CAMPUS® datasheet | ETPV 90A01 NC010


This datasheet of ETPV 90A01 NC010 from DuPont Engineering Polymers is provided by the international plastics database CAMPUS.

CAMPUS is organized by a group of leading international resin producers, who have agreed to test their material according to uniform conditions, based on ISO standards (ISO 10350, ISO 11403), in order to offer comparable data to the market.

This datasheet includes:

  ETPV 90A01 NC010 | TPV | DuPont Engineering Polymers
Product Texts
DuPont ETPV eliminates the manufacturing boundary between rubber and plastics, by creating a new class of material called Engineering ThermoPlastic Vulcanizates (ETPV).

It is a high-performance elastomer, molecularly fused into a high-performance thermoplastic base resin.

Parts made of DuPont ETPV can withstand service temperatures up to 160°C, much higher than thermoplastic elastomers (TPEs).

Manufacturing is done on conventional plastics equipment -- up to 10 times faster than traditional rubber processing.
Rubber-like flexibility and toughness is retained down to -40°C.

Parts made of the new material are highly resistant to oil, grease and chemicals.

DuPont ETPV contains no extractables, so it is more storage stable than traditional elastomers. Like most thermoplastics, DuPont ETPV is fully recyclable.

Rheological propertiesValueUnitTest Standard
Melt volume-flow rate (MVR) 30 cm³/10min ISO 1133
Temperature 250 °C ISO 1133
Load 10 kg ISO 1133
Molding shrinkage (parallel) 1.6 % ISO 294-4, 2577
Molding shrinkage (normal) 1.3 % ISO 294-4, 2577
Mechanical propertiesValueUnitTest Standard
Tensile Modulus 70 MPa ISO 527-1/-2
Stress at 50% strain 6.5 MPa ISO 527-1/-2
Stress at 10% elongation 3.8 MPa ISO 527-1/-2
Stress at 100% elongation 7.6 MPa ISO 527-1/-2
Stress at break TPE 9 MPa ISO 527-1/-2
Strain at break >50 % ISO 527-1/-2
Strain at break TPE 180 % ISO 527-1/-2
Tensile creep modulus (1h) 36 MPa ISO 899-1
Tensile creep modulus (1000h) 26 MPa ISO 899-1
Charpy impact strength (+23°C) N kJ/m² ISO 179/1eU
Charpy notched impact strength (+23°C) N kJ/m² ISO 179/1eA
Compression Set under constant strain (100°C) 45 % ISO 815
Thermal propertiesValueUnitTest Standard
Melting temperature (10°C/min) 203 °C ISO 11357-1/-3
Glass transition temperature (10°C/min) -25 °C ISO 11357-1/-2
Burning Behav. at 1.5 mm nom. thickn. HB class IEC 60695-11-10
Thickness tested 1.5 mm IEC 60695-11-10
Electrical propertiesValueUnitTest Standard
Volume resistivity >1E13 Ohm*m IEC 60093
Electric strength 28 kV/mm IEC 60243-1
Other propertiesValueUnitTest Standard
Density 1120 kg/m³ ISO 1183
Rheological calculation propertiesValueUnitTest Standard
Density of melt 960 kg/m³ -
Ejection temperature 140 °C -
Diagrams
Viscosity-shear rate , ETPV 90A01 NC010, TPV, DuPont
Shearstress-shear rate , ETPV 90A01 NC010, TPV, DuPont
Dynamic Tensile modulus-temperature , ETPV 90A01 NC010, TPV, DuPont
Stress-strain (isochronous) 23°C, ETPV 90A01 NC010, TPV, DuPont
Creep modulus-time 23°C, ETPV 90A01 NC010, TPV, DuPont
Stress-strain (isochronous) 150°C, ETPV 90A01 NC010, TPV, DuPont
Specific volume-temperature (pvT) , ETPV 90A01 NC010, TPV, DuPont
LTHA-Stress at Break 2mm, ETPV 90A01 NC010, TPV, DuPont
LTHA-Strain at Break 2mm, ETPV 90A01 NC010, TPV, DuPont
Characteristics
Processing
Injection Molding, Film Extrusion, Profile Extrusion, Sheet Extrusion, Other Extrusion, Coating, Casting
Delivery form
Pellets
Additives
Release agent
Regional Availability
Other text information
Injection molding

PREPROCESSING


Drying Temperature = 80°C
Drying Time, Dehumidified Dryer = 2-3 h
Processing Moisture Content = <0.08 %


PROCESSING


Melt Temperature Optimum = 245°C
Melt Temperature Range = 240-250°C
Mold Temperature Optimum = 35°C


Moulding guide

Profile extrusion

PREPROCESSING


Drying Temperature = 80°C
Drying Time, Dehumidified Dryer = 2-3 h
Processing Moisture Content = <0.05 %


PROCESSING


Melt Temperature Optimum = 225°C
Melt Temperature Range = 215-230°C


Extrusion guide

Disclaimer

E.I. du Pont de Nemours and Company is pleased to provide information about its products with the CAMPUS electronic database.

The information provided is gratis and DuPont assumes no obligation or liability for any advice furnished or for any results obtained with respect to this information.

All such advice is given and accepted at the risk of the buyer. The disclosure of information herein is not an express or implied license to operate under any patent of DuPont or others.

DuPont warrants that the use or sale of any material which is described herein and is offered for sale by DuPont does not infringe any patent covering the material itself, but does not warrant against infringement by reason of the use thereof in combination with other materials or the operation of any process.

Unless otherwise noted, the property values are for natural color (NC010) resins only. Colorants or other additives may alter some or all of the properties.
The data listed herein fall within the normal range of product properties and they should not be used to establish specification limits nor used alone as the basis of design.

Material Safety Data Sheets (SDSs) can be obtained from local sales offices.

Products listed herein should not be used in medical applications involving permanent implantation in the human body or contact with internal body fluids or tissues unless the material has been provided from DuPont under a written contract that is consistent with DuPont policy regarding medical applications and expressly acknowledges the contemplated use.

For further information, please contact your DuPont representative.

You may also request a copy of DuPont policy regarding medical applications H-50103-2 and DuPont caution regarding medical applications H-50102-2.

Products listed herein may from time to time be modified or removed.
Please call your local sales office to determine current availability.


The CAMPUS internet database is hosted by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

CAMPUS® is a Registered trademark of CWFG mbH, Frankfurt/Main, 1991