  Novamid® 1011CH5 | PA6 | DSM Engineering Plastics
Product Texts
Heat Stabilized, Easy Molding Grade

ISO 1043 PA6

Akulon® polyamide 6 and 66 resins
Rheological propertiesdry / condUnitTest Standard
Melt volume-flow rate (MVR) 38 / * cm³/10min ISO 1133
Temperature 230 / * °C ISO 1133
Load 2.16 / * kg ISO 1133
Mechanical propertiesdry / condUnitTest Standard
Tensile Modulus 3100 / 1000 MPa ISO 527-1/-2
Yield stress 80 / 40 MPa ISO 527-1/-2
Yield strain 5.2 / 21 % ISO 527-1/-2
Nominal strain at break 19 / >50 % ISO 527-1/-2
Charpy impact strength (+23°C) N / N kJ/m² ISO 179/1eU
Charpy notched impact strength (+23°C) 3 / 31 kJ/m² ISO 179/1eA
Thermal propertiesdry / condUnitTest Standard
Temp. of deflection under load (1.80 MPa) 57 / * °C ISO 75-1/-2
Temp. of deflection under load (0.45 MPa) 175 / * °C ISO 75-1/-2
Coeff. of linear therm. expansion (parallel) 70 / * E-6/K ISO 11359-1/-2
Coeff. of linear therm. expansion (normal) 80 / * E-6/K ISO 11359-1/-2
Burning Behav. at thickness h V-2 / * class IEC 60695-11-10
Thickness tested 0.8 / * mm IEC 60695-11-10
UL recognition UL / * - -
Electrical propertiesdry / condUnitTest Standard
Relative permittivity (100Hz) 4 / - - IEC 60250
Relative permittivity (1MHz) 4 / - - IEC 60250
Dissipation factor (100Hz) 120 / - E-4 IEC 60250
Dissipation factor (1MHz) 220 / - E-4 IEC 60250
Volume resistivity >1E13 / - Ohm*m IEC 60093
Surface resistivity * / 2E14 Ohm IEC 60093
Electric strength 26 / - kV/mm IEC 60243-1
Comparative tracking index 600 / - - IEC 60112
Other propertiesdry / condUnitTest Standard
Humidity absorption 3.3 / * % Sim. to ISO 62
Density 1140 / - kg/m³ ISO 1183
Characteristics
Processing
Injection Molding
Delivery form
Pellets
Additives
Release agent
Special Characteristics
Heat stabilized or stable to heat
Regional Availability
North America, Europe, Asia Pacific
Other text information
Injection molding
<font face="Arial" size="2">Injection Molding Recommendations
Disclaimer
 All information supplied by or on behalf of DSM in relation to its
products, whether in the nature of data, recommendations or otherwise,
is supported by research and, in good faith, believed reliable, but DSM
assumes no liability and makes no warranties of any kind, express or
implied, including, but not limited to, those of title, merchantability,
fitness for a particular purpose or non-infringement or any warranty
arising from a course of dealing, usage, or trade practice whatsoever
in respect of application, processing or use made of the aforementioned
information or product. The user assumes all responsibility for the use
of all information provided and shall verify quality and other properties or
any consequence from the use of all such information.

Typical values are indicative only and are not to be construed as being
binding specifications.

The CAMPUS internet database is hosted by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

CAMPUS® is a Registered trademark of CWFG mbH, Frankfurt/Main, 1991