offers extended functionality!CAMPUS® datasheet | KYNAR 340
This datasheet of KYNAR 340 from ARKEMA is provided by the international plastics database CAMPUS.
CAMPUS is organized by a group of leading international resin producers, who have agreed to test their material according to uniform conditions, based on ISO standards (ISO 10350, ISO 11403), in order to offer comparable data to the market.
KYNAR 340 | PVDF-CD | ARKEMA
Product Texts
The KYNAR FLEX 340 is a thermoplastic fluorinated polymer The properties are the same as standard grade: chemical resistance, resistance to UV, low permeation, high purity, excellent mechanical behaviour. More over, this grade is electrically conductive. This grade is available as pellet form for injection, extrusion, compression.
| Rheological properties | Value | Unit | Test Standard |
| Melt volume-flow rate (MVR) | 4 | cm³/10min | ISO 1133 |
| Temperature | 230 | °C | ISO 1133 |
| Load | 10 | kg | ISO 1133 |
| Mechanical properties | Value | Unit | Test Standard |
| Charpy notched impact strength (+23°C) | 8 | kJ/m² | ISO 179/1eA |
| Thermal properties | Value | Unit | Test Standard |
| Melting temperature (10°C/min) | 166 | °C | ISO 11357-1/-3 |
| Oxygen index | 43 | % | ISO 4589-1/-2 |
| Other properties | Value | Unit | Test Standard |
| Density | 1780 | kg/m³ | ISO 1183 |
Characteristics
Processing
Injection Molding, Profile Extrusion, Sheet Extrusion, Other Extrusion, Transfer Molding
Delivery form
Granules
Special Characteristics
Light stabilized or stable to light, U.V. stabilized or stable to weather, Heat stabilized or stable to heat
Regional Availability
Disclaimer
This database provides the main properties of technical thermoplastics
marketed by ARKEMA.
The information contained in this document is based on trials carried
out by our Research Centres and data selected from the literature, but
shall in no event be held to constitute or imply any warranty,
undertaking, express or implied commitment from our part.
Our format specifications define the limit of our commitment.
No liability whatsoever can be accepted by ARKEMA with regard to the
handling processing or use of the product or products concerned which
much in all cases be employed in accordance with all relevant laws
and/or regulations in force in the country or countries concerned.
For information about the other products marketed
by our company consult :
ARKEMAGROUP.COM
The CAMPUS internet database is hosted by M-Base Engineering + Software GmbH.
M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors.
Any decision about the application of materials must be double checked with the producer of this material.
CAMPUS® is a Registered trademark of CWFG mbH, Frankfurt/Main, 1991
CAMPUS® is a Registered trademark of CWFG mbH, Frankfurt/Main, 1991