View list of

CAMPUS® datasheet | P84 NT1 40G


This datasheet of P84 NT1 40G from Evonik Industries AG is provided by the international plastics database CAMPUS.

CAMPUS is organized by a group of leading international resin producers, who have agreed to test their material according to uniform conditions, based on ISO standards (ISO 10350, ISO 11403), in order to offer comparable data to the market.

You may contact the supplier for more information about this grade.

This datasheet includes:

  P84® NT1 40G | PI-CD | Evonik Industries AG
Product Texts
Polyimid P84® NT - at a glance

 

  • Excellent performance at high temperatures
  • High strength and excellent shape stability
  • Very good impact resistance
  • High heat deflection temperature
  • Very good creep resistance even at elevated temperatures
  • Machinable with standard tools
  • Low wear and friction behaviour
  • Processing by Hot compression molding or Direct forming

 

 

Application examples

bushings, seals, bearings components, guides, gear wheels, and valve parts

in the automotive and aerospace industries and in industrial equipment.

Mechanical propertiesdry / condUnitTest Standard
Tensile Modulus 4700 / - MPa ISO 527-1/-2
Stress at break 54 / - MPa ISO 527-1/-2
Strain at break 2.7 / - % ISO 527-1/-2
Thermal propertiesdry / condUnitTest Standard
Temp. of deflection under load (1.80 MPa) 325 / * °C ISO 75-1/-2
Temp. of deflection under load (0.45 MPa) 358 / * °C ISO 75-1/-2
Coeff. of linear therm. expansion (parallel) 11 / * E-6/K ISO 11359-1/-2
Other propertiesdry / condUnitTest Standard
Density 1580 / - kg/m³ ISO 1183
Characteristics
Delivery form
Granules, Powder
Additives
Lubricants
Special Characteristics
Heat stabilized or stable to heat
Regional Availability
Other text information
Compression molding

Hot compression molding

Production of big semi-finished parts (plates, rods, tubes)

High pressure 400 kg/cm² and temperature above Tg (350-380 °C)

Cycle time = hours

Processing of precise parts by machining

Best mechanical properties

 

 

Direct forming

High number of small parts

Production of green parts at ambient temperature and very high pressure of 3 t/cm²

Cycle time = econds

Sub sequent sintering above Tg (350-380 °C)

No or little machining necessary

Disclaimer
With the following data, which reflect our current knowledge and experience,
we wish to describe possible applications, however this information is given
without guarantee or assurance of the appropriate properties for a specific
application.

The processor is not relieved of the responsibility for incoming quality control
nor from his own testing and analysis.

All data concerning product safety (EG-guideline, BGVV, FDA) are of principle
nature and can be limitied regarding migration, temperature and type of food.
They reflect the status as of Feb. 29, 2012. To insure that this data reflects the
current state, please contact our Product Safety Department.

Should you have any questions, wishes or suggestions about CAMPUS,
please refer to the following address:

  Link to Evonik Industries AG homepage

In any case, we hope you enjoy working with CAMPUS!

The CAMPUS internet database is hosted by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

CAMPUS® is a Registered trademark of CWFG mbH, Frankfurt/Main, 1991