This datasheet of EDISTIR® RT 461F from Polimeri Europa is provided by the international plastics database CAMPUS.
CAMPUS is organized by a group of leading international resin producers, who have agreed to test their material according to uniform conditions, based on ISO standards (ISO 10350, ISO 11403), in order to offer comparable data to the market.
You may contact the supplier for more information about this grade.
EDISTIR® RT 461F | PS-I | Polimeri Europa
Product Texts
Symbol according to ISO 1043-1: PS-I
Designation: Thermoplastics ISO 2897-PS-I,M,093-06-07-18
High impact, heat resistant polystyrene with good stiffness.
Recommended for improving the thermal performance of injection moulded
technical parts which are submitted to high temperature in service.
Edistir RT 461F is certified BSI 415/94 according to IEC 65-20-2 at 2.5 mm.
Applications:
Cabinet and back cover for TV sets, electrical appliances, ventilator housings.
| Rheological properties | Value | Unit | Test Standard |
| Melt volume-flow rate (MVR) | 4.1 | cm³/10min | ISO 1133 |
| Temperature | 200 | °C | ISO 1133 |
| Load | 5 | kg | ISO 1133 |
| Mechanical properties | Value | Unit | Test Standard |
| Tensile Modulus | 2000 | MPa | ISO 527-1/-2 |
| Yield stress | 30 | MPa | ISO 527-1/-2 |
| Yield strain | 1.6 | % | ISO 527-1/-2 |
| Nominal strain at break | >50 | % | ISO 527-1/-2 |
| Charpy impact strength (+23°C) | 120 | kJ/m² | ISO 179/1eU |
| Charpy notched impact strength (+23°C) | 8 | kJ/m² | ISO 179/1eA |
| Thermal properties | Value | Unit | Test Standard |
| Glass transition temperature (10°C/min) | 97 | °C | ISO 11357-1/-2 |
| Temp. of deflection under load (1.80 MPa) | 75 | °C | ISO 75-1/-2 |
| Vicat softening temperature (50°C/h 50N) | 95 | °C | ISO 306 |
| Coeff. of linear therm. expansion (parallel) | 90 | E-6/K | ISO 11359-1/-2 |
| Burning Behav. at 1.5 mm nom. thickn. | HB | class | IEC 60695-11-10 |
| Thickness tested | 1.5 | mm | IEC 60695-11-10 |
| UL recognition | UL | - | - |
| Burning Behav. at thickness h | HB | class | IEC 60695-11-10 |
| Thickness tested | 3.0 | mm | IEC 60695-11-10 |
| UL recognition | UL | - | - |
| Electrical properties | Value | Unit | Test Standard |
| Relative permittivity (100Hz) | 2.5 | - | IEC 60250 |
| Relative permittivity (1MHz) | 2.5 | - | IEC 60250 |
| Dissipation factor (100Hz) | 3 | E-4 | IEC 60250 |
| Dissipation factor (1MHz) | 3 | E-4 | IEC 60250 |
| Volume resistivity | >1E13 | Ohm*m | IEC 60093 |
| Surface resistivity | >1E15 | Ohm | IEC 60093 |
| Electric strength | 65 | kV/mm | IEC 60243-1 |
| Comparative tracking index | 500 | - | IEC 60112 |
| Other properties | Value | Unit | Test Standard |
| Water absorption | 0.06 | % | Sim. to ISO 62 |
| Humidity absorption | 0.04 | % | Sim. to ISO 62 |
| Density | 1040 | kg/m³ | ISO 1183 |
| Rheological calculation properties | Value | Unit | Test Standard |
| Density of melt | 950 | kg/m³ | - |
| Spec. heat capacity melt | 2050 | J/(kg K) | - |
| Test specimen production | Value | Unit | Test Standard |
| Processing conditions acc. ISO | 2900 | - | ISO ....-2 |
| Injection Molding, melt temperature | 220 | °C | ISO 294 |
| Injection Molding, mold temperature | 45 | °C | ISO 10724 |
| Injection Molding, injection velocity | 200 | mm/s | ISO 294 |
| Injection Molding, pressure at hold | 70 | MPa | ISO 294 |
Diagrams
Characteristics
Processing
Injection Molding
Delivery form
Pellets
Regional Availability
North America, Europe, Asia Pacific, South and Central America, Near East/Africa
Other text information
Injection molding
0 Injection Molding
PREPROCESSING
PREPROCESSING
Drying normally not required
PROCESSING
Typical processing temperature range:
Melt temperature 210 - 260 °C
Mold temperature 20 - 60 °C
Disclaimer
Dear CAMPUS User, The data, information and suggestions are provided for guidance purpose only. The Company accepts no responsibility for the results obtained therefrom, as neither for their utilisation in infringement of possible patents rights. All indicated data refer to natural grades. On the subject of the experimental products, the Company reserves the right to change without prewarning the characteristics, to optimise the performances. If you have any questions regarding CAMPUS, please send an e-mail to:Pe Campus For further information regarding Polimeri Europa: Polimeri Europa Homepage
The CAMPUS internet database is hosted by M-Base Engineering + Software GmbH.
M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors.
Any decision about the application of materials must be double checked with the producer of this material.
CAMPUS® is a Registered trademark of CWFG mbH, Frankfurt/Main, 1991
CAMPUS® is a Registered trademark of CWFG mbH, Frankfurt/Main, 1991