CAMPUS® Datasheet | Grilamid 1SBVX-50H LDS black


This datasheet of Grilamid 1SBVX-50H LDS black from EMS-GRIVORY - a unit of EMS-CHEMIE AG is provided by the international plastics database CAMPUS.

You may contact the supplier for more information about this grade.

This datasheet includes:

Grilamid 1SBVX-50H LDS black | PA1010-GF50 | EMS-GRIVORY | a unit of EMS-CHEMIE AG
Product Texts
Product-nomenclature according to ISO 1874:
PA1010 + X, MH, 16-140, GF 50

 

Bio based Polyamide

Product Attributes

  Improved flowability and demoulding, Improved impact resistance

Markets

  Automotive
  Automotive electr. and electronics, lighting, Powertrain and Chassis
  Electricals & Electronics
  Mobile phones and other portable devices
  Industry & Consumer goods
  Medical devices
Rheological propertiesdry / condUnitTest Standard
Molding shrinkage, parallel 0.1 / * % ISO 294-4, 2577
Molding shrinkage, normal 0.4 / * % ISO 294-4, 2577
Mechanical propertiesdry / condUnitTest Standard
Tensile Modulus 15000 / 12000 MPa ISO 527-1/-2
Stress at break 145 / 120 MPa ISO 527-1/-2
Strain at break 1.9 / 2 % ISO 527-1/-2
Charpy impact strength, +23°C 50 / 50 kJ/m² ISO 179/1eU
Charpy impact strength, -30°C 50 / 45 kJ/m² ISO 179/1eU
Charpy notched impact strength, +23°C 10 / 10 kJ/m² ISO 179/1eA
Charpy notched impact strength, -30°C 7 / 6 kJ/m² ISO 179/1eA
Thermal propertiesdry / condUnitTest Standard
Melting temperature, 10°C/min 200 / * °C ISO 11357-1/-3
Temp. of deflection under load, 1.80 MPa 175 / * °C ISO 75-1/-2
Temp. of deflection under load, 8.00 MPa 125 / * °C ISO 75-1/-2
Coeff. of linear therm. expansion, parallel 10 / * E-6/K ISO 11359-1/-2
Coeff. of linear therm. expansion, normal 80 / * E-6/K ISO 11359-1/-2
Burning Behav. at thickness h HB / * class IEC 60695-11-10
Thickness tested 0.8 / * mm IEC 60695-11-10
Electrical propertiesdry / condUnitTest Standard
Volume resistivity 1E9 / 1E9 Ohm*m IEC 60093
Surface resistivity * / 1E10 Ohm IEC 60093
Electric strength 39 / 37 kV/mm IEC 60243-1
Comparative tracking index - / 600 - IEC 60112
Other propertiesdry / condUnitTest Standard
Water absorption 1.7 / * % Sim. to ISO 62
Humidity absorption 0.9 / * % Sim. to ISO 62
Density 1580 / - kg/m³ ISO 1183
Characteristics
Processing
Injection Molding
Delivery form
Pellets
Special Characteristics
Platable, Light stabilized or stable to light
Regional Availability
EMS-CHEMIE AG
Business Unit EMS-GRIVORY

Homepage : EMS-GRIVORY
eMail    : welcome@emsgrivory.com


The values are intended to serve as an aid in preselecting materials and for
an overview of the EMS-GRIVORY product  range. The information contained
in this publication is based on our present knowledge and experience.
The given figures and data are guidance values and do not represent binding
material specifications. No warranties of any kind, either express or implied,
including warranties of merchantability or fitness for a particular purpose, are
given regarding products, design, data and information. The customer is not
released from his obligation to investigate the products fitness and the suitability
for the intended application, compliance with legal requirements and intellectual
property rights. We reserve the right to change the information at any time and
without prior notice. The information in this publication is not to be considered
a contractual obligation and any liability whatsoever is expressly declined.
For further questions about our products please contact our experts.

The CAMPUS internet database is hosted by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.