View list of
  • All ARKEMA grades
  • All PVDF grades
  • All grades beginning with K

CAMPUS® datasheet | KYNAR ADX 121


This datasheet of KYNAR ADX 121 from ARKEMA is provided by the international plastics database CAMPUS.

CAMPUS is organized by a group of leading international resin producers, who have agreed to test their material according to uniform conditions, based on ISO standards (ISO 10350, ISO 11403), in order to offer comparable data to the market.

This datasheet includes:

  KYNAR ADX 121 | PVDF | ARKEMA
Product Texts
KYNAR ADX  121 is a thermoplastic fluorinated functionnalized polymer.

The properties are the same as standard grade: 
chemical resistance, resistance to UV, low permeation, high purity, excellent mechanical behaviour.

More over, this grade increases the potential of adhesion on metals and can be processed by powder coating spraying or by solvent application.
Characteristics
Processing
Coating
Delivery form
Powder
Special Characteristics
Light stabilized or stable to light, U.V. stabilized or stable to weather, Heat stabilized or stable to heat
Regional Availability
Disclaimer

This database provides the main properties of technical thermoplastics
marketed by ARKEMA.

      The information contained in this document is based on trials carried
out by our Research Centres and data selected from the literature, but
shall in no event be held to constitute or imply any warranty,
undertaking, express or implied commitment from our part.
Our format specifications define the limit of our commitment.
No liability whatsoever can be accepted by ARKEMA with regard to the
handling processing or use of the product or products concerned which
much in all cases be employed in accordance with all relevant laws
and/or regulations in force in the country or countries concerned.

For information about the other products marketed
by our company consult :
ARKEMAGROUP.COM

The CAMPUS internet database is hosted by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.