This datasheet includes:

  Elastollan® C 74 D | TPU | BASF Polyurethanes GmbH
Product Texts
DESCRIPTION
Elastollan C 74 D is a polyester based TPU

SPECIAL PROPERTIES
high tensile strength, excellent tear strength,
very good damping behavior, good rebound elasticity,
very good wear performance, good flexibility at low temperature
and resistance to hydrolysis

TYPICAL APPLICATIONS
technical parts

OTHER HINTS
predrying: 2-3h at 100-120°C
(air circulating oven or dehumidified air dryer),
max. content of humidity before processing: 0,02%
annealing: 20 h at 100°C in order to get optimum properties

CHEMICAL RESISTANCE
For detailed information on the chemical resistance of our
materials refer to this list of chemical resistance
Mechanical propertiesValueUnitTest Standard
Tensile Modulus 730 MPa ISO 527-1/-2
Stress at 50% strain 30 MPa ISO 527-1/-2
Stress at 100% elongation 30 MPa ISO 527-1/-2
Stress at 300% elongation 35 MPa ISO 527-1/-2
Stress at break TPE 45 MPa ISO 527-1/-2
Strain at break >50 % ISO 527-1/-2
Strain at break TPE >300 % ISO 527-1/-2
Charpy notched impact strength (+23°C) N kJ/m² ISO 179/1eA
Charpy notched impact strength (-30°C) 4 kJ/m² ISO 179/1eA
Tensile notched impact strength (+23°C) 310 kJ/m² ISO 8256/1
Compression Set under constant strain (23°C) 40 % ISO 815
Compression Set under constant strain (70°C) 60 % ISO 815
Tear strength 240 kN/m ISO 34-1
Abrasion resistance 25 mm³ ISO 4649
Shore D hardness (15s) 71 - ISO 868
Thermal propertiesValueUnitTest Standard
Glass transition temperature (10°C/min) -8 °C ISO 11357-1/-2
Temp. of deflection under load (1.80 MPa) 50 °C ISO 75-1/-2
Temp. of deflection under load (0.45 MPa) 102 °C ISO 75-1/-2
Coeff. of linear therm. expansion (normal) 100 E-6/K ISO 11359-1/-2
Burning Behav. at thickness h HB class IEC 60695-11-10
UL recognition UL - -
Electrical propertiesValueUnitTest Standard
Relative permittivity (1MHz) 4 - IEC 60250
Dissipation factor (100Hz) 310 E-4 IEC 60250
Dissipation factor (1MHz) 350 E-4 IEC 60250
Volume resistivity >1E13 Ohm*m IEC 60093
Surface resistivity >1E15 Ohm IEC 60093
Electric strength 31 kV/mm IEC 60243-1
Comparative tracking index 600 - IEC 60112
Other propertiesValueUnitTest Standard
Water absorption 1 % Sim. to ISO 62
Density 1250 kg/m³ ISO 1183
Test specimen productionValueUnitTest Standard
Injection Molding, melt temperature 235 °C ISO 294
Injection Molding, mold temperature 60 °C ISO 10724
Diagrams
Dynamic Shear modulus-temperature , Elastollan® C 74 D, TPU, BASF PU
Stress-strain , Elastollan® C 74 D, TPU, BASF PU
Stress-Strain (TPE) , Elastollan® C 74 D, TPU, BASF PU
Characteristics
Processing
Injection Molding
Delivery form
Pellets
Regional Availability
Other text information
Injection molding
Barrel temperature : 220 - 235 °C
Melt temperature : 235 °C
Mold temperature: 25 - 60 °C
Disclaimer
The data contained in this publication are based on
our current knowledge and experience. In view of
the many factors that may affect processing and
application of our product, these data do not relieve
processors from carrying out their own investigations
and tests.  Any descriptions, drawings, photographs,
data, proportions, weights etc. given herein may
change without prior information and do not constitute
the agreed contractual quality of the product. It is
the responsibility of the recipient  of our products
to ensure that any proprietary rights and existing
laws and legislation are observed. NO WARRANTIES
OF ANY KIND, EITHER EXPRESS OR IMPLIED,
INCLUDING WARRANTIES OFMERCHANTABILITY OR
FITNESS FOR A PARTICULAR PURPOSE, ARE MADE
REGARDING PRODUCTS DESCRIBED OR DESIGNS,
DATA OR INFORMATION SET FORTH, OR THAT THE
PRODUCTS, DESIGNS, DATA OR INFORMATION MAY
BE USED WITHOUT INFRINGING THEINTELLECTUAL
PROPERTY RIGHTS OF OTHERS.

In order to check the availability of products please
contact us or our sales agency.


For more information about our products contact your
local BASF representative or

    BASF Polyurethanes GmbH
    European Business Management
    Thermoplastische Polyurethane
    Elastogranstraße 60
    D-49448 Lemförde
    Deutschland
    Telefon ++49 5443 122500
    Telefax ++49 5443 122555
    e-mail: pu-elastomere@basf.com
    www.pu.basf.de 
CAMPUS® is a registered trademark of CWFG (Chemie Wirtschaftsfoerderungsgesellschaft GmbH, Frankfurt) 

The CAMPUS internet database is hosted by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

CAMPUS® is a Registered trademark of CWFG mbH, Frankfurt/Main, 1991