View list of

CAMPUS® datasheet | Grivory GV-5 FWA black 9225


This datasheet of Grivory GV-5 FWA black 9225 from EMS-GRIVORY | a unit of EMS-CHEMIE AG is provided by the international plastics database CAMPUS.

CAMPUS is organized by a group of leading international resin producers, who have agreed to test their material according to uniform conditions, based on ISO standards (ISO 10350, ISO 11403), in order to offer comparable data to the market.

You may contact the supplier for more information about this grade.

This datasheet includes:

  Grivory GV-5 FWA black 9225 | PA*-GF50 | EMS-GRIVORY | a unit of EMS-CHEMIE AG
Product Texts
Product designation according to ISO 1874: PA66+PA6I/X, MH, 14-190, GF50

 

Partially aromatic Polyamide

Markets

  Industry & Consumer goods
  Housewares, Hydraulics & Pneumatics, Mechanical Engineering, Power transmission,
Sanitary, water and gas supply

Approvals

  Food Contact
  EU Requirements, FDA
  Water contact
  NSF 61, KTW, WRAS, ACS, DVGW W270
Rheological propertiesdry / condUnitTest Standard
Molding shrinkage (parallel) 0.1 / * % ISO 294-4, 2577
Molding shrinkage (normal) 0.4 / * % ISO 294-4, 2577
Mechanical propertiesdry / condUnitTest Standard
Tensile Modulus 18000 / 17000 MPa ISO 527-1/-2
Stress at break 250 / 220 MPa ISO 527-1/-2
Strain at break 2.5 / 2.5 % ISO 527-1/-2
Charpy impact strength (+23°C) 90 / 90 kJ/m² ISO 179/1eU
Charpy impact strength (-30°C) 80 / 80 kJ/m² ISO 179/1eU
Charpy notched impact strength (+23°C) 15 / 15 kJ/m² ISO 179/1eA
Charpy notched impact strength (-30°C) 13 / 13 kJ/m² ISO 179/1eA
Thermal propertiesdry / condUnitTest Standard
Melting temperature (10°C/min) 260 / * °C ISO 11357-1/-3
Temp. of deflection under load (1.80 MPa) 235 / * °C ISO 75-1/-2
Temp. of deflection under load (8.00 MPa) 165 / * °C ISO 75-1/-2
Burning Behav. at thickness h HB / * class IEC 60695-11-10
Thickness tested 0.8 / * mm IEC 60695-11-10
Electrical propertiesdry / condUnitTest Standard
Volume resistivity 1E12 / 1E12 Ohm*m IEC 60093
Surface resistivity * / 1E13 Ohm IEC 60093
Electric strength 33 / 33 kV/mm IEC 60243-1
Comparative tracking index - / 600 - IEC 60112
Other propertiesdry / condUnitTest Standard
Water absorption 4 / * % Sim. to ISO 62
Humidity absorption 1.4 / * % Sim. to ISO 62
Density 1560 / - kg/m³ ISO 1183
Diagrams
Viscosity-shear rate , Grivory GV-5 FWA black 9225, PA*-GF50, EMS-GRIVORY
Shearstress-shear rate , Grivory GV-5 FWA black 9225, PA*-GF50, EMS-GRIVORY
Dynamic Shear modulus-temperature , Grivory GV-5 FWA black 9225, PA*-GF50, EMS-GRIVORY
Dynamic Shear modulus-temperature , Grivory GV-5 FWA black 9225, PA*-GF50, EMS-GRIVORY
Stress-strain , Grivory GV-5 FWA black 9225, PA*-GF50, EMS-GRIVORY
Stress-strain , Grivory GV-5 FWA black 9225, PA*-GF50, EMS-GRIVORY
Secant modulus-strain , Grivory GV-5 FWA black 9225, PA*-GF50, EMS-GRIVORY
Secant modulus-strain , Grivory GV-5 FWA black 9225, PA*-GF50, EMS-GRIVORY
Stress-strain (isochronous) 23°C, Grivory GV-5 FWA black 9225, PA*-GF50, EMS-GRIVORY
Creep modulus-time 23°C, Grivory GV-5 FWA black 9225, PA*-GF50, EMS-GRIVORY
Stress-strain (isochronous) 60°C, Grivory GV-5 FWA black 9225, PA*-GF50, EMS-GRIVORY
Creep modulus-time 60°C, Grivory GV-5 FWA black 9225, PA*-GF50, EMS-GRIVORY
Stress-strain (isochronous) 80°C, Grivory GV-5 FWA black 9225, PA*-GF50, EMS-GRIVORY
Creep modulus-time 80°C, Grivory GV-5 FWA black 9225, PA*-GF50, EMS-GRIVORY
Specific volume-temperature (pvT) , Grivory GV-5 FWA black 9225, PA*-GF50, EMS-GRIVORY
Tensile modulus-temperature , Grivory GV-5 FWA black 9225, PA*-GF50, EMS-GRIVORY
Characteristics
Processing
Injection Molding
Delivery form
Pellets
Regional Availability
Disclaimer
EMS-CHEMIE AG
Business Unit EMS-GRIVORY

Homepage : EMS-GRIVORY
eMail    : welcome@emsgrivory.com


In the line with the aims of CAMPUS, the values are intended to serve as
an aid in preselecting materials and  for an overview of the EMS-GRIVORY
product  range.  They  correspond  to our  current  knowledge,  a  legal
guarantee concerning the application and the manufacture can however not
be assumed.  This data does not  cancel the processor's  own testing and
inspection obligations.

The CAMPUS internet database is hosted by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

CAMPUS® is a Registered trademark of CWFG mbH, Frankfurt/Main, 1991