This datasheet of HERAFLEX® E 7722 from RadiciPlastics is provided by the international plastics database CAMPUS.
CAMPUS is organized by a group of leading international resin producers, who have agreed to test their material according to uniform conditions, based on ISO standards (ISO 10350, ISO 11403), in order to offer comparable data to the market.
You may contact the supplier for more information about this grade.
HERAFLEX® E 7722 | TPC | RadiciPlastics
Product Texts
DESIGNATION:
Thermoplastics Elastomer ISO 1043-1 TPC-ET
BRIEF DESCRIPTION:
Thermoplastics Elastomer injection moulding grade
High Modulus, Nominal Shore D/15s 69
Thermoplastics Elastomer ISO 1043-1 TPC-ET
BRIEF DESCRIPTION:
Thermoplastics Elastomer injection moulding grade
High Modulus, Nominal Shore D/15s 69
| Mechanical properties | Value | Unit | Test Standard |
| Charpy impact strength (+23°C) | N | kJ/m² | ISO 179/1eU |
| Charpy notched impact strength (+23°C) | 30 | kJ/m² | ISO 179/1eA |
| Abrasion resistance | 39 | mm³ | ISO 4649 |
| Shore D hardness (15s) | 69 | - | ISO 868 |
| Thermal properties | Value | Unit | Test Standard |
| Melting temperature (10°C/min) | 220 | °C | ISO 11357-1/-3 |
| Vicat softening temperature (50°C/h 50N) | 211 | °C | ISO 306 |
| Burning Behav. at 1.5 mm nom. thickn. | HB | class | IEC 60695-11-10 |
| Thickness tested | 1.6 | mm | IEC 60695-11-10 |
| Electrical properties | Value | Unit | Test Standard |
| Comparative tracking index | 600 | - | IEC 60112 |
| Other properties | Value | Unit | Test Standard |
| Density | 1250 | kg/m³ | ISO 1183 |
Characteristics
Processing
Injection Molding, Other Extrusion
Delivery form
Pellets
Regional Availability
Disclaimer
This database provides the technical properties of thermoplastics produced and marketed by RADICI NOVACIPS and his subsidiaries companies: RADILON® A Polyamide 66 RADILON® S Polyamide 6 RADILON® CA Copolyamide 66/6 RADILON® CS Copolyamide 6 semiaromatic RADITER® B Poly(butylene terephthalate) RADIFLAM® A Polyamide 66, self-extinguishing RADIFLAM® S Polyamide 6, self-extinguishing RADIFLAM® B Polybutylene terephthalate, self-extinguishing HERAFLEX® A Stirenic Thermoplastic Elastomer SEBS HERAFLEX® E Ether-Ester Thermoplastic Elastomer HERAFLEX® B Stirenic Thermoplastic Elastomer SBS HERAFLEX® P Modified Polypropylene RADILENE® R Polyethylene and Polypropylene The data and graphs contained in this database were carried out by our Research Centers and shall in no event be held to constitute or imply any warranty, undertaking, express or implied commitment from our part.
The CAMPUS internet database is hosted by M-Base Engineering + Software GmbH.
M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors.
Any decision about the application of materials must be double checked with the producer of this material.