FR(17) DuPont Engineering Polymers
Crastin® SK642FR NC010 PBT-GF15 FR(17) DuPont Engineering Polymers
Crastin® SK643FR NC010 PBT-GF20 FR(17) DuPont Engineering Polymers
Crastin® SK645FR NC010 PBT-GF30 FR(17) DuPont Engineering Polymers
Crastin® SO653 NC010 PBT-GB20 DuPont Engineering Polymers
Crastin® ST820 NC010 PBT-I DuPont Engineering Polymers
Crastin® ST830FRUV NC010 PBT-I FR(17) DuPont Engineering Polymers
Crastin® T835FRUV NC010 PBT-I-GF5 FR(17) DuPont Engineering Polymers
Crastin® T845FR NC010 PBT-GF30 FR(17) DuPont Engineering Polymers
CYROLITE® CG-97 (MBS) Evonik Röhm GmbH
CYROLITE® G 20 (MBS) Evonik Röhm GmbH
CYROLITE® G 20 HIFLO (MBS) Evonik Röhm GmbH
CYROLITE® GS 90 (MBS) Evonik Röhm GmbH
CYROLITE® Med 2 (MBS) Evonik Röhm GmbH