This datasheet includes:

  ALTECH PC B 1000/588 UV AS | PC | ALBIS Plastic GmbH
Rheological propertiesValueUnitTest Standard
Melt volume-flow rate (MVR) 22 cm³/10min ISO 1133
Temperature 300 °C ISO 1133
Load 1.2 kg ISO 1133
Mechanical propertiesValueUnitTest Standard
Tensile Modulus 2700 MPa ISO 527-1/-2
Stress at break 68 MPa ISO 527-1/-2
Strain at break 12 % ISO 527-1/-2
Charpy impact strength (+23°C) N kJ/m² ISO 179/1eU
Charpy notched impact strength (+23°C) 7.5 kJ/m² ISO 179/1eA
Thermal propertiesValueUnitTest Standard
Temp. of deflection under load (1.80 MPa) 121 °C ISO 75-1/-2
Vicat softening temperature (50°C/h 50N) 134 °C ISO 306
Other propertiesValueUnitTest Standard
Density 1240 kg/m³ ISO 1183
Characteristics
Processing
Injection Molding
Special Characteristics
U.V. stabilized or stable to weather
Regional Availability
North America, Europe, Asia Pacific, South and Central America, Near East/Africa
Disclaimer
Any information given on the chemical and physical characteristics of
our products, including technical advice on applications whether
verbally, in writing or by testing the product, is given to the best
of our knowledge, but without warranty. It does not exempt the buyer
from carrying out his own investigations and tests in order to
ascertain the products' specific suitability for the purpose intended.

The buyer is solely responsible for the application, utilisation and
processing of the products, and must observe the laws and government
regulations and the consequential rights of any third party. At all
times our Conditions of Sale apply.

The test values given are guide values, not binding minimum or maximum
figures, which have been determined on standardized test specimen and
can be affected by pigmentation, mold design and processing conditions.

The CAMPUS internet database is hosted by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

CAMPUS® is a Registered trademark of CWFG mbH, Frankfurt/Main, 1991