Grade Name Family Producer
Technylstar™ S 216 L2 V30 BLACK PA6-GF30 Rhodia Polyamide Engineering Plastics
Technylstar™ S 216 V30 PA6-GF30 Rhodia Polyamide Engineering Plastics
Technylstar™ S 216 V35 PA6-GF35 Rhodia Polyamide Engineering Plastics
Technylstar™ S 218 MT40 PA6-MD40 Rhodia Polyamide Engineering Plastics
Technylstar™ S 218 V30 PA6-GF30 Rhodia Polyamide Engineering Plastics
Technylstar™ S 60G1 V30 PA6-GF30 FR Rhodia Polyamide Engineering Plastics
Technylstar™ SX 216 V50 PA6-GF50 Rhodia Polyamide Engineering Plastics
Technylstar™ SX 218 V50 PA6-GF50 Rhodia Polyamide Engineering Plastics
Technylstar™ SX 218 V60 PA6-GF60 Rhodia Polyamide Engineering Plastics
Technyl® 2710IR PA66-I Rhodia Polyamide Engineering Plastics
Technyl® A 20 V25 PA66-GF25 FR Rhodia Polyamide Engineering Plastics
Technyl® A 20 V35 PA66-GF35 FR Rhodia Polyamide Engineering Plastics
Technyl® A 205F PA66 Rhodia Polyamide Engineering Plastics
Technyl® A 208F PA66 Rhodia Polyamide Engineering Plastics
Technyl® A 21 T3 V25 PA66-GF25 Rhodia Polyamide Engineering Plastics
Technyl® A 216 PA66 Rhodia Polyamide Engineering Plastics
Technyl® A 216 NAT FA PA66 Rhodia Polyamide Engineering Plastics
Technyl® A 216 S30 PA66-GB30 Rhodia Polyamide Engineering Plastics
Technyl® A 216 S40 PA66-GB40 Rhodia Polyamide Engineering Plastics
Technyl® A 216 V20 PA66-GF20 Rhodia Polyamide Engineering Plastics
Technyl® A 216 V30 PA66-GF30 Rhodia Polyamide Engineering Plastics
Technyl® A 216 V30 Natural FA PA66-GF30 Rhodia Polyamide Engineering Plastics
Technyl® A 216 V33 PA66-GF33 Rhodia Polyamide Engineering Plastics
Technyl® A 216T V33 BLACK 1N PA66-GF33 Rhodia Polyamide Engineering Plastics
Technyl® A 217 PA66 Rhodia Polyamide Engineering Plastics
Technyl® A 218 PA66 Rhodia Polyamide Engineering Plastics
Technyl® A 218 MZ15 V25 PA66-(GF+MF)40 Rhodia Polyamide Engineering Plastics
Technyl® A 218 S30 PA66-GB30 Rhodia Polyamide Engineering Plastics
Technyl® A 218 S40 PA66-GB40 Rhodia Polyamide Engineering Plastics
Technyl® A 218 V15 PA66-GF15 Rhodia Polyamide Engineering Plastics
Technyl® A 218 V20 PA66-GF20 Rhodia Polyamide Engineering Plastics
Technyl® A 218 V25 PA66-GF25 Rhodia Polyamide Engineering Plastics
Technyl® A 218 V25 black 21NHFE PA66-GF25 Rhodia Polyamide Engineering Plastics
Technyl® A 218 V25 Nat BA PA66-GF25 Rhodia Polyamide Engineering Plastics
Technyl® A 218 V25 Natural B PA66-GF25 Rhodia Polyamide Engineering Plastics
Technyl® A 218 V30 PA66-GF30 Rhodia Polyamide Engineering Plastics
Technyl® A 218 V30 Black 21 NHFE PA66-GF30 Rhodia Polyamide Engineering Plastics
Technyl® A 218 V30 black 34NG PA66-GF30 Rhodia Polyamide Engineering Plastics
Technyl® A 218 V30 Black 34NG-K PA66-GF30 Rhodia Polyamide Engineering Plastics
Technyl® A 218 V35 PA66-GF35 Rhodia Polyamide Engineering Plastics
Technyl® A 218 V35 black 21NHFE PA66-GF35 Rhodia Polyamide Engineering Plastics
Technyl® A 218 V35 black 34NG PA66-GF35 Rhodia Polyamide Engineering Plastics
