  Desmopan® DP 8798A | TPU | Bayer MaterialScience
Product Texts
  • injection molding grade
  • with special UV stabilizers
  • Easy release
  • short cycle times

Application
  • Sports shoe soles
Mechanical propertiesValueUnitTest Standard
Compression Set under constant strain (23°C) 25 % ISO 815
Compression Set under constant strain (70°C) 45 % ISO 815
Abrasion resistance 25 mm³ ISO 4649
Shore A hardness (3s) 96 - ISO 868
Shore D hardness (15s) 53 - ISO 868
Other propertiesValueUnitTest Standard
Density 1220 kg/m³ ISO 1183
Rheological calculation propertiesValueUnitTest Standard
Density of melt 1040 kg/m³ -
Thermal conductivity of melt 0.141 W/(m K) -
Spec. heat capacity melt 1700 J/(kg K) -
Eff. thermal diffusivity 8E-8 m²/s -
Ejection temperature 50 °C -
Diagrams
Viscosity-shear rate , Desmopan® DP 8798A, TPU, Bayer MatSc
Shearstress-shear rate , Desmopan® DP 8798A, TPU, Bayer MatSc
Characteristics
Regional Availability
Other text information
Injection molding

 Preprocessing

Max. Water content ≤0.05 %
Drying temperature 70-110 °C

Drying time
Dry air dryer 1-2 h

 Processing

Melt temperature 190-220 °C
Mold temperature 20-40 °C
Other extrusion

 Preprocessing

Max. Water content ≤0.05 %
Drying temperature 70-110 °C
Dry air dryer 1-2 h

 Processing

Melt temperature 180-200 °C
Profile extrusion

 Preprocessing

Max. Water content ≤0.05 %
Drying temperature 70-110 °C
Dry air dryer 1-2 h

 Processing

Melt temperature 180-200 °C
Disclaimer

Bayer MaterialScience AG

This information and our technical advice - whether verbal, in writing or by way of trials - are given in good faith but without warranty, and this also applies where proprietary rights of third parties are involved. Our advice does not release you from the obligation to check its validity and to test our products as to their suitability for the intended processes and uses. The application, use and processing of our products and the products manufactured by you on the basis of our technical advice are beyond our control and, therefore, entirely your own responsibility. Our products are sold in accordance with our General Conditions of and Delivery. The values stored in the databank should only be used as guidelines for component design. In giving these values neither guarantee, nor assurance of particular material properties can be given.

plastics.bayer.com



Bayer MaterialScience LLC - CAMPUS version 5.x

This database, the data, reports, and graphs generated by the software [as of March 2010] have been provided pursuant to an agreement containing restrictions of their use between Bayer and Wirtschaftsförderungs-Gesellschaft CWF GmbH, Frankfurt am Main, Germany. They are also protected by Copyright and cannot be copied, or distributed, transmitted, transcribed, or translated into any human or computer language, in any form or by any means without the expressed written consent of Bayer Materialscience LLC, Pittsburgh, Pa. 15205-9741.


DISCLAIMER OF ALL WARRANTIES AND LIMITATION OF LIABILITY

BAYER MATERIALSCIENCE LLC DISCLAIMS ALL WARRANTIES WITH REGARD TO THIS SOFTWARE, INCLUDING ALL IMPLIED WARRANTIES OF MERCHANTABILITY AND FITNESS FOR A PARTICULAR PURPOSE. IN NO EVENT SHALL BAYER MATERIALSCIENCE LLC BE LIABLE FOR ANY DAMAGES WHATSOEVER OF WHATEVER NATURE, WHETHER DIRECT, SPECIAL, INDIRECT, INCIDENTAL, OR CONSEQUENTIAL, ARISING FROM BREACH OF CONTRACT OR WARRANTY, NEGLIGENCE, OR ANY OTHER ACT, AND WHICH ARISE OUT OF OR IN CONNECTION WITH THE USE OR PERFORMANCE OF THIS SOFTWARE.


Bayer MaterialScience LLC - Standard Disclaimer

The manner in which you use and the purpose to which you put and utilize our products, technical assistance and information (whether verbal, written or by way of production evaluations), including any suggested formulations and recommendations are beyond our control. Therefore, it is imperative that you test our products, technical assistance and information to determine to your own satisfaction whether they are suitable for your intended uses and applications. This application-specific analysis must at least include testing to determine suitability from a technical as well as health, safety, and environmental. Such testing has not necessarily been done by us. Unless we otherwise agree in writing, all products are sold strictly pursuant to the terms of our standard conditions of sale. All information and technical assistance is given without warranty or guarantee and is subject to change without notice. It is expressly understood and agreed that you assume and hereby expressly release us from all liability, in tort, contract or otherwise, incurred in connection with the use of our products, technical assistance, and information. Any statement or recommendation not contained herein is unauthorized and shall not bind us. Nothing herein shall be construed as a recommendation to use any product in conflict with patents covering any material or its use. No license is implied or in fact granted under the claims of any patent.

www.bayerplastics.com

The CAMPUS internet database is hosted by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

CAMPUS® is a Registered trademark of CWFG mbH, Frankfurt/Main, 1991