Durethan® DP BKV 35 XF | PA6-GF35 | LANXESS Deutschland GmbH
Product Texts
PA 6, 35 % glass fibres, injection moulding, improved flowability, improved surface finish
| Rheological properties | dry / cond | Unit | Test Standard |
| Molding shrinkage, parallel | 0.2 / * | % | ISO 294-4, 2577 |
| Molding shrinkage, normal | 0.6 / * | % | ISO 294-4, 2577 |
| Mechanical properties | dry / cond | Unit | Test Standard |
| Tensile Modulus | 9500 / 6300 | MPa | ISO 527-1/-2 |
| Stress at break | 165 / 104 | MPa | ISO 527-1/-2 |
| Strain at break | 2.9 / 5.1 | % | ISO 527-1/-2 |
| Charpy impact strength, +23°C | 80 / 80 | kJ/m² | ISO 179/1eU |
| Thermal properties | dry / cond | Unit | Test Standard |
| Melting temperature, 10°C/min | 220 / * | °C | ISO 11357-1/-3 |
| Temp. of deflection under load, 1.80 MPa | 209 / * | °C | ISO 75-1/-2 |
| Temp. of deflection under load, 0.45 MPa | 220 / * | °C | ISO 75-1/-2 |
| Coeff. of linear therm. expansion, parallel | 20 / * | E-6/K | ISO 11359-1/-2 |
| Coeff. of linear therm. expansion, normal | 90 / * | E-6/K | ISO 11359-1/-2 |
| Other properties | dry / cond | Unit | Test Standard |
| Density | 1360 / - | kg/m³ | ISO 1183 |
Characteristics
Processing
Injection Molding
Delivery form
Pellets
Additives
Release agent
Regional Availability
Disclaimer
This information and our technical advice - whether verbal, in writing or by way of trials - are given in good faith but without warranty, and this also applies where proprietary rights of third parties are involved. Our advice does not release you from the obligation to check its validity and to test our products as to their suitability for the intended processes and uses. The application, use and processing of our products and the products manufactured by you on the basis of our technical advice are beyond our control and, therefore, entirely your own responsibility. Our products are sold in accordance with our General Conditions of Sale and Delivery. The values stored in the databank should only be used as guidelines for component design. In giving these values neither guarantee, nor assurance of particular material properties can be given. techcenter.lanxess.com
The CAMPUS internet database is hosted by M-Base Engineering + Software GmbH.
M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors.
Any decision about the application of materials must be double checked with the producer of this material.
CAMPUS® is a registered trademark of CWFG mbH, Frankfurt am Main, 2012
CAMPUS® is a registered trademark of CWFG mbH, Frankfurt am Main, 2012