CAMPUS® datasheet | Luran® S 797 SE


This datasheet of Luran® S 797 SE from Styrolution Group GmbH is provided by the international plastics database CAMPUS.

You may contact the supplier for more information about this grade.

This datasheet includes:

  Luran® S 797 SE | ASA | Styrolution Group GmbH
Product Texts
Extrusion grade with especially high notched impact strength (eg for door panels and surf boards)
Rheological propertiesValueUnitTest Standard
Melt volume-flow rate, MVR 5.5 cm³/10min ISO 1133
Temperature 220 °C ISO 1133
Load 10 kg ISO 1133
Molding shrinkage, parallel 0.5 % ISO 294-4, 2577
Molding shrinkage, normal 0.9 % ISO 294-4, 2577
Mechanical propertiesValueUnitTest Standard
Tensile Modulus 2000 MPa ISO 527-1/-2
Yield stress 42 MPa ISO 527-1/-2
Yield strain 3.5 % ISO 527-1/-2
Nominal strain at break 11 % ISO 527-1/-2
Tensile creep modulus, 1000h 1100 MPa ISO 899-1
Charpy impact strength, +23°C 250 kJ/m² ISO 179/1eU
Charpy impact strength, -30°C 180 kJ/m² ISO 179/1eU
Charpy notched impact strength, +23°C 40 kJ/m² ISO 179/1eA
Charpy notched impact strength, -30°C 9 kJ/m² ISO 179/1eA
Thermal propertiesValueUnitTest Standard
Temp. of deflection under load, 1.80 MPa 95 °C ISO 75-1/-2
Temp. of deflection under load, 0.45 MPa 100 °C ISO 75-1/-2
Vicat softening temperature, 50°C/h 50N 90 °C ISO 306
Coeff. of linear therm. expansion, parallel 95 E-6/K ISO 11359-1/-2
Burning Behav. at 1.5 mm nom. thickn. HB class IEC 60695-11-10
Thickness tested 1.6 mm IEC 60695-11-10
UL recognition UL - -
Burning Behav. at thickness h HB class IEC 60695-11-10
Thickness tested 0.8 mm IEC 60695-11-10
UL recognition UL - -
Oxygen index 19 % ISO 4589-1/-2
Electrical propertiesValueUnitTest Standard
Relative permittivity, 100Hz 3.8 - IEC 60250
Relative permittivity, 1MHz 3.3 - IEC 60250
Dissipation factor, 100Hz 90 E-4 IEC 60250
Dissipation factor, 1MHz 260 E-4 IEC 60250
Volume resistivity 1E12 Ohm*m IEC 60093
Surface resistivity 1E13 Ohm IEC 60093
Electric strength 35 kV/mm IEC 60243-1
Comparative tracking index 600 - IEC 60112
Other propertiesValueUnitTest Standard
Water absorption 1.65 % Sim. to ISO 62
Humidity absorption 0.35 % Sim. to ISO 62
Density 1070 kg/m³ ISO 1183
Rheological calculation propertiesValueUnitTest Standard
Ejection temperature 95 °C -
Test specimen productionValueUnitTest Standard
Injection Molding, melt temperature 250 °C ISO 294
Injection Molding, mold temperature 60 °C ISO 10724
Injection Molding, injection velocity 200 mm/s ISO 294
Diagrams
Viscosity-shear rate , Luran® S 797 SE, ASA, Styrolution
Shearstress-shear rate , Luran® S 797 SE, ASA, Styrolution
Stress-strain , Luran® S 797 SE, ASA, Styrolution
Secant modulus-strain , Luran® S 797 SE, ASA, Styrolution
Stress-strain (isochronous) 23°C, Luran® S 797 SE, ASA, Styrolution
Creep modulus-time 23°C, Luran® S 797 SE, ASA, Styrolution
Stress-strain (isochronous) 40°C, Luran® S 797 SE, ASA, Styrolution
Creep modulus-time 40°C, Luran® S 797 SE, ASA, Styrolution
Stress-strain (isochronous) 60°C, Luran® S 797 SE, ASA, Styrolution
Creep modulus-time 60°C, Luran® S 797 SE, ASA, Styrolution
Stress-strain (isochronous) 80°C, Luran® S 797 SE, ASA, Styrolution
Creep modulus-time 80°C, Luran® S 797 SE, ASA, Styrolution
Specific volume-temperature (pvT) , Luran® S 797 SE, ASA, Styrolution
Tensile modulus-temperature , Luran® S 797 SE, ASA, Styrolution
Characteristics
Processing
Profile Extrusion, Sheet Extrusion, Other Extrusion
Delivery form
Pellets
Additives
Release agent
Special Characteristics
Light stabilized or stable to light, U.V. stabilized or stable to weather, Heat stabilized or stable to heat
Regional Availability
Other text information
Other extrusion
PREPROCESSING
Pre/Post-processing, Pre-drying, Temperature: 80 °C
Pre/Post-processing, Pre-drying, Time: 2 - 4 h

PROCESSING
Extrusion, Pipes, Melt temperature: 200 - 240 °C
Profile extrusion
PREPROCESSING
Pre/Post-processing, Pre-drying, Temperature: 80 °C
Pre/Post-processing, Pre-drying, Time: 2 - 4 h

PROCESSING
Extrusion, Profiles, Melt temperature: 200 - 240 °C
Sheet extrusion
PREPROCESSING
Pre/Post-processing, Pre-drying, Temperature: 80 °C
Pre/Post-processing, Pre-drying, Time: 2 - 4 h

PROCESSING
Extrusion, Plates, Melt temperature: 210 - 250 °C
Disclaimer
The data contained in this publication are based on our current
knowledge and experience. In view of the many factors that may affect
processing and application of our product, these data do not relieve
processors from carrying out their own investigations and tests. Any
descriptions, drawings, photographs, data, proportions, weights etc.
given herein may change without prior information and do not constitute
the agreed contractual quality of the product. It is the responsibility
of the recipient of our products to ensure that any proprietary rights
and existing laws and legislation are observed. NO WARRANTIES OF ANY
KIND, EITHER EXPRESS OR IMPLIED, INCLUDING WARRANTIES OFMERCHANTABILITY
OR FITNESS FOR A PARTICULAR PURPOSE, ARE MADE REGARDING PRODUCTS
DESCRIBED OR DESIGNS, DATA OR INFORMATION SET FORTH, OR THAT THE
PRODUCTS, DESIGNS, DATA OR INFORMATION MAY BE USED WITHOUT INFRINGING
THEINTELLECTUAL PROPERTY RIGHTS OF OTHERS.

In order to check the availability of products please contact us or our
sales agency.


For more information about our products contact

Styrolution GmbH
Styrolution Infopoint
mailto:styrenics.infopoint@basf.com
Tel: +49 621 60 41446

CAMPUS® is a registered trademark of CWFG (Chemie
Wirtschaftsfoerderungsgesellschaft GmbH, Frankfurt)

The CAMPUS internet database is hosted by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

CAMPUS® is a registered trademark of CWFG mbH, Frankfurt am Main, 2012