CAMPUS® datasheet | Grilon F 47 NL nat 6028


This datasheet of Grilon F 47 NL nat 6028 from EMS-GRIVORY | a unit of EMS-CHEMIE AG is provided by the international plastics database CAMPUS.

CAMPUS is organized by a group of leading international resin producers, who have agreed to test their material according to uniform conditions, based on ISO standards (ISO 10350, ISO 11403), in order to offer comparable data to the market.

You may contact the supplier for more information about this grade.

This datasheet includes:

  Grilon F 47 NL nat 6028 | PA6 | EMS-GRIVORY | a unit of EMS-CHEMIE AG
Product Texts
Product designation according to ISO 1874: PA6, FS, 32-030/N

 

Product Attributes

  High viscosity, Barrier Properties, Nucleated

Markets

  Industry & Consumer goods
  Mechanical Engineering
  Packaging
  Blow moulded containers, Non oriented film, Oriented film, Tubes

Approvals

  Food Contact
  EU Requirements, FDA
Rheological propertiesdry / condUnitTest Standard
Melt volume-flow rate (MVR) 15 / * cm³/10min ISO 1133
Temperature 275 / * °C ISO 1133
Load 5 / * kg ISO 1133
Mechanical propertiesdry / condUnitTest Standard
Tensile Modulus 3000 / 750 MPa ISO 527-1/-2
Thermal propertiesdry / condUnitTest Standard
Melting temperature (10°C/min) 222 / * °C ISO 11357-1/-3
Other propertiesdry / condUnitTest Standard
Water absorption 9 / * % Sim. to ISO 62
Humidity absorption 3 / * % Sim. to ISO 62
Density 1140 / - kg/m³ ISO 1183
Film Propertiesdry / condUnitTest Standard
Stress at yield (parallel) 35 / * MPa ISO 527-3
Stress at yield (normal) 30 / * MPa ISO 527-3
Strain at yield (parallel) 15 / * % ISO 527-3
Strain at yield (normal) 15 / * % ISO 527-3
Maximum strain (parallel) 700 / * % ISO 527-3
Maximum strain (normal) 700 / * % ISO 527-3
Elmendorf Tear resistance (parallel) 10 / * N ISO 6383-2
Elmendorf Tear resistance (normal) 10 / * N ISO 6383-2
Trouser Tear resistance (parallel) 30 / * N/mm ISO 6383-1
Trouser Tear resistance (normal) 30 / * N/mm ISO 6383-1
Dynamic coefficient of friction 0.25 / * - ISO 8295
Gloss, 60° 100 / * - ISO 2813
WVTR (23°C/85%r.h.) 15 / * g/(m²*d) DIS 15106-1/-2
Oxygen transmission rate (23°C/0%r.h.) 25 / * cm³/(m²*d*bar) DIS 15105-1/-2
Oxygen transmission rate (23°C/85%r.h.) 50 / * cm³/(m²*d*bar) DIS 15105-1/-2
Carbon Dioxide transm. rate (23°C/0%r.h.) 80 / * cm³/(m²*d*bar) DIS 15105-1/-2
Carbon Dioxide transm. rate (23°C/85%r.h.) 250 / * cm³/(m²*d*bar) DIS 15105-1/-2
Diagrams
Viscosity-shear rate , Grilon F 47 NL nat 6028, PA6, EMS-GRIVORY
Shearstress-shear rate , Grilon F 47 NL nat 6028, PA6, EMS-GRIVORY
Stress-Strain (Film Grades) , Grilon F 47 NL nat 6028, PA6, EMS-GRIVORY
Characteristics
Processing
Film Extrusion, Other Extrusion, Blow Molding
Delivery form
Pellets
Regional Availability
Chemical Media Resistance
Acids
Acetic Acid (5% by mass) (23°C)
Citric Acid solution (10% by mass) (23°C)
Lactic Acid (10% by mass) (23°C)
Hydrochloric Acid (36% by mass) (23°C)
Nitric Acid (40% by mass) (23°C)
Sulfuric Acid (38% by mass) (23°C)
Sulfuric Acid (5% by mass) (23°C)
Chromic Acid solution (40% by mass) (23°C)
Bases
Sodium Hydroxide solution (35% by mass) (23°C)
Sodium Hydroxide solution (1% by mass) (23°C)
Ammonium Hydroxide solution (10% by mass) (23°C)
Alcohols
Isopropyl alcohol (23°C)
Methanol (23°C)
Ethanol (23°C)
Hydrocarbons
n-Hexane (23°C)
Toluene (23°C)
iso-Octane (23°C)
Ketones
Acetone (23°C)
Ethers
Diethyl ether (23°C)
Mineral oils
SAE 10W40 multigrade motor oil (23°C)
SAE 10W40 multigrade motor oil (130°C)
SAE 80/90 hypoid-gear oil (130°C)
Insulating Oil (23°C)
Standard Fuels
ISO 1817 Liquid 1 (60°C)
ISO 1817 Liquid 2 (60°C)
ISO 1817 Liquid 3 (60°C)
ISO 1817 Liquid 4 (60°C)
Standard fuel without alcohol (pref. ISO 1817 Liquid C) (23°C)
Standard fuel with alcohol (pref. ISO 1817 Liquid 4) (23°C)
Diesel fuel (pref. ISO 1817 Liquid F) (23°C)
Diesel fuel (pref. ISO 1817 Liquid F) (90°C)
Diesel fuel (pref. ISO 1817 Liquid F) (>90°C)
Salt solutions
Sodium Chloride solution (10% by mass) (23°C)
Sodium Hypochlorite solution (10% by mass) (23°C)
Sodium Carbonate solution (20% by mass) (23°C)
Sodium Carbonate solution (2% by mass) (23°C)
Zinc Chloride solution (50% by mass) (23°C)
Other
Ethyl Acetate (23°C)
Hydrogen peroxide (23°C)
DOT No. 4 Brake fluid (130°C)
Ethylene Glycol (50% by mass) in water (108°C)
1% nonylphenoxy-polyethyleneoxy ethanol in water (23°C)
50% Oleic acid + 50% Olive Oil (23°C)
Water (23°C)
Deionized water (90°C)
Phenol solution (5% by mass) (23°C)
Disclaimer
EMS-CHEMIE AG
Business Unit EMS-GRIVORY

Homepage : EMS-GRIVORY
eMail    : welcome@emsgrivory.com


In the line with the aims of CAMPUS, the values are intended to serve as
an aid in preselecting materials and  for an overview of the EMS-GRIVORY
product  range.  They  correspond  to our  current  knowledge,  a  legal
guarantee concerning the application and the manufacture can however not
be assumed.  This data does not  cancel the processor's  own testing and
inspection obligations.