View list of
Creating a Property Table?
- All ALBIS Plastic grades
- All PC grades
- All grades beginning with A
FREE DOWNLOAD
Interested inCreating a Property Table?
The CAMPUS desktop version
offers extended functionality!CAMPUS® datasheet | ALTECH PC A 1000227
This datasheet of ALTECH PC A 1000227 from ALBIS Plastic GmbH is provided by the international plastics database CAMPUS.
CAMPUS is organized by a group of leading international resin producers, who have agreed to test their material according to uniform conditions, based on ISO standards (ISO 10350, ISO 11403), in order to offer comparable data to the market.
You may contact the supplier for more information about this grade.
ALTECH PC A 1000/227 | PC | ALBIS Plastic GmbH
| Rheological properties | Value | Unit | Test Standard |
| Melt volume-flow rate (MVR) | 20 | cm³/10min | ISO 1133 |
| Temperature | 300 | °C | ISO 1133 |
| Load | 1.2 | kg | ISO 1133 |
| Mechanical properties | Value | Unit | Test Standard |
| Tensile Modulus | 2400 | MPa | ISO 527-1/-2 |
| Yield stress | 60 | MPa | ISO 527-1/-2 |
| Yield strain | 6 | % | ISO 527-1/-2 |
| Charpy impact strength (+23°C) | N | kJ/m² | ISO 179/1eU |
| Charpy notched impact strength (+23°C) | 11.5 | kJ/m² | ISO 179/1eA |
| Thermal properties | Value | Unit | Test Standard |
| Temp. of deflection under load (1.80 MPa) | 127 | °C | ISO 75-1/-2 |
| Vicat softening temperature (50°C/h 50N) | 146 | °C | ISO 306 |
| Other properties | Value | Unit | Test Standard |
| Density | 1190 | kg/m³ | ISO 1183 |
Characteristics
Processing
Injection Molding
Special Characteristics
U.V. stabilized or stable to weather
Regional Availability
North America, Europe, Asia Pacific, South and Central America, Near East/Africa
Disclaimer
Any information given on the chemical and physical characteristics of our products, including technical advice on applications whether verbally, in writing or by testing the product, is given to the best of our knowledge, but without warranty. It does not exempt the buyer from carrying out his own investigations and tests in order to ascertain the products' specific suitability for the purpose intended. The buyer is solely responsible for the application, utilisation and processing of the products, and must observe the laws and government regulations and the consequential rights of any third party. At all times our Conditions of Sale apply. The test values given are guide values, not binding minimum or maximum figures, which have been determined on standardized test specimen and can be affected by pigmentation, mold design and processing conditions.
The CAMPUS internet database is hosted by M-Base Engineering + Software GmbH.
M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors.
Any decision about the application of materials must be double checked with the producer of this material.
CAMPUS® is a Registered trademark of CWFG mbH, Frankfurt/Main, 1991
CAMPUS® is a Registered trademark of CWFG mbH, Frankfurt/Main, 1991