offers extended functionality!CAMPUS® datasheet | Grilamid LVX-65H SST nat
This datasheet of Grilamid LVX-65H SST nat from EMS-GRIVORY | a unit of EMS-CHEMIE AG is provided by the international plastics database CAMPUS.
CAMPUS is organized by a group of leading international resin producers, who have agreed to test their material according to uniform conditions, based on ISO standards (ISO 10350, ISO 11403), in order to offer comparable data to the market.
You may contact the supplier for more information about this grade.
Grilamid LVX-65H SST nat | PA12-GF65 | EMS-GRIVORY | a unit of EMS-CHEMIE AG
Product Texts
Product designation according to ISO 1874: PA12, MHR, 18-190, GF65
Product Attributes
| Improved flowability and demoulding, Improved impact resistance, Improved heat resistance, Improved UV resistance (outdoor use) |
Markets
| Automotive | |
| Compressed air systems, Hydraulic systems, Automotive electr. and electronics, lighting, Powertrain and Chassis | |
| Electricals & Electronics | |
| Electrical appliances, Electrical equipment, Connectors, Mobile phones and other portable devices | |
| Industry & Consumer goods | |
| Housewares, Hydraulics & Pneumatics, Mechanical Engineering, Medical devices, Power transmission, Sanitary, water and gas supply, Sports & Leisure, Tools & Accessories |
| Rheological properties | dry / cond | Unit | Test Standard |
| Molding shrinkage (parallel) | 0.1 / * | % | ISO 294-4, 2577 |
| Molding shrinkage (normal) | 0.3 / * | % | ISO 294-4, 2577 |
| Mechanical properties | dry / cond | Unit | Test Standard |
| Tensile Modulus | 19000 / 17000 | MPa | ISO 527-1/-2 |
| Stress at break | 210 / 185 | MPa | ISO 527-1/-2 |
| Strain at break | 2.5 / 2.5 | % | ISO 527-1/-2 |
| Charpy impact strength (+23°C) | 90 / 90 | kJ/m² | ISO 179/1eU |
| Charpy impact strength (-30°C) | 85 / 85 | kJ/m² | ISO 179/1eU |
| Charpy notched impact strength (+23°C) | 25 / 25 | kJ/m² | ISO 179/1eA |
| Charpy notched impact strength (-30°C) | 20 / 20 | kJ/m² | ISO 179/1eA |
| Thermal properties | dry / cond | Unit | Test Standard |
| Melting temperature (10°C/min) | 178 / * | °C | ISO 11357-1/-3 |
| Temp. of deflection under load (1.80 MPa) | 175 / * | °C | ISO 75-1/-2 |
| Temp. of deflection under load (8.00 MPa) | 160 / * | °C | ISO 75-1/-2 |
| Burning Behav. at thickness h | HB / * | class | IEC 60695-11-10 |
| Thickness tested | 0.8 / * | mm | IEC 60695-11-10 |
| Electrical properties | dry / cond | Unit | Test Standard |
| Volume resistivity | - / 1E10 | Ohm*m | IEC 60093 |
| Surface resistivity | * / 1E11 | Ohm | IEC 60093 |
| Electric strength | 43 / 43 | kV/mm | IEC 60243-1 |
| Comparative tracking index | - / 600 | - | IEC 60112 |
| Other properties | dry / cond | Unit | Test Standard |
| Water absorption | 0.8 / * | % | Sim. to ISO 62 |
| Humidity absorption | 0.4 / * | % | Sim. to ISO 62 |
| Density | 1700 / - | kg/m³ | ISO 1183 |
Characteristics
Processing
Injection Molding
Delivery form
Pellets
Special Characteristics
U.V. stabilized or stable to weather, Heat stabilized or stable to heat
Regional Availability
Disclaimer
EMS-CHEMIE AG Business Unit EMS-GRIVORY Homepage : EMS-GRIVORY eMail : welcome@emsgrivory.com In the line with the aims of CAMPUS, the values are intended to serve as an aid in preselecting materials and for an overview of the EMS-GRIVORY product range. They correspond to our current knowledge, a legal guarantee concerning the application and the manufacture can however not be assumed. This data does not cancel the processor's own testing and inspection obligations.
The CAMPUS internet database is hosted by M-Base Engineering + Software GmbH.
M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors.
Any decision about the application of materials must be double checked with the producer of this material.
CAMPUS® is a Registered trademark of CWFG mbH, Frankfurt/Main, 1991
CAMPUS® is a Registered trademark of CWFG mbH, Frankfurt/Main, 1991