  Akulon® K240-HPG3 | PA6-I-GF15 | DSM Engineering Plastics
Product Texts
15% Glass Reinforced, Heat Stabilized, Extrusion Blow Molding

ISO 1043 PA6-I-GF15

Akulon® polyamide 6 and 66 resins
Rheological propertiesdry / condUnitTest Standard
Melt volume-flow rate (MVR) 40 / * cm³/10min ISO 1133
Temperature 275 / * °C ISO 1133
Load 21.6 / * kg ISO 1133
Molding shrinkage (parallel) 0.2 / * % ISO 294-4, 2577
Molding shrinkage (normal) 1.2 / * % ISO 294-4, 2577
Mechanical propertiesdry / condUnitTest Standard
Tensile Modulus 5600 / 3000 MPa ISO 527-1/-2
Stress at break 110 / 60 MPa ISO 527-1/-2
Strain at break 5 / 15 % ISO 527-1/-2
Charpy impact strength (+23°C) 80 / N kJ/m² ISO 179/1eU
Charpy impact strength (-30°C) 90 / 90 kJ/m² ISO 179/1eU
Charpy notched impact strength (+23°C) 20 / 30 kJ/m² ISO 179/1eA
Charpy notched impact strength (-30°C) 10 / 10 kJ/m² ISO 179/1eA
Thermal propertiesdry / condUnitTest Standard
Melting temperature (10°C/min) 220 / * °C ISO 11357-1/-3
Temp. of deflection under load (1.80 MPa) 185 / * °C ISO 75-1/-2
Temp. of deflection under load (0.45 MPa) 210 / * °C ISO 75-1/-2
Other propertiesdry / condUnitTest Standard
Water absorption 6.8 / * % Sim. to ISO 62
Humidity absorption 2 / * % Sim. to ISO 62
Density 1200 / - kg/m³ ISO 1183
Diagrams
Dynamic Shear modulus-temperature , Akulon® K240-HPG3, PA6-I-GF15, DSM
Stress-strain , Akulon® K240-HPG3, PA6-I-GF15, DSM
Secant modulus-strain , Akulon® K240-HPG3, PA6-I-GF15, DSM
Characteristics
Processing
Blow Molding
Delivery form
Pellets
Special Characteristics
Heat stabilized or stable to heat
Regional Availability
Other text information
Injection molding
Disclaimer
 All information supplied by or on behalf of DSM in relation to its
products, whether in the nature of data, recommendations or otherwise,
is supported by research and, in good faith, believed reliable, but DSM
assumes no liability and makes no warranties of any kind, express or
implied, including, but not limited to, those of title, merchantability,
fitness for a particular purpose or non-infringement or any warranty
arising from a course of dealing, usage, or trade practice whatsoever
in respect of application, processing or use made of the aforementioned
information or product. The user assumes all responsibility for the use
of all information provided and shall verify quality and other properties or
any consequence from the use of all such information.

Typical values are indicative only and are not to be construed as being
binding specifications.

The CAMPUS internet database is hosted by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

CAMPUS® is a Registered trademark of CWFG mbH, Frankfurt/Main, 1991