  KYNAR FLEX 3120-50 | PVDF | ARKEMA
Product Texts
DESIGNATION : ISO 12086-VDF/HFP-K, EG1N, P.?E7.D.G.B.C ,, ? (3,5-7,5)

KYNAR FLEX PVDF are fluorinated thermoplastic copolymers.

Outstanding characteristics of KYNAR FLEX : chemical resistance, 
imperviousness to UV, high barrier properties, high purity,good mechanical
and thermomechanical properties.

Main applications of KYNAR FLEX : corrosion protection in the chemical
industry, coating (painting, extrusion), wire and cable.

KYNAR FLEX 3120-50 is a grade which exhibits, compared to 2800, 
a higher melting point which allows a greater range for use.  
For cable coating, extrusion of tube and plaque, compression moulding
of bulky parts.
Rheological propertiesValueUnitTest Standard
Melt volume-flow rate (MVR) 0.5 cm³/10min ISO 1133
Temperature 230 °C ISO 1133
Load 5 kg ISO 1133
Mechanical propertiesValueUnitTest Standard
Tensile Modulus 690 MPa ISO 527-1/-2
Yield stress 28 MPa ISO 527-1/-2
Yield strain 12 % ISO 527-1/-2
Nominal strain at break >50 % ISO 527-1/-2
Thermal propertiesValueUnitTest Standard
Melting temperature (10°C/min) 165 °C ISO 11357-1/-3
Glass transition temperature (10°C/min) -46 °C ISO 11357-1/-2
Other propertiesValueUnitTest Standard
Density 1780 kg/m³ ISO 1183
Test specimen productionValueUnitTest Standard
Compression Molding, molding temperature 225 °C ISO 293
Compression Molding, molding time 3 min ISO 293
Compression Molding, demolding temperature 120 °C ISO 293
Characteristics
Processing
Profile Extrusion, Other Extrusion
Delivery form
Pellets
Special Characteristics
Light stabilized or stable to light, U.V. stabilized or stable to weather, Heat stabilized or stable to heat
Regional Availability
Chemical Media Resistance
Acids
Acetic Acid (5% by mass) (23°C)
Citric Acid solution (10% by mass) (23°C)
Lactic Acid (10% by mass) (23°C)
Hydrochloric Acid (36% by mass) (23°C)
Nitric Acid (40% by mass) (23°C)
Sulfuric Acid (38% by mass) (23°C)
Sulfuric Acid (5% by mass) (23°C)
Chromic Acid solution (40% by mass) (23°C)
Bases
Sodium Hydroxide solution (35% by mass) (23°C)
Sodium Hydroxide solution (1% by mass) (23°C)
Ammonium Hydroxide solution (10% by mass) (23°C)
Alcohols
Isopropyl alcohol (23°C)
Methanol (23°C)
Ethanol (23°C)
Hydrocarbons
n-Hexane (23°C)
Toluene (23°C)
iso-Octane (23°C)
Ketones
Acetone (23°C)
Ethers
Diethyl ether (23°C)
Mineral oils
SAE 10W40 multigrade motor oil (23°C)
SAE 10W40 multigrade motor oil (130°C)
SAE 80/90 hypoid-gear oil (130°C)
Insulating Oil (23°C)
Standard Fuels
ISO 1817 Liquid 1 (60°C)
ISO 1817 Liquid 2 (60°C)
ISO 1817 Liquid 3 (60°C)
ISO 1817 Liquid 4 (60°C)
Standard fuel without alcohol (pref. ISO 1817 Liquid C) (23°C)
Standard fuel with alcohol (pref. ISO 1817 Liquid 4) (23°C)
Diesel fuel (pref. ISO 1817 Liquid F) (23°C)
Diesel fuel (pref. ISO 1817 Liquid F) (90°C)
Diesel fuel (pref. ISO 1817 Liquid F) (>90°C)
Salt solutions
Sodium Chloride solution (10% by mass) (23°C)
Sodium Hypochlorite solution (10% by mass) (23°C)
Sodium Carbonate solution (20% by mass) (23°C)
Sodium Carbonate solution (2% by mass) (23°C)
Zinc Chloride solution (50% by mass) (23°C)
Other
Ethyl Acetate (23°C)
Hydrogen peroxide (23°C)
Ethylene Glycol (50% by mass) in water (108°C)
Water (23°C)
Deionized water (90°C)
Phenol solution (5% by mass) (23°C)
Disclaimer

This database provides the main properties of technical thermoplastics
marketed by ARKEMA.

      The information contained in this document is based on trials carried
out by our Research Centres and data selected from the literature, but
shall in no event be held to constitute or imply any warranty,
undertaking, express or implied commitment from our part.
Our format specifications define the limit of our commitment.
No liability whatsoever can be accepted by ARKEMA with regard to the
handling processing or use of the product or products concerned which
much in all cases be employed in accordance with all relevant laws
and/or regulations in force in the country or countries concerned.

For information about the other products marketed
by our company consult :
ARKEMAGROUP.COM

The CAMPUS internet database is hosted by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

CAMPUS® is a Registered trademark of CWFG mbH, Frankfurt/Main, 1991