CAMPUS® datasheet | Delrin® FG100TL NC010
This datasheet of Delrin® FG100TL NC010 from DuPont Engineering Polymers is provided by the international plastics database CAMPUS.
Delrin® FG100TL NC010 | POM | DuPont Engineering Polymers
Produkttext
Common features of Delrin® acetal resin include mechanical and physical properties such as high mechanical strength and rigidity, excellent fatigue and impact resistance, as well as resistance to moisture, gasoline, lubricants, solvents and many other neutral chemicals. Delrin® acetal resins also have excellent dimensional stability and good electrical insulating characteristics. They are naturally resilient, self-lubricating and available in a variety of colours and speciality grades.
The good melt stability of Delrin® acetal resin normally enables the recycling of properly handled production waste. If recycling is not possible, DuPont recommends, as the preferred option, incineration with energy recovery (-17 kJ/g of base polymer) in appropriately equipped installations. For disposal, local regulations have to be observed.
Delrin® acetal resin typically is used in demanding applications in the automotive, domestic appliances, sports, industrial engineering, electronics and consumer goods industries.
Delrin® FG100TL is a 1.5% Teflon® PTFE Micropowder filled, high viscosity acetal homopolymer for injection molding. It is specifically suitable for the food industry.
| Rheologische Eigenschaften | Wert | Einheit | Prüfnorm |
| Schmelzevolumenrate, MVR | 1.9 | cm³/10min | ISO 1133 |
| Temperatur | 190 | °C | ISO 1133 |
| Belastung | 2.16 | kg | ISO 1133 |
| Verarbeitungsschwindung, parallel | 1.8 | % | ISO 294-4, 2577 |
| Verarbeitungsschwindung, senkrecht | 1.7 | % | ISO 294-4, 2577 |
| Mechanische Eigenschaften | Wert | Einheit | Prüfnorm |
| Zug-Modul | 3000 | MPa | ISO 527-1/-2 |
| Streckspannung | 71 | MPa | ISO 527-1/-2 |
| Streckdehnung | 25 | % | ISO 527-1/-2 |
| Nominelle Bruchdehnung | 33 | % | ISO 527-1/-2 |
| Charpy-Schlagzähigkeit, +23°C | 150 | kJ/m² | ISO 179/1eU |
| Charpy-Kerbschlagzähigkeit, +23°C | 9 | kJ/m² | ISO 179/1eA |
| Charpy-Kerbschlagzähigkeit, -30°C | 8 | kJ/m² | ISO 179/1eA |
| Thermische Eigenschaften | Wert | Einheit | Prüfnorm |
| Schmelztemperatur, 10°C/min | 178 | °C | ISO 11357-1/-3 |
| Formbeständigkeitstemperatur, 1.80 MPa | 95 | °C | ISO 75-1/-2 |
| Formbeständigkeitstemperatur, 0.45 MPa | 158 | °C | ISO 75-1/-2 |
| Längenausdehnungskoeffizient, parallel | 110 | E-6/K | ISO 11359-1/-2 |
| Längenausdehnungskoeffizient, senkrecht | 110 | E-6/K | ISO 11359-1/-2 |
| Brennbarkeit bei nominal 1.5mm | HB | class | IEC 60695-11-10 |
| geprüfte Probekörperdicke | 1.5 | mm | IEC 60695-11-10 |
| Brennbarkeit bei Dicke h | HB | class | IEC 60695-11-10 |
| geprüfte Probekörperdicke | 0.8 | mm | IEC 60695-11-10 |
| Elektrische Eigenschaften | Wert | Einheit | Prüfnorm |
| Spezifischer Oberflächenwiderstand | >1E15 | Ohm | IEC 60093 |
| Vergleichszahl der Kriechwegbildung | 600 | - | IEC 60112 |
| Andere Eigenschaften | Wert | Einheit | Prüfnorm |
| Wasseraufnahme | 0.9 | % | Ähnlich ISO 62 |
| Feuchtigkeitsaufnahme | 0.2 | % | Ähnlich ISO 62 |
| Dichte | 1430 | kg/m³ | ISO 1183 |
| Kennwerte f. rheologische Berechn. | Wert | Einheit | Prüfnorm |
| Dichte der Schmelze | 1180 | kg/m³ | - |
Merkmale
Verarbeitungsmethoden
Spritzgießen
Lieferformen
Granulat
Regionale Verfügbarkeit
Haftungsausschluss
All data provided according to ISO 10350 for single points and ISO 11403 for multipoints.
