CAMPUS® datasheet | Durethan® DP 2801


This datasheet of Durethan® DP 2801 from LANXESS Deutschland GmbH is provided by the international plastics database CAMPUS.

CAMPUS is organized by a group of leading international resin producers, who have agreed to test their material according to uniform conditions, based on ISO standards (ISO 10350, ISO 11403), in order to offer comparable data to the market.

This datasheet includes:

  Durethan® DP 2801 | PA66 FR | LANXESS Deutschland GmbH
Product Texts
PA 66, non-reinforced, injection moulding, halogen free flame retardant
Rheological propertiesdry / condUnitTest Standard
Molding shrinkage (parallel) 1.1 / * % ISO 294-4, 2577
Molding shrinkage (normal) 1.2 / * % ISO 294-4, 2577
Mechanical propertiesdry / condUnitTest Standard
Tensile Modulus 3500 / 1400 MPa ISO 527-1/-2
Yield stress 94 / 55 MPa ISO 527-1/-2
Yield strain 4.2 / 20 % ISO 527-1/-2
Nominal strain at break 10 / >50 % ISO 527-1/-2
Charpy impact strength (+23°C) 110 / N kJ/m² ISO 179/1eU
Charpy impact strength (-30°C) 120 / 185 kJ/m² ISO 179/1eU
Charpy notched impact strength (+23°C) 10 / 15 kJ/m² ISO 179/1eA
Charpy notched impact strength (-30°C) 10 / 10 kJ/m² ISO 179/1eA
Puncture - maximum force (+23°C) 3730 / 4630 N ISO 6603-2
Puncture - maximum force (-30°C) 2400 / - N ISO 6603-2
Puncture energy (+23°C) 13.1 / 27.2 J ISO 6603-2
Puncture energy (-30°C) 5.1 / 5.1 J ISO 6603-2
Thermal propertiesdry / condUnitTest Standard
Melting temperature (10°C/min) 265 / * °C ISO 11357-1/-3
Temp. of deflection under load (1.80 MPa) 75 / * °C ISO 75-1/-2
Temp. of deflection under load (0.45 MPa) 210 / * °C ISO 75-1/-2
Coeff. of linear therm. expansion (parallel) 70 / * E-6/K ISO 11359-1/-2
Coeff. of linear therm. expansion (normal) 90 / * E-6/K ISO 11359-1/-2
Burning Behav. at thickness h V-2 / * class IEC 60695-11-10
Thickness tested 0.8 / * mm IEC 60695-11-10
Oxygen index 30 / * % ISO 4589-1/-2
Electrical propertiesdry / condUnitTest Standard
Comparative tracking index 600 / - - IEC 60112
Other propertiesdry / condUnitTest Standard
Density 1140 / - kg/m³ ISO 1183
Material specific propertiesdry / condUnitTest Standard
Viscosity number 133 / * cm³/g ISO 307, 1157, 1628
Test specimen productionValueUnitTest Standard
Injection Molding, melt temperature 290 °C ISO 294
Injection Molding, mold temperature 80 °C ISO 10724
Characteristics
Processing
Injection Molding
Delivery form
Pellets
Additives
Plasticizer
Special Characteristics
Light stabilized or stable to light
Regional Availability
Other text information
Injection molding

PREPROCESSING
Max. Water content: 0.1 %
Drying temperature: 80 °C

 

Drying time:
Dry air dryer     2-20 h (will depend on the initial moisture content)

 

PROCESSING
Melt temperature:    260 - 270 °C
Mold temperature:     80 - 100 °C

Disclaimer
This information and our  technical advice - whether verbal, in  writing
or by way of trials - are  given in good faith but without warranty, and
this  also  applies  where  proprietary  rights  of  third  parties  are
involved.  Our advice does not release you from  the obligation to check
its validity and to test our  products  as to their  suitability for the
intended processes and uses.  The  application, use  and  processing  of
our products and the products manufactured  by  you  on the basis of our
technical  advice  are  beyond our control and, therefore, entirely your
own  responsibility.  Our  products  are  sold  in  accordance  with our
General  Conditions of Sale and Delivery.
The values  stored in the databank should only be used as guidelines for
component   design.  In  giving  these  values  neither  guarantee,  nor
assurance of particular material properties can be given.