ORGALLOY LT 4060ES noir T6L | PA6... | ARKEMA
Product Texts
ORGALLOY LT 4060ES noir T6L - LT 4060 Very flexible polyamide alloys: easy to process, low moisture absorption, good mechanical properties at low temperature. Demonstrate a good balance of properties eg, high flexibility (200 MPa), good thermal performance and and ductility at low temperatures. LT 4060ES NOIR T6L : Suited to blow moulded parts under the bonnet (air intake...) Sequential extrusion with RS or LE series (rigid-flexible combinations). LT 4060 : standard grade, injection moulding or tubes, mandrels... LT 4060ES NOIR T6L : blow moulding grade or tube extrusion.
| Rheological properties | dry / cond | Unit | Test Standard |
| Melt volume-flow rate (MVR) | 0.5 / * | cm³/10min | ISO 1133 |
| Temperature | 235 / * | °C | ISO 1133 |
| Load | 5 / * | kg | ISO 1133 |
| Mechanical properties | dry / cond | Unit | Test Standard |
| Tensile Modulus | - / 300 | MPa | ISO 527-1/-2 |
| Stress at 50% strain | - / 22 | MPa | ISO 527-1/-2 |
| Strain at break | - / >50 | % | ISO 527-1/-2 |
| Charpy impact strength (+23°C) | N / N | kJ/m² | ISO 179/1eU |
| Charpy notched impact strength (+23°C) | N / N | kJ/m² | ISO 179/1eA |
| Thermal properties | dry / cond | Unit | Test Standard |
| Melting temperature (10°C/min) | 220 / * | °C | ISO 11357-1/-3 |
| Temp. of deflection under load (0.45 MPa) | 60 / * | °C | ISO 75-1/-2 |
| Burning Behav. at 1.5 mm nom. thickn. | HB / * | class | IEC 60695-11-10 |
| Thickness tested | 1.6 / * | mm | IEC 60695-11-10 |
| Burning Behav. at thickness h | HB / * | class | IEC 60695-11-10 |
| Thickness tested | 3.2 / * | mm | IEC 60695-11-10 |
| Electrical properties | dry / cond | Unit | Test Standard |
| Comparative tracking index | * / 600 | - | IEC 60112 |
| Other properties | dry / cond | Unit | Test Standard |
| Water absorption | 5 / * | % | Sim. to ISO 62 |
| Humidity absorption | 1.1 / * | % | Sim. to ISO 62 |
| Density | 1040 / 1040 | kg/m³ | ISO 1183 |
| Test specimen production | Value | Unit | Test Standard |
| Injection Molding, melt temperature | 260 | °C | ISO 294 |
| Injection Molding, mold temperature | 60 | °C | ISO 10724 |
Diagrams
Characteristics
Processing
Film Extrusion, Profile Extrusion, Sheet Extrusion, Other Extrusion, Blow Molding
Delivery form
Pellets
Special Characteristics
Platable, Light stabilized or stable to light, Heat stabilized or stable to heat
Regional Availability
Other text information
Profile extrusion
PREPROCESSING
Max water content: 0,05-0,15 %
Notice text : ORGALLOY grades are delivered ready for use.
: If Orgalloy is not used within 4 hours of opening
: the bag,the product should be redried at 90°C
: during 4 hours.
PROCESSING
Melt temperature : 255-265 °C
Notice text : It is recommended to use an extruder equipped with
: a 25D or greater polyamide screw.It is also
: recommended to avoid high levels of shearing action.
: For extrusion of tubes, a calibration device should
: be used which has a conical entry and good
: regulation of cooling water flow.
Blow molding
PREPROCESSING
Max water content: 0,05-0,15 %
Notice text : ORGALLOY grades are delivered ready for use.
: If Orgalloy is not used within 4 hours of opening
: the bag,the product should be redried at 90°C
: during 4 hours.
PROCESSING
Melt temperature : 245-255 °C
Notice text : These products are suited to all types of blow
: moulded components, including sequential 3D. It is
: necessary to select grades with comparable melt
: strength and swelling. Processable ona PE screw.
: The ideal melt temperature is around 250°C.
Chemical Media Resistance
Disclaimer
This database provides the main properties of technical thermoplastics
marketed by ARKEMA.
The information contained in this document is based on trials carried
out by our Research Centres and data selected from the literature, but
shall in no event be held to constitute or imply any warranty,
undertaking, express or implied commitment from our part.
Our format specifications define the limit of our commitment.
No liability whatsoever can be accepted by ARKEMA with regard to the
handling processing or use of the product or products concerned which
much in all cases be employed in accordance with all relevant laws
and/or regulations in force in the country or countries concerned.
For information about the other products marketed
by our company consult :
ARKEMAGROUP.COM
The CAMPUS internet database is hosted by M-Base Engineering + Software GmbH.
M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors.
Any decision about the application of materials must be double checked with the producer of this material.
CAMPUS® is a Registered trademark of CWFG mbH, Frankfurt/Main, 1991
CAMPUS® is a Registered trademark of CWFG mbH, Frankfurt/Main, 1991