CAMPUS® datasheet | Kynar® ADX 1740-15


This datasheet of Kynar® ADX 1740-15 from ARKEMA is provided by the international plastics database CAMPUS.

This datasheet includes:

  Kynar® ADX 1740-15 | PVDF | ARKEMA
Product Texts
 

Kynar® ADX 1740-15

 

Kynar® ADX 1740-15 is a thermoplastic fluorinated functionnalized polymer.

 

The properties are the same as standard grade:

chemical resistance, resistance to UV, low permeation, high purity, excellent mechanical behaviour.

 

More over, this grade increases the potential of adhesion on materials as polyamides, polyolefins and can be coextruded.

Mechanical propertiesValueUnitTest Standard
Yield stress 50 MPa ISO 527-1/-2
Yield strain 9 % ISO 527-1/-2
Nominal strain at break >50 % ISO 527-1/-2
Thermal propertiesValueUnitTest Standard
Melting temperature, 10°C/min 169 °C ISO 11357-1/-3
Temp. of deflection under load, 1.80 MPa 105 °C ISO 75-1/-2
Other propertiesValueUnitTest Standard
Density 1750 kg/m³ ISO 1183
Characteristics
Processing
Other Extrusion
Delivery form
Granules
Special Characteristics
Light stabilized or stable to light, U.V. stabilized or stable to weather, Heat stabilized or stable to heat
Regional Availability
Disclaimer
This database provides the main properties of technical thermoplastics
marketed by ARKEMA.

      The information contained in this document is based on trials carried
out by our Research Centres and data selected from the literature, but
shall in no event be held to constitute or imply any warranty,
undertaking, express or implied commitment from our part.
Our format specifications define the limit of our commitment.
No liability whatsoever can be accepted by ARKEMA with regard to the
handling processing or use of the product or products concerned which
much in all cases be employed in accordance with all relevant laws
and/or regulations in force in the country or countries concerned.

For information about the other products marketed
by our company consult :
ARKEMA,

The CAMPUS internet database is hosted by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

CAMPUS® is a registered trademark of CWFG mbH, Frankfurt am Main, 2012