Contact DuPont for Material Safety Data Sheet, general guides and/or additional information about ventilation, handling, purging, drying, etc.
Test temperatures are 23°C unless otherwise stated.
The DuPont Oval Logo, DuPont™, The miracles of science™ and ® are trademarks or registered trademarks of DuPont Company.
Copyright© 2011 E.I. du Pont de Nemours and Company. All Rights Reserved.
The information provided in this data sheet corresponds to our knowledge on the subject at the date of its publication.
This information may be subject to revision as new knowledge and experience becomes available.
The data provided fall within the normal range of product properties and relate only to the specific material designated; these data may not be
valid for such material used in combination with any other materials, additives or pigments or in any process, unless expressly indicated otherwise.
The data provided should not be used to establish specification limits or used alone as the basis of design; they are not intended to substitute
for any testing you may need to conduct to determine for yourself the suitability of a specific material for your particular purposes.
Since DuPont cannot anticipate all variations in actual end-use conditions DuPont makes no warranties and assumes no liability in connection
with any use of this information.
Nothing in this publication is to be considered as a license to operate under or a recommendation to infringe any patent rights.
DuPont advises you to seek independent counsel for a freedom to practice opinion on the intended application or end-use of our products.
CAUTION: DO NOT USE DUPONT MATERIALS IN MEDICAL APPLICATIONS INVOLVING IMPLANTATION IN THE HUMAN BODY OR
CONTACT WITH INTERNAL BODY FLUIDS OR TISSUES UNLESS THE MATERIAL HAS BEEN PROVIDED FROM DUPONT UNDER A
WRITTEN CONTRACT THAT IS CONSISTENT WITH DUPONT POLICY REGARDING MEDICAL APPLICATIONS AND EXPRESSLY
ACKNOWLEDGES THE CONTEMPLATED USE.
For further information, please contact your DuPont representative. You may also request a copy of DuPont POLICY Regarding Medical
Applications... H-50103-3 and DuPont CAUTION Regarding Medical Applications... H-50102-3.
Contact DuPont for Material Safety Data Sheet, general guides and/or additional information about ventilation, handling, purging, drying, etc.
Test temperatures are 23°C unless otherwise stated.
The DuPont Oval Logo, DuPont™, The miracles of science™ and ® are trademarks or registered trademarks of DuPont Company.
Copyright© 2011 E.I. du Pont de Nemours and Company. All Rights Reserved.
The information provided in this data sheet corresponds to our knowledge on the subject at the date of its publication.
This information may be subject to revision as new knowledge and experience becomes available.
The data provided fall within the normal range of product properties and relate only to the specific material designated; these data may not be
valid for such material used in combination with any other materials, additives or pigments or in any process, unless expressly indicated otherwise.
The data provided should not be used to establish specification limits or used alone as the basis of design; they are not intended to substitute
for any testing you may need to conduct to determine for yourself the suitability of a specific material for your particular purposes.
Since DuPont cannot anticipate all variations in actual end-use conditions DuPont makes no warranties and assumes no liability in connection
with any use of this information.
Nothing in this publication is to be considered as a license to operate under or a recommendation to infringe any patent rights.
DuPont advises you to seek independent counsel for a freedom to practice opinion on the intended application or end-use of our products.
CAUTION: DO NOT USE DUPONT MATERIALS IN MEDICAL APPLICATIONS INVOLVING IMPLANTATION IN THE HUMAN BODY OR
CONTACT WITH INTERNAL BODY FLUIDS OR TISSUES UNLESS THE MATERIAL HAS BEEN PROVIDED FROM DUPONT UNDER A
WRITTEN CONTRACT THAT IS CONSISTENT WITH DUPONT POLICY REGARDING MEDICAL APPLICATIONS AND EXPRESSLY
ACKNOWLEDGES THE CONTEMPLATED USE.
For further information, please contact your DuPont representative. You may also request a copy of DuPont POLICY Regarding Medical
Applications... H-50103-3 and DuPont CAUTION Regarding Medical Applications... H-50102-3.
The CAMPUS internet database is hosted by M-Base Engineering + Software GmbH.
M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors.
Any decision about the application of materials must be double checked with the producer of this material.
CAMPUS® is a registered trademark of CWFG mbH, Frankfurt am Main, 2012
CAMPUS® is a registered trademark of CWFG mbH, Frankfurt am Main, 2012