View list of
  • All Ticona grades
  • All POM grades
  • All grades beginning with H

CAMPUS® datasheet | HOSTAFORM C 27021 GV330


This datasheet of HOSTAFORM C 27021 GV330 from Ticona is provided by the international plastics database CAMPUS.

CAMPUS is organized by a group of leading international resin producers, who have agreed to test their material according to uniform conditions, based on ISO standards (ISO 10350, ISO 11403), in order to offer comparable data to the market.

You may contact the supplier for more information about this grade.

This datasheet includes:

  HOSTAFORM C 27021 GV3/30 | POM-GB30 | Ticona
Product Texts
Chemical abbreviation according to ISO 1043-1: POM
Molding compound ISO 9988- POM-K, M-GNR, 05-002, GB30

POM copolymer

With 30 % glass spheres reinforced, very easy flowing injection
molding type; low-warpage; high resistance to thermal and oxidative
degradation.

Burning rate ISO 3795 and FMVSS 302 < 100 mm/min for a thickness
more than 1 mm.

Ranges of applications: low-warpage and dimensionally stable molded
parts with higher rigidity and hardness.

FMVSS = Federal Motor Vehicle Safety Standard (USA)
Rheological propertiesValueUnitTest Standard
Melt volume-flow rate (MVR) 16 cm³/10min ISO 1133
Temperature 190 °C ISO 1133
Load 2.16 kg ISO 1133
Mechanical propertiesValueUnitTest Standard
Tensile Modulus 3800 MPa ISO 527-1/-2
Yield stress 38 MPa ISO 527-1/-2
Yield strain 6 % ISO 527-1/-2
Nominal strain at break 12 % ISO 527-1/-2
Tensile creep modulus (1h) 3300 MPa ISO 899-1
Tensile creep modulus (1000h) 2100 MPa ISO 899-1
Charpy impact strength (+23°C) 30 kJ/m² ISO 179/1eU
Charpy impact strength (-30°C) 30 kJ/m² ISO 179/1eU
Charpy notched impact strength (+23°C) 2.5 kJ/m² ISO 179/1eA
Charpy notched impact strength (-30°C) 3 kJ/m² ISO 179/1eA
Thermal propertiesValueUnitTest Standard
Melting temperature (10°C/min) 166 °C ISO 11357-1/-3
Temp. of deflection under load (1.80 MPa) 112 °C ISO 75-1/-2
Vicat softening temperature (50°C/h 50N) 151 °C ISO 306
Coeff. of linear therm. expansion (parallel) 80 E-6/K ISO 11359-1/-2
Electrical propertiesValueUnitTest Standard
Relative permittivity (100Hz) 5 - IEC 60250
Relative permittivity (1MHz) 4.5 - IEC 60250
Dissipation factor (100Hz) 300 E-4 IEC 60250
Dissipation factor (1MHz) 80 E-4 IEC 60250
Volume resistivity 1E12 Ohm*m IEC 60093
Surface resistivity 1E14 Ohm IEC 60093
Electric strength 40 kV/mm IEC 60243-1
Comparative tracking index 600 - IEC 60112
Other propertiesValueUnitTest Standard
Water absorption 0.9 % Sim. to ISO 62
Humidity absorption 0.12 % Sim. to ISO 62
Density 1590 kg/m³ ISO 1183
Test specimen productionValueUnitTest Standard
Processing conditions acc. ISO 9990 - ISO ....-2
Injection Molding, melt temperature 205 °C ISO 294
Injection Molding, mold temperature 90 °C ISO 10724
Injection Molding, injection velocity 200 mm/s ISO 294
Injection Molding, pressure at hold 90 MPa ISO 294
Diagrams
Viscosity-shear rate , HOSTAFORM C 27021 GV3/30, POM-GB30, Ticona
Shearstress-shear rate , HOSTAFORM C 27021 GV3/30, POM-GB30, Ticona
Characteristics
Processing
Injection Molding
Delivery form
Pellets
Additives
Release agent
Regional Availability
Other text information
Injection molding
PREPROCESSING

General drying is not necessary due to low moisture absorption of
the resin.

In case of bad storage conditions (water contact or condensed water)
the use of a recirculating air dryer (100 to 120 °C / max. 40 mm
layer / 3 to 6 hours) is recommended.

Max. Water content 0,2 %



PROCESSING

Standard injection moulding machines with three phase (15 to 25 D)
plasticating screws will fit.

Melt tempera ture 190-230 °C
Mould temperature 80-120 °C

POSTPROCESSING

Conditioning e.g. moisturizing is not necessary.
Disclaimer
NOTICE TO USERS: Values shown are based on testing
of laboratory test specimens and represent data that fall
within the standard range of properties for natural material.
These values alone do not represent a sufficient basis for
any part design and are not intended for use in
establishing maximum, minimum, or ranges of values for
specification purposes. Colorants or other additives may
cause significant variations in data values.

Properties of molded parts can be influenced by a wide
variety of factors including, but not limited to, material
selection, additives, part design, processing conditions and
environmental exposure. Any determination of the
suitability of a particular material and part design for any
use contemplated by the users and the manner of such
use is the sole responsibility of the users, who must assure
themselves that the material as subsequently processed
meets the needs of their particular product or use.

To the best of our knowledge, the information contained in
this publication is accurate; however, we do not assume
any liability whatsoever for the accuracy and completeness
of such information. The information contained in this
publication should not be construed as a promise or
guarantee of specific properties of our products. It is the
sole responsibility of the users to investigate whether any
existing patents are infringed by the use of the materials
mentioned in this publication.

Moreover, there is a need to reduce human exposure to
many materials to the lowest practical limits in view of
possible adverse effects. To the extent that any hazards
may have been mentioned in this publication, we neither
suggest nor guarantee that such hazards are the only ones
which exist. We recommend that persons intending to rely
on any recommendation or to use any equipment,
processing technique, or material mentioned in this
publication should satisfy themselves that they can meet
all applicable safety and health standards.

We strongly recommend that users seek and adhere to the
manufacturer's current instructions for handling each
material they use, and to entrust the handling of such
material to adequately trained personnel only. Please call
the telephone numbers listed for additional technical
information. Call Customer Services for the appropriate
Materials Safety Data Sheets (MSDS) before attempting to
process our products.

The products mentioned herein are not intended for use in
medical or dental implants.

The CAMPUS internet database is hosted by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

CAMPUS® is a Registered trademark of CWFG mbH, Frankfurt/Main, 1991