offers extended functionality!CAMPUS® datasheet | PEBAX 5533 SN 70 NOIR
This datasheet of PEBAX 5533 SN 70 NOIR from ARKEMA is provided by the international plastics database CAMPUS.
CAMPUS is organized by a group of leading international resin producers, who have agreed to test their material according to uniform conditions, based on ISO standards (ISO 10350, ISO 11403), in order to offer comparable data to the market.
PEBAX 5533 SN 70 NOIR | TPA-CD... | ARKEMA
Product Texts
POLYETHER BLOCK AMIDE (PEBA) PEBAX 5533 SN 70 noir is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This SN 70 grade is made conductive thanks to carbon black.
| Rheological properties | dry / cond | Unit | Test Standard |
| Melt volume-flow rate (MVR) | 5 / * | cm³/10min | ISO 1133 |
| Temperature | 250 / * | °C | ISO 1133 |
| Load | 5 / * | kg | ISO 1133 |
| Mechanical properties | dry / cond | Unit | Test Standard |
| Tensile Modulus | 305 / 298 | MPa | ISO 527-1/-2 |
| Yield stress | 18 / 17 | MPa | ISO 527-1/-2 |
| Yield strain | 31 / 36 | % | ISO 527-1/-2 |
| Nominal strain at break | >50 / >50 | % | ISO 527-1/-2 |
| Charpy impact strength (+23°C) | N / - | kJ/m² | ISO 179/1eU |
| Charpy impact strength (-30°C) | N / - | kJ/m² | ISO 179/1eU |
| Charpy notched impact strength (+23°C) | N / - | kJ/m² | ISO 179/1eA |
| Charpy notched impact strength (-30°C) | 18 / - | kJ/m² | ISO 179/1eA |
| Shore D hardness (15s) | 51 / * | - | ISO 868 |
| Thermal properties | dry / cond | Unit | Test Standard |
| Melting temperature (10°C/min) | 159 / * | °C | ISO 11357-1/-3 |
| Burning Behav. at 1.5 mm nom. thickn. | HB / * | class | IEC 60695-11-10 |
| Thickness tested | 1.6 / * | mm | IEC 60695-11-10 |
| Burning Behav. at thickness h | HB / * | class | IEC 60695-11-10 |
| Thickness tested | 3.2 / * | mm | IEC 60695-11-10 |
| Electrical properties | dry / cond | Unit | Test Standard |
| Volume resistivity | 110000 / - | Ohm*m | IEC 60093 |
| Surface resistivity | * / 5500 | Ohm | IEC 60093 |
| Other properties | dry / cond | Unit | Test Standard |
| Water absorption | 1.2 / * | % | Sim. to ISO 62 |
| Density | 1090 / 1090 | kg/m³ | ISO 1183 |
| Test specimen production | Value | Unit | Test Standard |
| Injection Molding, melt temperature | 260 | °C | ISO 294 |
| Injection Molding, mold temperature | 30 | °C | ISO 10724 |
| Injection Molding, injection velocity | 200 | mm/s | ISO 294 |
| Injection Molding, pressure at hold | 30 | MPa | ISO 294 |
Diagrams
Characteristics
Processing
Injection Molding, Film Extrusion, Profile Extrusion, Other Extrusion, Transfer Molding, Casting, Thermoforming
Delivery form
Pellets
Special Characteristics
Increased electrical conductivity, Anti-static, Platable, Light stabilized or stable to light, U.V. stabilized or stable to weather, Heat stabilized or stable to heat
Regional Availability
Other text information
Injection molding
PREPROCESSING
Max water content: 0.03 - 0.15 %
Notice text : Our products are delivered pre-dried and in sealed
: bags.Therefore, they do not require any drying
: stage before use:
: 1- Keep the bags at the workshop temperature for
: several hours before use.
: 2- Re-dry the product whenever the bags have
: remained open for more than 4 hours.
PROCESSING
Melt temperature : 220 - 280 °C
Mold temperature : 20 - 40 °C
Notice text : Under specific conditions, our product can easily
: withstand 20 to 30 degrees more than the
: recommended temperatures.
Profile extrusion
PREPROCESSING
Max water content: 0.03 - 0.15 %
Notice text : Our products are delivered pre-dried and in sealed
: bags.Therefore, they do not require any drying
: stage before use:
: 1- Keep the bags at the workshop temperature for
: several hours before use.
: 2- Re-dry the product whenever the bags have
: remained open for more than 4 hours.
PROCESSING
Melt temperature : 190 - 230 °C
Notice text : Too high temperatures can generate sticking of the
: melt on the sizer.
Chemical Media Resistance
| Acids | |
![]() | Sulfuric Acid (38% by mass) (23°C) |
| Bases | |
![]() | Sodium Hydroxide solution (1% by mass) (23°C) |
| Alcohols | |
![]() | Ethanol (23°C) |
| Hydrocarbons | |
![]() | iso-Octane (23°C) |
| Ketones | |
![]() | Acetone (23°C) |
| Salt solutions | |
![]() | Zinc Chloride solution (50% by mass) (23°C) |
| Other | |
![]() | Water (23°C) |
Disclaimer
This database provides the main properties of technical thermoplastics
marketed by ARKEMA.
The information contained in this document is based on trials carried
out by our Research Centres and data selected from the literature, but
shall in no event be held to constitute or imply any warranty,
undertaking, express or implied commitment from our part.
Our format specifications define the limit of our commitment.
No liability whatsoever can be accepted by ARKEMA with regard to the
handling processing or use of the product or products concerned which
much in all cases be employed in accordance with all relevant laws
and/or regulations in force in the country or countries concerned.
For information about the other products marketed
by our company consult :
ARKEMAGROUP.COM
The CAMPUS internet database is hosted by M-Base Engineering + Software GmbH.
M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors.
Any decision about the application of materials must be double checked with the producer of this material.
CAMPUS® is a Registered trademark of CWFG mbH, Frankfurt/Main, 1991
CAMPUS® is a Registered trademark of CWFG mbH, Frankfurt/Main, 1991