  Arnitel® PB582-H | TPC | DSM Engineering Plastics
Product Texts
58 Shore D, Blow Molding Grade, Heat Stabilized

ISO 18064 TPC-ET

Arnitel® copolyester elastomers
Rheological propertiesValueUnitTest Standard
Melt volume-flow rate (MVR) 3 cm³/10min ISO 1133
Temperature 230 °C ISO 1133
Load 10 kg ISO 1133
Mechanical propertiesValueUnitTest Standard
Tensile Modulus 300 MPa ISO 527-1/-2
Stress at 10% elongation 16.5 MPa ISO 527-1/-2
Stress at 100% elongation 26.7 MPa ISO 527-1/-2
Stress at break TPE 30 MPa ISO 527-1/-2
Charpy notched impact strength (+23°C) N kJ/m² ISO 179/1eA
Charpy notched impact strength (-30°C) 14 kJ/m² ISO 179/1eA
Tear strength 100 kN/m ISO 34-1
Shore D hardness (15s) 56 - ISO 868
Thermal propertiesValueUnitTest Standard
Melting temperature (10°C/min) 220 °C ISO 11357-1/-3
Temp. of deflection under load (0.45 MPa) 100 °C ISO 75-1/-2
Vicat softening temperature (50°C/h 50N) 105 °C ISO 306
Other propertiesValueUnitTest Standard
Density 1230 kg/m³ ISO 1183
Characteristics
Processing
Blow Molding
Delivery form
Pellets
Special Characteristics
Heat stabilized or stable to heat
Regional Availability
Disclaimer
 All information supplied by or on behalf of DSM in relation to its
products, whether in the nature of data, recommendations or otherwise,
is supported by research and, in good faith, believed reliable, but DSM
assumes no liability and makes no warranties of any kind, express or
implied, including, but not limited to, those of title, merchantability,
fitness for a particular purpose or non-infringement or any warranty
arising from a course of dealing, usage, or trade practice whatsoever
in respect of application, processing or use made of the aforementioned
information or product. The user assumes all responsibility for the use
of all information provided and shall verify quality and other properties or
any consequence from the use of all such information.

Typical values are indicative only and are not to be construed as being
binding specifications.

The CAMPUS internet database is hosted by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

CAMPUS® is a Registered trademark of CWFG mbH, Frankfurt/Main, 1991