Technyl® A 218 V40 PA66-GF40 Rhodia Polyamide Engineering Plastics
Technyl® A 218 V40 black 21NHFE PA66-GF40 Rhodia Polyamide Engineering Plastics
Technyl® A 218 V50 PA66-GF50 Rhodia Polyamide Engineering Plastics
Technyl® A 218C V10 PA66-GF10 Rhodia Polyamide Engineering Plastics
Technyl® A 218G V30 PA66-GF30 Rhodia Polyamide Engineering Plastics
Technyl® A 218G V33 BLACK 34N PA66-GF33 Rhodia Polyamide Engineering Plastics
Technyl® A 218G1 V25 BLACK 34N PA66-GF25 Rhodia Polyamide Engineering Plastics
Technyl® A 218G1 V30 BLACK 34N PA66-GF30 Rhodia Polyamide Engineering Plastics
Technyl® A 218G2 V30 BLACK 34N PA66-GF30 Rhodia Polyamide Engineering Plastics
Technyl® A 218HP V30 black 21N PA66-GF30 Rhodia Polyamide Engineering Plastics
Technyl® A 218HP V35 black 21N PA66-GF35 Rhodia Polyamide Engineering Plastics
Technyl® A 218HP V50 black 21N PA66-GF50 Rhodia Polyamide Engineering Plastics
Technyl® A 218W V30 PA66-GF30 Rhodia Polyamide Engineering Plastics
Technyl® A 218W V30 black FA PA66-GF30 Rhodia Polyamide Engineering Plastics
Technyl® A 218W V33 Natural T PA66-GF33 Rhodia Polyamide Engineering Plastics
Technyl® A 221 PA66 Rhodia Polyamide Engineering Plastics
Technyl® A 221 Natural FA PA66 Rhodia Polyamide Engineering Plastics
Technyl® A 222 PA66 Rhodia Polyamide Engineering Plastics
Technyl® A 225F PA66 Rhodia Polyamide Engineering Plastics
Technyl® A 230 PA66 Rhodia Polyamide Engineering Plastics
Technyl® A 238 PA66 Rhodia Polyamide Engineering Plastics
Technyl® A 238 V13 PA66-GF13 Rhodia Polyamide Engineering Plastics
Technyl® A 246M PA66 Rhodia Polyamide Engineering Plastics
Technyl® A 248 V33 PA66-GF33 Rhodia Polyamide Engineering Plastics
Technyl® A 258 P1 Black 2N PA66 Rhodia Polyamide Engineering Plastics
Technyl® A 30G1 PA66 FR Rhodia Polyamide Engineering Plastics
Technyl® A 30H1 V25 PA66-GF25 FR Rhodia Polyamide Engineering Plastics
Technyl® A 30H1 V30 PA66-GF30 FR Rhodia Polyamide Engineering Plastics
Technyl® A 32G1 PA66 Rhodia Polyamide Engineering Plastics
Technyl® A 402 PA66 Rhodia Polyamide Engineering Plastics
Technyl® A 402 H1 PA66 Rhodia Polyamide Engineering Plastics
Technyl® A 402 Natural FA PA66 Rhodia Polyamide Engineering Plastics
Technyl® A 50H1 PA66 FR Rhodia Polyamide Engineering Plastics
Technyl® A 52 G1 MX 20 PA66-MF Rhodia Polyamide Engineering Plastics
Technyl® A 548B V15 Black 23N PA666-GF15 Rhodia Polyamide Engineering Plastics
Technyl® A 548B2 V15 Black 23N PA66-GF15 Rhodia Polyamide Engineering Plastics
Technyl® A 60 G1 V25 PA66-GF25 FR Rhodia Polyamide Engineering Plastics
Technyl® A 60 G2 V30 PA66-GF30 FR Rhodia Polyamide Engineering Plastics
Technyl® A 60G1 V30 PA66-GF30 FR Rhodia Polyamide Engineering Plastics
Technyl® A 718 V30 PA66-GF30 Rhodia Polyamide Engineering Plastics
Technyl® AFX 218 V50 PA66-GF50 Rhodia Polyamide Engineering Plastics
Technyl® AFX 218 V60 PA66-GF60 Rhodia Polyamide Engineering Plastics
