View list of
  • All DSM grades
  • All PA6 grades
  • All grades beginning with A

CAMPUS® datasheet | Akulon® F130-E1


This datasheet of Akulon® F130-E1 from DSM Engineering Plastics is provided by the international plastics database CAMPUS.

CAMPUS is organized by a group of leading international resin producers, who have agreed to test their material according to uniform conditions, based on ISO standards (ISO 10350, ISO 11403), in order to offer comparable data to the market.

This datasheet includes:

  Akulon® F130-E1 | PA6 | DSM Engineering Plastics
Product Texts
Medium Viscosity, Nucleated, Lubricated, Film Extrusion

ISO 1043 PA6

Akulon® polyamide 6 and 66 resins
Thermal propertiesdry / condUnitTest Standard
Melting temperature (10°C/min) 220 / * °C ISO 11357-1/-3
Coeff. of linear therm. expansion (parallel) 90 / * E-6/K ISO 11359-1/-2
Coeff. of linear therm. expansion (normal) 90 / * E-6/K ISO 11359-1/-2
Other propertiesdry / condUnitTest Standard
Water absorption 9 / * % Sim. to ISO 62
Humidity absorption 2.8 / * % Sim. to ISO 62
Density 1130 / - kg/m³ ISO 1183
Material specific propertiesdry / condUnitTest Standard
Viscosity number 195 / * cm³/g ISO 307, 1157, 1628
Film Propertiesdry / condUnitTest Standard
Stress at yield (parallel) 34 / * MPa ISO 527-3
Maximum stress (parallel) 96 / * MPa ISO 527-3
Maximum strain (parallel) 350 / * % ISO 527-3
Trouser Tear resistance (parallel) 33 / * N/mm ISO 6383-1
Dynamic coefficient of friction 0.8 / * - ISO 8295
WVTR (23°C/85%r.h.) 35 / * g/(m²*d) DIS 15106-1/-2
Oxygen transmission rate (23°C/0%r.h.) 20 / * cm³/(m²*d*bar) DIS 15105-1/-2
Oxygen transmission rate (23°C/85%r.h.) 31 / * cm³/(m²*d*bar) DIS 15105-1/-2
Type of extrusion cast / * - -
Thickness of specimen 0.05 / * mm -
Characteristics
Processing
Film Extrusion, Other Extrusion, Casting
Delivery form
Pellets
Additives
Lubricants
Regional Availability
North America, Europe, Asia Pacific
Other text information
Film extrusion
<font face="Arial" size="2">Processing of Akulon film grades
Disclaimer
 All information supplied by or on behalf of DSM in relation to its
products, whether in the nature of data, recommendations or otherwise,
is supported by research and, in good faith, believed reliable, but DSM
assumes no liability and makes no warranties of any kind, express or
implied, including, but not limited to, those of title, merchantability,
fitness for a particular purpose or non-infringement or any warranty
arising from a course of dealing, usage, or trade practice whatsoever
in respect of application, processing or use made of the aforementioned
information or product. The user assumes all responsibility for the use
of all information provided and shall verify quality and other properties or
any consequence from the use of all such information.

Typical values are indicative only and are not to be construed as being
binding specifications.

The CAMPUS internet database is hosted by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

CAMPUS® is a Registered trademark of CWFG mbH, Frankfurt/Main, 1991