  HERAFLEX® HA 60-22-60 | TPS | RadiciPlastics
Product Texts
DESIGNATION:
Thermoplastics ISO 1043-1 TPS

BRIEF DESCRIPTION:
Shore hardness: 60A
Good adhesion on PA6
Application examples: Soft touch grip for powertools
Mechanical propertiesValueUnitTest Standard
Stress at 100% elongation 1.9 MPa ISO 527-1/-2
Stress at 300% elongation 2.7 MPa ISO 527-1/-2
Stress at break TPE 5.5 MPa ISO 527-1/-2
Strain at break TPE >300 % ISO 527-1/-2
Shore A hardness, 3s 60 - ISO 868
Other propertiesValueUnitTest Standard
Density 980 kg/m³ ISO 1183
Test specimen productionValueUnitTest Standard
Injection Molding, melt temperature 230 °C ISO 294
Injection Molding, mold temperature 40 °C ISO 10724
Characteristics
Processing
Injection Molding, Other Extrusion
Delivery form
Pellets
Regional Availability
Disclaimer
This database provides the technical properties
of thermoplastics produced and marketed by
RADICI NOVACIPS
and his subsidiaries companies:

RADILON® A          Polyamide 66
RADILON® S          Polyamide 6
RADILON® CA       Copolyamide 66/6
RADILON® CS       Copolyamide 6 semiaromatic
RADITER® B          Poly(butylene terephthalate)
RADIFLAM® A         Polyamide 66,  self-extinguishing
RADIFLAM® S         Polyamide 6,   self-extinguishing
RADIFLAM® B         Polybutylene terephthalate, self-extinguishing
HERAFLEX® A        Stirenic Thermoplastic Elastomer SEBS
HERAFLEX® E        Ether-Ester Thermoplastic Elastomer
HERAFLEX® B        Stirenic Thermoplastic Elastomer SBS
HERAFLEX® P        Modified Polypropylene
RADILENE® R        Polyethylene and Polypropylene

The data and graphs contained in this database were carried out
by our Research Centers and shall in no event be held to
constitute or imply any warranty, undertaking, express or
implied commitment from our part.

The CAMPUS internet database is hosted by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

CAMPUS® is a registered trademark of CWFG mbH, Frankfurt am Main, 2012