Technyl® AR 130/GF BLACK PA66-GF30 Rhodia Polyamide Engineering Plastics
Technyl® AR 218 V30 Black PA66-GF30 Rhodia Polyamide Engineering Plastics
Technyl® B 216 Nat D PA666 Rhodia Polyamide Engineering Plastics
Technyl® B 216 V30 PA666-GF30 Rhodia Polyamide Engineering Plastics
Technyl® B 218 PA666 Rhodia Polyamide Engineering Plastics
Technyl® B 218 V30 PA666-GF30 Rhodia Polyamide Engineering Plastics
Technyl® B 218L V20 BLACK 44 N PA666-GF20 Rhodia Polyamide Engineering Plastics
Technyl® B 218L V30 BLACK 44 N PA666-GF30 Rhodia Polyamide Engineering Plastics
Technyl® B 230 PA666 Rhodia Polyamide Engineering Plastics
Technyl® B 238 PA666 Rhodia Polyamide Engineering Plastics
Technyl® B 50H1 PA666 FR Rhodia Polyamide Engineering Plastics
Technyl® C 206 PA6 Rhodia Polyamide Engineering Plastics
Technyl® C 216 PA6 Rhodia Polyamide Engineering Plastics
Technyl® C 216 V15 PA6-GF15 Rhodia Polyamide Engineering Plastics
Technyl® C 216 V30 PA6-GF30 Rhodia Polyamide Engineering Plastics
Technyl® C 216 V35 PA6-GF35 Rhodia Polyamide Engineering Plastics
Technyl® C 216 V40 PA6-GF40 Rhodia Polyamide Engineering Plastics
Technyl® C 216 V50 PA6-GF50 Rhodia Polyamide Engineering Plastics
Technyl® C 218 MZ20 V10 PA6-MD30 Rhodia Polyamide Engineering Plastics
Technyl® C 218 V15 PA6-GF15 Rhodia Polyamide Engineering Plastics
Technyl® C 218 V18 PA6-GF18 Rhodia Polyamide Engineering Plastics
Technyl® C 218 V30 PA6-GF30 Rhodia Polyamide Engineering Plastics
Technyl® C 218 V35 PA6-GF35 Rhodia Polyamide Engineering Plastics
Technyl® C 218 V45 PA6-GF45 Rhodia Polyamide Engineering Plastics
Technyl® C 218 V50 PA6-GF50 Rhodia Polyamide Engineering Plastics
Technyl® C 230 PA6 Rhodia Polyamide Engineering Plastics
Technyl® C 236SI PA6 Rhodia Polyamide Engineering Plastics
Technyl® C 246 V30 PA6-GF30 Rhodia Polyamide Engineering Plastics
Technyl® C 246M PA6 Rhodia Polyamide Engineering Plastics
Technyl® C 246SI V11 PA6-GF11 Rhodia Polyamide Engineering Plastics
Technyl® C 246SI V30 PA6-GF30 Rhodia Polyamide Engineering Plastics
Technyl® C 30H1 V30 PA6-GF30 FR Rhodia Polyamide Engineering Plastics
Technyl® C 402M PA6 Rhodia Polyamide Engineering Plastics
Technyl® C 442 BLACK V PA6-I Rhodia Polyamide Engineering Plastics
Technyl® C 502XT PA6 Rhodia Polyamide Engineering Plastics
Technyl® C 50H2 PA6 FR Rhodia Polyamide Engineering Plastics
Technyl® C 52G1 MX 25 Grey 7035 PA6-MF25 Rhodia Polyamide Engineering Plastics
Technyl® C 52G1 V20 PA6-GF20 Rhodia Polyamide Engineering Plastics
Technyl® C 52G1 V25 PA6-GF25 Rhodia Polyamide Engineering Plastics
Technyl® C 52G3 MZ25 PA6 Rhodia Polyamide Engineering Plastics
Technyl® C 52G4 MZ25 PA6-MF25 FR Rhodia Polyamide Engineering Plastics
Technyl® C 536XT PA6-I Rhodia Polyamide Engineering Plastics
Technyl® C 548B BLACK PA6-I Rhodia Polyamide Engineering Plastics
Technyl® C 548B V15 black PA6-GF15 Rhodia Polyamide Engineering Plastics
