  BERGADUR® PB40GK30 | PBT-GB30 | PolyOne Engineered Materials Europe
Product Texts
PBT, reinforced
30% glass bead
general-purpose injection molding grade
Mechanical propertiesValueUnitTest Standard
Tensile Modulus 4000 MPa ISO 527-1/-2
Stress at break 57 MPa ISO 527-1/-2
Strain at break 6 % ISO 527-1/-2
Tensile creep modulus (1h) 3600 MPa ISO 899-1
Tensile creep modulus (1000h) 2500 MPa ISO 899-1
Charpy impact strength (+23°C) 50 kJ/m² ISO 179/1eU
Charpy impact strength (-30°C) 50 kJ/m² ISO 179/1eU
Charpy notched impact strength (+23°C) 4 kJ/m² ISO 179/1eA
Charpy notched impact strength (-30°C) 3 kJ/m² ISO 179/1eA
Thermal propertiesValueUnitTest Standard
Melting temperature (10°C/min) 224 °C ISO 11357-1/-3
Temp. of deflection under load (1.80 MPa) 70 °C ISO 75-1/-2
Temp. of deflection under load (0.45 MPa) 170 °C ISO 75-1/-2
Coeff. of linear therm. expansion (parallel) 100 E-6/K ISO 11359-1/-2
Coeff. of linear therm. expansion (normal) 100 E-6/K ISO 11359-1/-2
Burning Behav. at 1.5 mm nom. thickn. HB class IEC 60695-11-10
Thickness tested 1.6 mm IEC 60695-11-10
Burning Behav. at thickness h HB class IEC 60695-11-10
Thickness tested 0.8 mm IEC 60695-11-10
Electrical propertiesValueUnitTest Standard
Relative permittivity (1MHz) 3.8 - IEC 60250
Dissipation factor (1MHz) 180 E-4 IEC 60250
Volume resistivity >1E13 Ohm*m IEC 60093
Surface resistivity >1E15 Ohm IEC 60093
Electric strength 25 kV/mm IEC 60243-1
Comparative tracking index 500 - IEC 60112
Other propertiesValueUnitTest Standard
Water absorption 0.35 % Sim. to ISO 62
Humidity absorption 0.14 % Sim. to ISO 62
Density 1530 kg/m³ ISO 1183
Test specimen productionValueUnitTest Standard
Injection Molding, melt temperature 230 °C ISO 294
Injection Molding, mold temperature 80 °C ISO 10724
Characteristics
Processing
Injection Molding
Delivery form
Pellets
Regional Availability
Other text information
Injection molding
PREPROCESSING
Max. Water Content 0,04%
Pre-Drying: 120°C 2-4 Hours
PROCESSING
Melt Temperature 240-260°C
Mould Temperature 80°C
Disclaimer

PolyOne Engineered Materials Europe

 

PolyOne

PolyOne Th.Bergmann GmbH

 

PolyOne Corporation makes no representations, guarantees or warranties of any kind with respect to the information contained in this document about its accuracy, suitability for particular applications ort he result obtained or obtainable using the information. Some of the information arises from laboratory work with small-case equipment which may not provide a reliable indication of performance or properties obtained or obtainable on larger-scale equipment. Processing conditions can cause material properties to shift from the values stated in data bases. PolyOne Corporation makes no guarantees or warranties respecting suitability of either PolyOne’s products or the information for your process or end-use application. You have the responsibility to conduct full-scale end-product performance testing to determine suitability in your application, and you assume all risks and liability arising from your use of the information and/or handling of any product. PolyOne Corporation makes no warranties, express or implied, including, but not limited to, implied warranties of merchantability and fitness for a particular purpose, either with respect to the information or products reflected by the information. These information shall not operate as permission, recommendation or inducement to practice any patented invention without permission of the patent owner.

 

Germany:

PolyOne Th.Bergmann GmbH

Adolf-Dambach-Strasse 2-4

D-76571 Gaggenau

Tel.: 07225 6802 0

Fax:07225 6802 10

e-mail

 

France:

PolyOne Engineered Materials SA, FRANCE

20, Rue Salvador Allende, BP 105

42353 La Talaudière Cedex, France

Tel.: +33 (0) 477 47 64 00

Tel.:+33 (0) 477 57 13

 

Spain:

Pol. Ind. Valle del Cinca

22300 Barbastro, Spain

Tel.: +34 (0) 974 31 03 14

Fax.: +34 (0) 974 31 43 11

e-mail

 

United Kingdom:

PolyOne Engineered Materials UL Ltd.

Newton Ayecliff

Durham DL5 6EA, UK

Tel.:+44 (0) 1325 30 08 48

Fax.:+44 (0) 1325 30 14 13

 

Turkey:

Tekno Polimer

103 Kücükcekmece

Istanbul, Turkey

Tel:+90 212 549 2256

Fax.:+90 212 549 2241

e-mail


The CAMPUS internet database is hosted by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

CAMPUS® is a Registered trademark of CWFG mbH, Frankfurt/Main, 1991