  KOBLEND® P 477E | PS-I... | Polimeri Europa
Product Texts
Symbol according to ISO 1043-1: (PS-I + PE)

Special polystyrene alloy which combines the easy processing of styrenics with superior impact strength and excellent environmental stress cracking resistance to chemicals, oils and fatty foods.

Koblend P 477E is recommended for the extrusion and the thermoforming of sheets for industrial applications, for inner liners of refrigerators and packaging for fatty foods.


Applications:

Thermoformed panels for tractors, inner liner for refrigerators where HCFC 141b is used as blowing agent for the insulating PU foam, tubs and lids for packaging of fatty foods such as margarine, salads etc.

Rheological propertiesValueUnitTest Standard
Melt volume-flow rate (MVR) 5.5 cm³/10min ISO 1133
Temperature 200 °C ISO 1133
Load 5 kg ISO 1133
Mechanical propertiesValueUnitTest Standard
Tensile Modulus 1200 MPa ISO 527-1/-2
Yield stress 20 MPa ISO 527-1/-2
Yield strain 3.1 % ISO 527-1/-2
Nominal strain at break >50 % ISO 527-1/-2
Charpy impact strength (+23°C) N kJ/m² ISO 179/1eU
Charpy impact strength (-30°C) N kJ/m² ISO 179/1eU
Charpy notched impact strength (+23°C) 29 kJ/m² ISO 179/1eA
Charpy notched impact strength (-30°C) 11 kJ/m² ISO 179/1eA
Thermal propertiesValueUnitTest Standard
Melting temperature (10°C/min) 114 °C ISO 11357-1/-3
Burning Behav. at 1.5 mm nom. thickn. HB class IEC 60695-11-10
Thickness tested 1.5 mm IEC 60695-11-10
Other propertiesValueUnitTest Standard
Density 1000 kg/m³ ISO 1183
Rheological calculation propertiesValueUnitTest Standard
Density of melt 880 kg/m³ -
Spec. heat capacity melt 2300 J/(kg K) -
Diagrams
Dynamic Shear modulus-temperature , KOBLEND® P 477E, PS-I..., Polimeri
Stress-strain , KOBLEND® P 477E, PS-I..., Polimeri
Secant modulus-strain , KOBLEND® P 477E, PS-I..., Polimeri
Spec. enthalpy/mass-temp. (DSC) , KOBLEND® P 477E, PS-I..., Polimeri
Characteristics
Processing
Film Extrusion, Sheet Extrusion, Other Extrusion, Thermoforming
Delivery form
Pellets
Regional Availability
North America, Europe, Asia Pacific, South and Central America, Near East/Africa
Other text information
Film extrusion
PREPROCESSING

Drying normally not required

 

PROCESSING

Melt temperature              200 - 230 °C

Other extrusion
Other  extrusion
PREPROCESSING

Drying normally not required

 

PROCESSING

Melt temperature              200 -230 °C

Sheet extrusion
PREPROCESSING

Drying normally not required

 

PROCESSING

Melt temperature              200 -230 °C

Disclaimer
Dear CAMPUS User,

The data, information and suggestions are provided for guidance
purpose only.
The Company accepts no responsibility for the results obtained
therefrom, as neither for their utilisation in infringement of
possible patents rights.
All indicated data refer to natural grades.
On the subject of the experimental products, the Company reserves the
right to change without prewarning the characteristics, to optimise
the performances.

If you have any questions regarding CAMPUS, please send
an e-mail to:Pe Campus


For further information regarding Polimeri Europa:
	Polimeri Europa Homepage


The CAMPUS internet database is hosted by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

CAMPUS® is a Registered trademark of CWFG mbH, Frankfurt/Main, 1991