View list of
VDA CAMPUS Datasheet?
FREE DOWNLOAD
Interested inVDA CAMPUS Datasheet?
The CAMPUS desktop version
offers extended functionality!CAMPUS® datasheet | Akulon® F126-C
This datasheet of Akulon® F126-C from DSM Engineering Plastics is provided by the international plastics database CAMPUS.
CAMPUS is organized by a group of leading international resin producers, who have agreed to test their material according to uniform conditions, based on ISO standards (ISO 10350, ISO 11403), in order to offer comparable data to the market.
Akulon® F126-C | PA6 | DSM Engineering Plastics
Product Texts
| Thermal properties | dry / cond | Unit | Test Standard |
| Melting temperature (10°C/min) | 220 / * | °C | ISO 11357-1/-3 |
| Coeff. of linear therm. expansion (parallel) | 90 / * | E-6/K | ISO 11359-1/-2 |
| Coeff. of linear therm. expansion (normal) | 100 / * | E-6/K | ISO 11359-1/-2 |
| Other properties | dry / cond | Unit | Test Standard |
| Water absorption | 9.5 / * | % | Sim. to ISO 62 |
| Humidity absorption | 2.5 / * | % | Sim. to ISO 62 |
| Density | 1130 / - | kg/m³ | ISO 1183 |
| Material specific properties | dry / cond | Unit | Test Standard |
| Viscosity number | 164 / * | cm³/g | ISO 307, 1157, 1628 |
| Film Properties | dry / cond | Unit | Test Standard |
| Stress at yield (parallel) | 32 / * | MPa | ISO 527-3 |
| Maximum stress (parallel) | 80 / * | MPa | ISO 527-3 |
| Maximum strain (parallel) | 350 / * | % | ISO 527-3 |
| Trouser Tear resistance (parallel) | 32 / * | N/mm | ISO 6383-1 |
| Dynamic coefficient of friction | 1.2 / * | - | ISO 8295 |
| WVTR (23°C/85%r.h.) | 35 / * | g/(m²*d) | DIS 15106-1/-2 |
| Oxygen transmission rate (23°C/0%r.h.) | 26 / * | cm³/(m²*d*bar) | DIS 15105-1/-2 |
| Oxygen transmission rate (23°C/85%r.h.) | 38 / * | cm³/(m²*d*bar) | DIS 15105-1/-2 |
| Type of extrusion | cast / * | - | - |
| Thickness of specimen | 0.05 / * | mm | - |
Characteristics
Processing
Film Extrusion, Other Extrusion, Coating, Casting
Delivery form
Pellets
Additives
Lubricants
Regional Availability
Disclaimer
All information supplied by or on behalf of DSM in relation to its products, whether in the nature of data, recommendations or otherwise, is supported by research and, in good faith, believed reliable, but DSM assumes no liability and makes no warranties of any kind, express or implied, including, but not limited to, those of title, merchantability, fitness for a particular purpose or non-infringement or any warranty arising from a course of dealing, usage, or trade practice whatsoever in respect of application, processing or use made of the aforementioned information or product. The user assumes all responsibility for the use of all information provided and shall verify quality and other properties or any consequence from the use of all such information. Typical values are indicative only and are not to be construed as being binding specifications.
The CAMPUS internet database is hosted by M-Base Engineering + Software GmbH.
M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors.
Any decision about the application of materials must be double checked with the producer of this material.