View list of
  • All ARKEMA grades
  • All PVDF grades
  • All grades beginning with K

CAMPUS® datasheet | Kynar® FLEX 2822


This datasheet of Kynar® FLEX 2822 from ARKEMA is provided by the international plastics database CAMPUS.

This datasheet includes:

  Kynar® FLEX 2822 | PVDF | ARKEMA
Product Texts
 

Kynar® FLEX 2822

 

 

Kynar® FLEX are fluorinated thermoplastic copolymers.

 

Outstanding characteristics of Kynar® FLEX : chemical resistance,

imperviousness to UV, high barrier properties,high purity, good mechanical

and thermomechanical properties

.

Main applications of Kynar® FLEX : corrosion protection in the chemical

industry, coating (painting, coextrusion), off shore, wire and cable.

 

Kynar® FLEX 2822 is a powder identical in composition with the

Kynar® FLEX 2821 but witha lower viscosity. To be used as an additive

in LLDPE to improve the extrusion rate.

Rheological propertiesValueUnitTest Standard
Melt volume-flow rate, MVR 2.8 cm³/10min ISO 1133
Temperature 230 °C ISO 1133
Load 5 kg ISO 1133
Mechanical propertiesValueUnitTest Standard
Tensile Modulus 680 MPa ISO 527-1/-2
Yield stress 24 MPa ISO 527-1/-2
Yield strain 12 % ISO 527-1/-2
Nominal strain at break >50 % ISO 527-1/-2
Thermal propertiesValueUnitTest Standard
Melting temperature, 10°C/min 142 °C ISO 11357-1/-3
Glass transition temperature, 10°C/min -36 °C ISO 11357-1/-2
Temp. of deflection under load, 1.80 MPa 48 °C ISO 75-1/-2
Vicat softening temperature, 50°C/h 50N 76 °C ISO 306
Coeff. of linear therm. expansion, parallel 160 E-6/K ISO 11359-1/-2
Burning Behav. at 1.5 mm nom. thickn. V-0 class IEC 60695-11-10
Thickness tested 1.6 mm IEC 60695-11-10
Burning Behav. at thickness h V-0 class IEC 60695-11-10
Thickness tested 0.8 mm IEC 60695-11-10
Oxygen index 42 % ISO 4589-1/-2
Electrical propertiesValueUnitTest Standard
Relative permittivity, 1MHz 6 - IEC 60250
Dissipation factor, 100Hz 570 E-4 IEC 60250
Dissipation factor, 1MHz 2340 E-4 IEC 60250
Other propertiesValueUnitTest Standard
Water absorption 0.03 % Sim. to ISO 62
Density 1770 kg/m³ ISO 1183
Diagrams
Specific volume-temperature (pvT) , Kynar® FLEX 2822, PVDF, ARKEMA
Characteristics
Delivery form
Powder
Special Characteristics
Light stabilized or stable to light, U.V. stabilized or stable to weather, Heat stabilized or stable to heat
Regional Availability
Chemical Media Resistance
Acids
Acetic Acid (5% by mass) (23°C)
Citric Acid solution (10% by mass) (23°C)
Lactic Acid (10% by mass) (23°C)
Hydrochloric Acid (36% by mass) (23°C)
Nitric Acid (40% by mass) (23°C)
Sulfuric Acid (38% by mass) (23°C)
Sulfuric Acid (5% by mass) (23°C)
Chromic Acid solution (40% by mass) (23°C)
Bases
Sodium Hydroxide solution (35% by mass) (23°C)
Sodium Hydroxide solution (1% by mass) (23°C)
Ammonium Hydroxide solution (10% by mass) (23°C)
Alcohols
Isopropyl alcohol (23°C)
Methanol (23°C)
Ethanol (23°C)
Hydrocarbons
n-Hexane (23°C)
Toluene (23°C)
iso-Octane (23°C)
Ketones
Acetone (23°C)
Ethers
Diethyl ether (23°C)
Mineral oils
SAE 10W40 multigrade motor oil (23°C)
SAE 10W40 multigrade motor oil (130°C)
SAE 80/90 hypoid-gear oil (130°C)
Insulating Oil (23°C)
Standard Fuels
ISO 1817 Liquid 1 (60°C)
ISO 1817 Liquid 2 (60°C)
ISO 1817 Liquid 3 (60°C)
ISO 1817 Liquid 4 (60°C)
Standard fuel without alcohol (pref. ISO 1817 Liquid C) (23°C)
Standard fuel with alcohol (pref. ISO 1817 Liquid 4) (23°C)
Diesel fuel (pref. ISO 1817 Liquid F) (23°C)
Diesel fuel (pref. ISO 1817 Liquid F) (90°C)
Diesel fuel (pref. ISO 1817 Liquid F) (>90°C)
Salt solutions
Sodium Chloride solution (10% by mass) (23°C)
Sodium Hypochlorite solution (10% by mass) (23°C)
Sodium Carbonate solution (20% by mass) (23°C)
Sodium Carbonate solution (2% by mass) (23°C)
Zinc Chloride solution (50% by mass) (23°C)
Other
Ethyl Acetate (23°C)
Hydrogen peroxide (23°C)
Ethylene Glycol (50% by mass) in water (108°C)
Water (23°C)
Deionized water (90°C)
Phenol solution (5% by mass) (23°C)
Disclaimer
This database provides the main properties of technical thermoplastics
marketed by ARKEMA.

      The information contained in this document is based on trials carried
out by our Research Centres and data selected from the literature, but
shall in no event be held to constitute or imply any warranty,
undertaking, express or implied commitment from our part.
Our format specifications define the limit of our commitment.
No liability whatsoever can be accepted by ARKEMA with regard to the
handling processing or use of the product or products concerned which
much in all cases be employed in accordance with all relevant laws
and/or regulations in force in the country or countries concerned.

For information about the other products marketed
by our company consult :
ARKEMA,

The CAMPUS internet database is hosted by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

CAMPUS® is a registered trademark of CWFG mbH, Frankfurt am Main, 2012