View list of
  • All LANXESS grades
  • All PA66 grades
  • All grades beginning with D

CAMPUS® datasheet | Durethan® AC 30 DUS027


This datasheet of Durethan® AC 30 DUS027 from LANXESS Deutschland GmbH is provided by the international plastics database CAMPUS.

CAMPUS is organized by a group of leading international resin producers, who have agreed to test their material according to uniform conditions, based on ISO standards (ISO 10350, ISO 11403), in order to offer comparable data to the market.

This datasheet includes:

  Durethan® AC 30 DUS027 | PA66 | LANXESS Deutschland GmbH
Product Texts
PA 66, non-reinforced, injection moulding, heat-ageing stabilized impact modified
Rheological propertiesdry / condUnitTest Standard
Molding shrinkage (parallel) 1.3 / * % ISO 294-4, 2577
Molding shrinkage (normal) 2.0 / * % ISO 294-4, 2577
Mechanical propertiesdry / condUnitTest Standard
Tensile Modulus 2800 / 1100 MPa ISO 527-1/-2
Yield stress 70 / 40 MPa ISO 527-1/-2
Yield strain 6 / 25 % ISO 527-1/-2
Nominal strain at break 18 / >50 % ISO 527-1/-2
Charpy notched impact strength (+23°C) 10 / 25 kJ/m² ISO 179/1eA
Charpy notched impact strength (-30°C) 10 / - kJ/m² ISO 179/1eA
Thermal propertiesdry / condUnitTest Standard
Melting temperature (10°C/min) 261 / * °C ISO 11357-1/-3
Other propertiesdry / condUnitTest Standard
Density 1110 / - kg/m³ ISO 1183
Rheological calculation propertiesValueUnitTest Standard
Density of melt 935 kg/m³ -
Thermal conductivity of melt 0.217 W/(m K) -
Spec. heat capacity melt 2950 J/(kg K) -
Eff. thermal diffusivity 7.87E-8 m²/s -
Ejection temperature 185 °C -
Test specimen productionValueUnitTest Standard
Injection Molding, melt temperature 280 °C ISO 294
Injection Molding, mold temperature 80 °C ISO 10724
Diagrams
Viscosity-shear rate , Durethan® AC 30 DUS027, PA66, LANXESS
Shearstress-shear rate , Durethan® AC 30 DUS027, PA66, LANXESS
Dynamic Shear modulus-temperature , Durethan® AC 30 DUS027, PA66, LANXESS
Stress-strain , Durethan® AC 30 DUS027, PA66, LANXESS
Stress-strain , Durethan® AC 30 DUS027, PA66, LANXESS
Stress-strain (isochronous) 23°C, Durethan® AC 30 DUS027, PA66, LANXESS
Stress-strain (isochronous) 23°C, Durethan® AC 30 DUS027, PA66, LANXESS
Stress-strain (isochronous) 40°C, Durethan® AC 30 DUS027, PA66, LANXESS
Stress-strain (isochronous) 60°C, Durethan® AC 30 DUS027, PA66, LANXESS
Stress-strain (isochronous) 80°C, Durethan® AC 30 DUS027, PA66, LANXESS
Characteristics
Processing
Injection Molding
Delivery form
Pellets
Additives
Release agent
Regional Availability
Other text information
Injection molding
PREPROCESSING
Max. Water content: 0.1 %
Drying temperature: 80 °C

Drying time:
Dry air dryer 2-20 h (will depend on the initial moisture content)

PROCESSING
Melt temperature: 280 - 300 °C
Mold temperature: 80 - 100 °C
Disclaimer
This information and our  technical advice - whether verbal, in  writing
or by way of trials - are  given in good faith but without warranty, and
this  also  applies  where  proprietary  rights  of  third  parties  are
involved.  Our advice does not release you from  the obligation to check
its validity and to test our  products  as to their  suitability for the
intended processes and uses.  The  application, use  and  processing  of
our products and the products manufactured  by  you  on the basis of our
technical  advice  are  beyond our control and, therefore, entirely your
own  responsibility.  Our  products  are  sold  in  accordance  with our
General  Conditions of Sale and Delivery.
The values  stored in the databank should only be used as guidelines for
component   design.  In  giving  these  values  neither  guarantee,  nor
assurance of particular material properties can be given.

techcenter.lanxess.com

The CAMPUS internet database is hosted by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

CAMPUS® is a Registered trademark of CWFG mbH, Frankfurt/Main, 1991