CAMPUS® datasheet | Arnite® T04 200


This datasheet of Arnite® T04 200 from DSM Engineering Plastics is provided by the international plastics database CAMPUS.

CAMPUS is organized by a group of leading international resin producers, who have agreed to test their material according to uniform conditions, based on ISO standards (ISO 10350, ISO 11403), in order to offer comparable data to the market.

This datasheet includes:

  Arnite® T04 200 | PBT | DSM Engineering Plastics
Product Texts
Low Viscosity, Extrusion

ISO 1043 PBT

Arnite® PBT and PET Polyesters
Thermal propertiesValueUnitTest Standard
Melting temperature (10°C/min) 225 °C ISO 11357-1/-3
Other propertiesValueUnitTest Standard
Water absorption 0.45 % Sim. to ISO 62
Humidity absorption 0.18 % Sim. to ISO 62
Density 1300 kg/m³ ISO 1183
Diagrams
Viscosity-shear rate , Arnite® T04 200, PBT, DSM
Shearstress-shear rate , Arnite® T04 200, PBT, DSM
Stress-strain , Arnite® T04 200, PBT, DSM
Secant modulus-strain , Arnite® T04 200, PBT, DSM
Characteristics
Processing
Other Extrusion
Delivery form
Pellets
Regional Availability
Other text information
Injection molding
Disclaimer
 All information supplied by or on behalf of DSM in relation to its
products, whether in the nature of data, recommendations or otherwise,
is supported by research and, in good faith, believed reliable, but DSM
assumes no liability and makes no warranties of any kind, express or
implied, including, but not limited to, those of title, merchantability,
fitness for a particular purpose or non-infringement or any warranty
arising from a course of dealing, usage, or trade practice whatsoever
in respect of application, processing or use made of the aforementioned
information or product. The user assumes all responsibility for the use
of all information provided and shall verify quality and other properties or
any consequence from the use of all such information.

Typical values are indicative only and are not to be construed as being
binding specifications.

The CAMPUS internet database is hosted by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

CAMPUS® is a Registered trademark of CWFG mbH, Frankfurt/Main, 1991