CAMPUS® datasheet | Durethan® AKV 15


This datasheet of Durethan® AKV 15 from LANXESS Deutschland GmbH is provided by the international plastics database CAMPUS.

CAMPUS is organized by a group of leading international resin producers, who have agreed to test their material according to uniform conditions, based on ISO standards (ISO 10350, ISO 11403), in order to offer comparable data to the market.

This datasheet includes:

  Durethan® AKV 15 | PA66-GF15 | LANXESS Deutschland GmbH
Product Texts
PA 66, 15 % glass fibres, injection moulding
Mechanical propertiesdry / condUnitTest Standard
Tensile Modulus 6700 / 4100 MPa ISO 527-1/-2
Stress at break 125 / 90 MPa ISO 527-1/-2
Strain at break 3 / 8 % ISO 527-1/-2
Charpy impact strength (+23°C) 40 / 50 kJ/m² ISO 179/1eU
Charpy impact strength (-30°C) 40 / 40 kJ/m² ISO 179/1eU
Charpy notched impact strength (+23°C) 10 / 10 kJ/m² ISO 179/1eA
Charpy notched impact strength (-30°C) 10 / 10 kJ/m² ISO 179/1eA
Thermal propertiesdry / condUnitTest Standard
Melting temperature (10°C/min) 263 / * °C ISO 11357-1/-3
Temp. of deflection under load (1.80 MPa) 250 / * °C ISO 75-1/-2
Temp. of deflection under load (0.45 MPa) 250 / * °C ISO 75-1/-2
Coeff. of linear therm. expansion (parallel) 40 / * E-6/K ISO 11359-1/-2
Coeff. of linear therm. expansion (normal) 90 / * E-6/K ISO 11359-1/-2
Burning Behav. at 1.5 mm nom. thickn. HB / * class IEC 60695-11-10
Thickness tested 1.6 / * mm IEC 60695-11-10
Oxygen index 22 / * % ISO 4589-1/-2
Electrical propertiesdry / condUnitTest Standard
Relative permittivity (100Hz) 4 / 9 - IEC 60250
Relative permittivity (1MHz) 4 / 4 - IEC 60250
Dissipation factor (100Hz) 80 / 1300 E-4 IEC 60250
Dissipation factor (1MHz) 150 / 700 E-4 IEC 60250
Volume resistivity 1E13 / 1E10 Ohm*m IEC 60093
Surface resistivity * / 1E12 Ohm IEC 60093
Electric strength 35 / 30 kV/mm IEC 60243-1
Comparative tracking index 600 / - - IEC 60112
Other propertiesdry / condUnitTest Standard
Water absorption 7 / * % Sim. to ISO 62
Humidity absorption 2.4 / * % Sim. to ISO 62
Density 1230 / - kg/m³ ISO 1183
Material specific propertiesdry / condUnitTest Standard
Viscosity number 146 / * cm³/g ISO 307, 1157, 1628
Rheological calculation propertiesValueUnitTest Standard
Density of melt 1050 kg/m³ -
Thermal conductivity of melt 0.234 W/(m K) -
Spec. heat capacity melt 2590 J/(kg K) -
Eff. thermal diffusivity 8.65E-8 m²/s -
Ejection temperature 185 °C -
Test specimen productionValueUnitTest Standard
Injection Molding, melt temperature 290 °C ISO 294
Injection Molding, mold temperature 80 °C ISO 10724
Diagrams
Viscosity-shear rate , Durethan® AKV 15, PA66-GF15, LANXESS
Shearstress-shear rate , Durethan® AKV 15, PA66-GF15, LANXESS
Dynamic Shear modulus-temperature , Durethan® AKV 15, PA66-GF15, LANXESS
Characteristics
Processing
Injection Molding
Delivery form
Pellets
Additives
Release agent
Regional Availability
Other text information
Injection molding
PREPROCESSING
Max. Water content: 0.1 %
Drying temperature: 80 °C

Drying time:
Dry air dryer 2-20 h (will depend on the initial moisture content)

PROCESSING
Melt temperature: 280 - 300 °C
Mold temperature: 80 - 120 °C
Disclaimer
This information and our  technical advice - whether verbal, in  writing
or by way of trials - are  given in good faith but without warranty, and
this  also  applies  where  proprietary  rights  of  third  parties  are
involved.  Our advice does not release you from  the obligation to check
its validity and to test our  products  as to their  suitability for the
intended processes and uses.  The  application, use  and  processing  of
our products and the products manufactured  by  you  on the basis of our
technical  advice  are  beyond our control and, therefore, entirely your
own  responsibility.  Our  products  are  sold  in  accordance  with our
General  Conditions of Sale and Delivery.
The values  stored in the databank should only be used as guidelines for
component   design.  In  giving  these  values  neither  guarantee,  nor
assurance of particular material properties can be given.