Technyl® CR 218 V30 black 1 N PA6-GF30 Rhodia Polyamide Engineering Plastics
Technyl® D 247F (PA66+PA610)-I Rhodia Polyamide Engineering Plastics
Technyl® eXten D 218 V30 PA610-GF30 Rhodia Polyamide Engineering Plastics
Technyl® eXten D 238 V30 PA610-I-GF30 Rhodia Polyamide Engineering Plastics
Technyl® eXten D 437P PA610 Rhodia Polyamide Engineering Plastics
Technyl® eXten D 458P PA610-I Rhodia Polyamide Engineering Plastics
Terblend® N NG-02 (ABS+PA6)-GF8 BASF
Terblend® N NG-02 EF (ABS+PA6)-GF8 BASF
Terblend® N NG-02 UV (ABS+PA6)-GF8 BASF
Terblend® N NG-04 (ABS+PA6)-GF20 BASF
Terblend® N NG-06 (ABS+PA6)-GF30 BASF
Terblend® N NM-11 (ABS+PA6) BASF
Terblend® N NM-12 (ABS+PA6) BASF
Terblend® N NM-12 UV (ABS+PA6) BASF
Terblend® N NM-13 (ABS+PA6) BASF
Terblend® N NM-19 (ABS+PA6) BASF
Terblend® N NM-19 XP (ABS+PA6) BASF
Terblend® N NM-21 EF (ABS+PA6) BASF
Terblend® N NMX04 (ABS+PA6) BASF
Terluran® GP-22 ABS BASF
Terluran® GP-35 ABS BASF
Terluran® HD-15 ABS BASF
Terluran® HH-112 ABS BASF
Terluran® HH-112 Q 457 ABS BASF
Terluran® HI-10 ABS BASF
Terluran® SP-6 ABS BASF
Terlux® 2802 HD MABS BASF
Terlux® 2802 TR MABS BASF
Terlux® 2812 HD MABS BASF
Terlux® 2812 TR MABS BASF
Terlux® 2822 HD MABS BASF
Texin® 185 TPU Bayer MaterialScience
Texin® 245 TPU Bayer MaterialScience
Texin® 250 TPU Bayer MaterialScience
Texin® 255 TPU Bayer MaterialScience
Texin® 260 TPU Bayer MaterialScience
Texin® 270 TPU Bayer MaterialScience
Texin® 285 TPU Bayer MaterialScience
Texin® 390 TPU Bayer MaterialScience
Texin® 4210 TPU Bayer MaterialScience
Texin® 4215 TPU Bayer MaterialScience
Texin® 945 U TPU Bayer MaterialScience
Texin® 950 TPU Bayer MaterialScience
Texin® 950 U TPU Bayer MaterialScience
Texin® 970 U TPU Bayer MaterialScience
Texin® 985 TPU Bayer MaterialScience
Texin® 985 U TPU Bayer MaterialScience
Texin® 990 TPU Bayer MaterialScience
Texin® 990 R TPU Bayer MaterialScience
Texin® DP7-1049 TPU Bayer MaterialScience
Texin® DP7-1050 TPU Bayer MaterialScience
Texin® DP7-1097 TPU Bayer MaterialScience
Texin® DP7-3007 TPU Bayer MaterialScience
THERMX CG023 PCT-GF20 Ticona
THERMX CG033 PCT-GF30 Ticona
THERMX CG923 PCT-GF20 Ticona
THERMX CG933 PCT-GF30 Ticona
THERMX TE3002 PCT-GF30 Ticona
THERMX TE4004 PCT-(GF+GX)40 Ticona
THERMX TE4005 PCT-(GF+MD)33 Ticona
TROGAMID BX7304 nc (nf) (PAIND/INDT+PA612) Evonik Industries AG
TROGAMID BX9724 blk (sw) (PAIND/INDT+PA66)-GF40 Evonik Industries AG
TROGAMID CX7323 nc (nf) PAIND/INDT Evonik Industries AG
TROGAMID CX9701 nc (nf) PAIND/INDT Evonik Industries AG
TROGAMID CX9704 PAIND/INDT Evonik Industries AG
TROGAMID CX9710 nc (nf) PAIND/INDT Evonik Industries AG
TROGAMID myCX PAIND/INDT Evonik Industries AG
TROGAMID T-GF35 nc (nf) PAIND/INDT-GF35 Evonik Industries AG
TROGAMID T5000 nc (nf) PAIND/INDT Evonik Industries AG
TROGAMID T5002 nc (nf) PAIND/INDT Evonik Industries AG
TROGAMID T5004 nc (nf) PAIND/INDT Evonik Industries AG
TROGAMID TX7389 nc (nf) PAIND/INDT Evonik Industries AG